JPS6459769A - Negative current collector for zinc-alkaline battery - Google Patents

Negative current collector for zinc-alkaline battery

Info

Publication number
JPS6459769A
JPS6459769A JP62214990A JP21499087A JPS6459769A JP S6459769 A JPS6459769 A JP S6459769A JP 62214990 A JP62214990 A JP 62214990A JP 21499087 A JP21499087 A JP 21499087A JP S6459769 A JPS6459769 A JP S6459769A
Authority
JP
Japan
Prior art keywords
current collector
zinc
alloy powder
negative current
alkaline battery
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
JP62214990A
Other languages
Japanese (ja)
Inventor
Akira Hayashi
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
ALKALI DRY BATTERY ENG LAB
ARUKARI KANDENCHI GIJUTSU KENKYU KUMIAI
Original Assignee
ALKALI DRY BATTERY ENG LAB
ARUKARI KANDENCHI GIJUTSU KENKYU KUMIAI
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ALKALI DRY BATTERY ENG LAB, ARUKARI KANDENCHI GIJUTSU KENKYU KUMIAI filed Critical ALKALI DRY BATTERY ENG LAB
Priority to JP62214990A priority Critical patent/JPS6459769A/en
Publication of JPS6459769A publication Critical patent/JPS6459769A/en
Pending legal-status Critical Current

Abstract

PURPOSE:To retard the hydrogen evolution in a zinc-alkaline battery in which unamalgamated zinc alloy powder or low amalgam zinc alloy powder having an amalgamation rate of 2wt.% or less is used by forming a negative current collector itself or the surface in contact with a gelled negative electrode of the negative current collector with a copper base alloy containing lead and/or tin. CONSTITUTION:A current collector is formed with a copper base alloy containing 0.2-5wt.% Pb and 0.1-6wt.% Sn. By selecting this alloy, the current collector having practical strength and a practical hydrogen gas evolution limit is obtained. If 0.002-2wt.% at least one metal selected from the group comprising Be, Ti, Zr, Mn, Zn, Cd, Al, In, Si, P, and Bi in addition to Pb and/or Sn is added, the hardness and ductility are increased without a remarkable increase in hydrogen gas evolution. By using this negative current collector 5, hydrogen gas evolution is retarded in a zinc-alkaline battery even if unamalgamated zinc alloy powder or low amalgam zinc alloy powder is used as a negative active material. The performance deterioration, bulging, and electrolyte leakage of the battery during storage are also prevented.
JP62214990A 1987-08-31 1987-08-31 Negative current collector for zinc-alkaline battery Pending JPS6459769A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
JP62214990A JPS6459769A (en) 1987-08-31 1987-08-31 Negative current collector for zinc-alkaline battery

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
JP62214990A JPS6459769A (en) 1987-08-31 1987-08-31 Negative current collector for zinc-alkaline battery

Publications (1)

Publication Number Publication Date
JPS6459769A true JPS6459769A (en) 1989-03-07

Family

ID=16664873

Family Applications (1)

Application Number Title Priority Date Filing Date
JP62214990A Pending JPS6459769A (en) 1987-08-31 1987-08-31 Negative current collector for zinc-alkaline battery

Country Status (1)

Country Link
JP (1) JPS6459769A (en)

Cited By (14)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPH0275160A (en) * 1988-09-09 1990-03-14 Yuasa Battery Co Ltd Zinc electrode
JPH0315156A (en) * 1988-12-01 1991-01-23 Yuasa Battery Co Ltd Zinc electrode plate for secondary battery
US4992343A (en) * 1989-08-17 1991-02-12 Eveready Battery Company, Inc. Lead-containing anode current collector for alkaline cells
US5112705A (en) * 1989-08-17 1992-05-12 Eveready Battery Company, Inc. Coated anode current collector for alkaline cells
US5348816A (en) * 1991-06-11 1994-09-20 Fuji Electrochemical Co., Ltd. Alkaline battery
JPH0785877A (en) * 1993-09-10 1995-03-31 Toshiba Battery Co Ltd Button type alkaline battery
JPH0794154A (en) * 1993-09-21 1995-04-07 Hitachi Maxell Ltd Alkaline button battery
EP0801432A1 (en) * 1996-04-12 1997-10-15 Rayovac Corporation Rechargeable alkaline electrochemical cell
US6602629B1 (en) 2000-05-24 2003-08-05 Eveready Battery Company, Inc. Zero mercury air cell
US7632605B2 (en) 2005-04-29 2009-12-15 Eveready Battery Co., Inc. Alkaline cell anode casing
US7993508B2 (en) 2006-11-01 2011-08-09 Eveready Battery Company, Inc. Method of forming an electrode casing for an alkaline electrochemical cell with reduced gassing
US8318340B2 (en) 2006-11-01 2012-11-27 Eveready Battery Company, Inc. Alkaline electrochemical cell with reduced gassing
EP2641292A4 (en) * 2010-11-17 2016-11-02 Luvata Appleton Llc Alkaline collector anode
WO2024080136A1 (en) * 2022-10-12 2024-04-18 東洋鋼鈑株式会社 Surface-treated metal sheet for battery

