BR0004551A - Martelada de choque de laser simultânea sobre dois lados em desvio - Google Patents
Martelada de choque de laser simultânea sobre dois lados em desvioInfo
- Publication number
- BR0004551A BR0004551A BR0004551-9A BR0004551A BR0004551A BR 0004551 A BR0004551 A BR 0004551A BR 0004551 A BR0004551 A BR 0004551A BR 0004551 A BR0004551 A BR 0004551A
- Authority
- BR
- Brazil
- Prior art keywords
- laser shock
- deviation
- sides
- simultaneous laser
- article
- Prior art date
Abstract
Applications Claiming Priority (2)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
US15685099P | 1999-09-30 | 1999-09-30 | |
US09/438,513 US6296448B1 (en) | 1999-09-30 | 1999-11-12 | Simultaneous offset dual sided laser shock peening |
Publications (1)
Publication Number | Publication Date |
---|---|
BR0004551A true BR0004551A (pt) | 2001-10-02 |
Family
ID=26853573
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
BR0004551-9A BR0004551A (pt) | 1999-09-30 | 2000-09-29 | Martelada de choque de laser simultânea sobre dois lados em desvio |
Country Status (7)
Country | Link |
---|---|
US (1) | US6296448B1 (pt) |
EP (1) | EP1088903B1 (pt) |
JP (1) | JP5188657B2 (pt) |
BR (1) | BR0004551A (pt) |
DE (1) | DE60021327T2 (pt) |
PL (1) | PL192741B1 (pt) |
TR (1) | TR200002794A2 (pt) |
Families Citing this family (19)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US6469275B2 (en) | 1999-01-20 | 2002-10-22 | Lsp Technologies, Inc | Oblique angle laser shock processing |
US6479790B1 (en) * | 2000-01-31 | 2002-11-12 | General Electric Company | Dual laser shock peening |
US6541733B1 (en) * | 2001-01-29 | 2003-04-01 | General Electric Company | Laser shock peening integrally bladed rotor blade edges |
US6759626B2 (en) * | 2001-08-01 | 2004-07-06 | L&P Technologies, Inc. | System for laser shock processing objects to produce enhanced stress distribution profiles |
US6570125B2 (en) * | 2001-08-31 | 2003-05-27 | General Electric Company | Simultaneous offset dual sided laser shock peening with oblique angle laser beams |
US6570126B2 (en) * | 2001-08-31 | 2003-05-27 | General Electric Company | Simultaneous offset dual sided laser shock peening using low energy laser beams |
US7109436B2 (en) * | 2003-08-29 | 2006-09-19 | General Electric Company | Laser shock peening target |
US7148448B2 (en) | 2003-10-31 | 2006-12-12 | General Electric Company | Monitored laser shock peening |
US20050194070A1 (en) * | 2004-03-02 | 2005-09-08 | Mannava Seetha R. | Lower fluence boundary oblique laser shock peening |
US7304266B2 (en) * | 2004-12-09 | 2007-12-04 | General Electric Company | Laser shock peening coating with entrapped confinement medium |
US7591057B2 (en) * | 2005-04-12 | 2009-09-22 | General Electric Company | Method of repairing spline and seal teeth of a mated component |
US7687151B2 (en) * | 2005-04-12 | 2010-03-30 | General Electric Company | Overlay for repairing spline and seal teeth of a mated component |
DE102010001287A1 (de) * | 2010-01-27 | 2011-07-28 | Rolls-Royce Deutschland Ltd & Co KG, 15827 | Verfahren und Vorrichtung zur Oberflächenverfestigung von Bliskschaufeln |
US11047017B2 (en) | 2014-09-09 | 2021-06-29 | G.C. Laser Systems, Inc. | Laser ablation devices that utilize beam profiling assemblies to clean and process surfaces |
US9914985B2 (en) * | 2014-09-09 | 2018-03-13 | G.C. Laser Systems, Inc. | Laser ablation and processing methods and systems |
CN104357648B (zh) * | 2014-10-13 | 2017-04-05 | 中国航空工业集团公司北京航空制造工程研究所 | 一种激光冲击强化方法及装置 |
CN105648200A (zh) * | 2016-01-27 | 2016-06-08 | 西安交通大学 | 一种基于光子晶体混强场的激光冲击设备及方法 |
CN106893855B (zh) * | 2017-02-06 | 2018-08-21 | 江苏大学 | 一种涡轮叶片主导边双面异步激光冲击强化方法 |
US11298799B2 (en) | 2018-05-03 | 2022-04-12 | General Electric Company | Dual sided shot peening of BLISK airfoils |
Family Cites Families (18)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US3850698A (en) * | 1972-06-23 | 1974-11-26 | Ind Materials Ltd | Altering material properties |
