CA2080762A1 - Zinc alloy powder for alkaline cell and method to produce the same - Google Patents
Zinc alloy powder for alkaline cell and method to produce the sameInfo
- Publication number
- CA2080762A1 CA2080762A1 CA2080762A CA2080762A CA2080762A1 CA 2080762 A1 CA2080762 A1 CA 2080762A1 CA 2080762 A CA2080762 A CA 2080762A CA 2080762 A CA2080762 A CA 2080762A CA 2080762 A1 CA2080762 A1 CA 2080762A1
- Authority
- CA
- Canada
- Prior art keywords
- weight
- bismuth
- aluminum
- produce
- alloy powder
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
A non-amalgamated zinc alloy powder for use in an alkaline cell which consists essentially of an elemental component selected from among the following compositions (1) to (4);
(1) 0.001 to 0.5 % by weight of aluminum and 0.01 to 0.5 % by weight of bismuth, (2) 0.001 to 0.5 % by weight of aluminum, 0.01 to 0.5 % by weight of bismuth and not more than 1.0 % by weight of indium, (3) 0.001 to 0.5% by weight of aluminum, 0.01 to 0.5 % by weight of bismuth and not more than 0.5 % by weight of lithium, and (4) 0.001 to 0.5 % by weight of aluminum, 0.01 to 0.5 % by weight of bismuth, not more than 1.0 % by weight of indium, and not more than 0.5 % by weight of calcium or not more than 0.5 % by weight of lithium;
and the balance being zinc and containing iron as an inevitably accidental impurity in an amount of not more than 1 ppm; and which can greatly suppress the evolution of hydrogen gas and maintain the discharge performance on a practical level:
and a method to produce the same.
(1) 0.001 to 0.5 % by weight of aluminum and 0.01 to 0.5 % by weight of bismuth, (2) 0.001 to 0.5 % by weight of aluminum, 0.01 to 0.5 % by weight of bismuth and not more than 1.0 % by weight of indium, (3) 0.001 to 0.5% by weight of aluminum, 0.01 to 0.5 % by weight of bismuth and not more than 0.5 % by weight of lithium, and (4) 0.001 to 0.5 % by weight of aluminum, 0.01 to 0.5 % by weight of bismuth, not more than 1.0 % by weight of indium, and not more than 0.5 % by weight of calcium or not more than 0.5 % by weight of lithium;
and the balance being zinc and containing iron as an inevitably accidental impurity in an amount of not more than 1 ppm; and which can greatly suppress the evolution of hydrogen gas and maintain the discharge performance on a practical level:
and a method to produce the same.
Applications Claiming Priority (2)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
JPHEI.3-294839 | 1991-10-16 | ||
JP29483991 | 1991-10-16 |
Publications (2)
Publication Number | Publication Date |
---|---|
CA2080762A1 true CA2080762A1 (en) | 1993-04-17 |
CA2080762C CA2080762C (en) | 1999-01-12 |
Family
ID=17812922
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
CA002080762A Expired - Lifetime CA2080762C (en) | 1991-10-16 | 1992-10-16 | Zinc alloy powder for alkaline cell and method to produce the same |
Country Status (2)
Country | Link |
---|---|
CA (1) | CA2080762C (en) |
MX (1) | MX9205861A (en) |
-
1992
- 1992-10-13 MX MX9205861A patent/MX9205861A/en not_active IP Right Cessation
- 1992-10-16 CA CA002080762A patent/CA2080762C/en not_active Expired - Lifetime
Also Published As
Publication number | Publication date |
---|---|
MX9205861A (en) | 1993-08-01 |
CA2080762C (en) | 1999-01-12 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
CA2061023A1 (en) | Zinc alloy powder for alkaline cell and method to produce the same | |
AU6325094A (en) | Battery grids and plates and lead-acid batteries made using such grids and plates | |
AU1883797A (en) | Lead-calcium alloys, particularly for battery grids | |
CA2219522A1 (en) | Electrochemical hydrogen storage alloys and batteries containing heterogeneous powder particles | |
TW354770B (en) | Kinetic solder paste composition | |
JPS6459769A (en) | Negative current collector for zinc-alkaline battery | |
CA2146356A1 (en) | Steel containing super-finely dispersed oxide system inclusions | |
PL357637A1 (en) | Alloy for thin positive grid for lead acid batteries and method for manufacture of grid | |
GB793083A (en) | Improvements relating to lead-acid accumulators | |
AU594661B2 (en) | Cell corrosion reduction | |
CA2080762A1 (en) | Zinc alloy powder for alkaline cell and method to produce the same | |
NZ328992A (en) | Tin and zinc based shot for ammunition including 12 - 60% lead and 0 - 5% aluminium | |
JPS5690943A (en) | Alloy for wire cut electrospark machining electrode | |
JPS57107565A (en) | Silver peroxide battery | |
JPS5622601A (en) | Hydrogen storing material | |
Uemura et al. | Zinc Alloy Powder for Alkaline Cell and Method to Produce the Same | |
JPS58218762A (en) | Alkaline battery | |
JPS6459768A (en) | Negative current collector for zinc-alkaline battery | |
JPS5565346A (en) | Aluminum alloy for galvanic anode | |
RU2012624C1 (en) | Lead-base alloy | |
IE48165B1 (en) | Method of preparing alloys for making electrode supports in lead accumulators | |
JPS5565345A (en) | Aluminum alloy for galvanic anode | |
JPS5569235A (en) | Aluminum alloy for galvanic anode | |
JPS6472464A (en) | Metallic oxide-hydrogen cell | |
Horst | Anode Alloy for Alkaline Electrolyte Battery |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
EEER | Examination request | ||
MKEX | Expiry | ||
MKEX | Expiry |
Effective date: 20121016 |