Cited By (17)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPH0275160A (en) * 1988-09-09 1990-03-14 Yuasa Battery Co Ltd Zinc electrode
JPH0315156A (en) * 1988-12-01 1991-01-23 Yuasa Battery Co Ltd Zinc electrode plate for secondary battery
US4992343A (en) * 1989-08-17 1991-02-12 Eveready Battery Company, Inc. Lead-containing anode current collector for alkaline cells
US5112705A (en) * 1989-08-17 1992-05-12 Eveready Battery Company, Inc. Coated anode current collector for alkaline cells
US5348816A (en) * 1991-06-11 1994-09-20 Fuji Electrochemical Co., Ltd. Alkaline battery
US5376480A (en) * 1991-06-11 1994-12-27 Fuji Electrochemical Co., Ltd. Alkaline battery
JPH0785877A (en) * 1993-09-10 1995-03-31 Toshiba Battery Co Ltd Button type alkaline battery
JPH0794154A (en) * 1993-09-21 1995-04-07 Hitachi Maxell Ltd Alkaline button battery
EP0801432A1 (en) * 1996-04-12 1997-10-15 Rayovac Corporation Rechargeable alkaline electrochemical cell
US6602629B1 (en) 2000-05-24 2003-08-05 Eveready Battery Company, Inc. Zero mercury air cell
US7632605B2 (en) 2005-04-29 2009-12-15 Eveready Battery Co., Inc. Alkaline cell anode casing
US7993508B2 (en) 2006-11-01 2011-08-09 Eveready Battery Company, Inc. Method of forming an electrode casing for an alkaline electrochemical cell with reduced gassing
US8318340B2 (en) 2006-11-01 2012-11-27 Eveready Battery Company, Inc. Alkaline electrochemical cell with reduced gassing
US8444840B2 (en) 2006-11-01 2013-05-21 Eveready Battery Company, Inc. Method of forming an electrode casing for an alkaline electrochemical cell with reduced gassing
EP2641292A4 (en) * 2010-11-17 2016-11-02 Luvata Appleton Llc Alkaline collector anode
US9601767B2 (en) 2010-11-17 2017-03-21 Luvata Appleton Llc Alkaline collector anode
WO2024080136A1 (en) * 2022-10-12 2024-04-18 東洋鋼鈑株式会社 Surface-treated metal sheet for battery

Similar Documents

Publication Publication Date Title
EP0172255B1 (en) Zinc alkaline battery
JPS6459769A (en) Negative current collector for zinc-alkaline battery
JP3215448B2 (en) Zinc alkaline battery
US4092462A (en) Electrode grids for lead accumulators
JP3215446B2 (en) Zinc alkaline battery
JP3215447B2 (en) Zinc alkaline battery
JP3081336B2 (en) Non-aqueous electrolyte secondary battery
AU594661B2 (en) Cell corrosion reduction
US3881953A (en) Battery electrode grids and method of making same from a lead-calcium-lithium-tin alloy
JPS6459768A (en) Negative current collector for zinc-alkaline battery
US3617384A (en) Zinc alkaline secondary cell
JP2832228B2 (en) Zinc alloy powder for alkaline battery and method for producing the same
JP2832227B2 (en) Zinc alloy powder for alkaline battery and method for producing the same
JPS6164076A (en) Electrochemical battery
JPH0418671B2 (en)
GB1496951A (en) Lead base calcium-tin alloy and use thereof
JPS57170459A (en) Button type alkaline battery
US4253871A (en) Alloys for making electrode supports in lead accumulators
JPS6158164A (en) Zinc alloy powder for negative electrode of nonmercury alkaline battery and its manufacture
KR890002672B1 (en) Zn-alkali battery
JPS5810820B2 (en) alkaline dench
JPS612270A (en) Alkaline battery
JP2832230B2 (en) Zinc alloy powder for alkaline battery and method for producing the same
JP2832229B2 (en) Zinc alloy powder for alkaline battery and method for producing the same
JP2832232B2 (en) Zinc alloy powder for alkaline batteries