US4401477A (en) * | 1982-05-17 | 1983-08-30 | Battelle Development Corporation | Laser shock processing |
US4937421A (en) * | 1989-07-03 | 1990-06-26 | General Electric Company | Laser peening system and method |
DE69020581T4 (de) * | 1990-01-11 | 1996-06-13 | Battelle Memorial Institute | Verbesserung von materialeigenschaften. |
US5492447A (en) * | 1994-10-06 | 1996-02-20 | General Electric Company | Laser shock peened rotor components for turbomachinery |
US6215097B1 (en) | 1994-12-22 | 2001-04-10 | General Electric Company | On the fly laser shock peening |
US5591009A (en) | 1995-01-17 | 1997-01-07 | General Electric Company | Laser shock peened gas turbine engine fan blade edges |
US5531570A (en) | 1995-03-06 | 1996-07-02 | General Electric Company | Distortion control for laser shock peened gas turbine engine compressor blade edges |
US5569018A (en) * | 1995-03-06 | 1996-10-29 | General Electric Company | Technique to prevent or divert cracks |
US5674328A (en) * | 1996-04-26 | 1997-10-07 | General Electric Company | Dry tape covered laser shock peening |
US5674329A (en) | 1996-04-26 | 1997-10-07 | General Electric Company | Adhesive tape covered laser shock peening |
US5911890A (en) * | 1997-02-25 | 1999-06-15 | Lsp Technologies, Inc. | Oblique angle laser shock processing |
US5911891A (en) | 1997-09-11 | 1999-06-15 | Lsp Technologies, Inc. | Laser shock peening with tailored multiple laser beams |
US5932120A (en) * | 1997-12-18 | 1999-08-03 | General Electric Company | Laser shock peening using low energy laser |
US6005219A (en) * | 1997-12-18 | 1999-12-21 | General Electric Company | Ripstop laser shock peening |
US5951790A (en) | 1998-06-26 | 1999-09-14 | General Electric Company | Method of monitoring and controlling laser shock peening using an in plane deflection test coupon |
US6200689B1 (en) * | 1998-10-14 | 2001-03-13 | General Electric Company | Laser shock peened gas turbine engine seal teeth |
US5948293A (en) | 1998-12-03 | 1999-09-07 | General Electric Company | Laser shock peening quality assurance by volumetric analysis of laser shock peened dimple |
-
1999
- 1999-11-12 US US09/438,513 patent/US6296448B1/en not_active Expired - Lifetime
-
2000
- 2000-09-22 EP EP00308318A patent/EP1088903B1/en not_active Expired - Lifetime
- 2000-09-22 DE DE60021327T patent/DE60021327T2/de not_active Expired - Lifetime
- 2000-09-28 TR TR2000/02794A patent/TR200002794A2/xx unknown
- 2000-09-29 JP JP2000297787A patent/JP5188657B2/ja not_active Expired - Fee Related
- 2000-09-29 BR BR0004551-9A patent/BR0004551A/pt not_active IP Right Cessation
- 2000-09-29 PL PL342868A patent/PL192741B1/pl not_active IP Right Cessation
Also Published As
Publication number | Publication date |
---|---|
JP5188657B2 (ja) | 2013-04-24 |
DE60021327D1 (de) | 2005-08-25 |
PL342868A1 (en) | 2001-04-09 |
EP1088903A1 (en) | 2001-04-04 |
EP1088903B1 (en) | 2005-07-20 |
TR200002794A2 (tr) | 2001-04-20 |
JP2001252775A (ja) | 2001-09-18 |
DE60021327T2 (de) | 2006-04-20 |
PL192741B1 (pl) | 2006-12-29 |
US6296448B1 (en) | 2001-10-02 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
BR0004551A (pt) | Martelada de choque de laser simultânea sobre dois lados em desvio | |
AR047232A1 (es) | Implante interespinal | |
BR9905366A (pt) | Dispositivo de remodelagem de eletrodo de soldagem | |
PE20030264A1 (es) | Conjunto de elementos de desgaste | |
AR009296A1 (es) | Elemento cortante insertable | |
CO5580730A2 (es) | Cepillo de dientes | |
BR0206370B1 (pt) | processo de corte das bordas de uma fita contìnua de vidro, e, dipositivo de corte de uma fita de vidro contìnua. | |
BR9612083A (pt) | Processo de junção ou soldagem de pelo menos duas partes sólidas entre si, união entre um cabo e um objeto oco cilíndrico, cabo supercondutor, e, aparelho para conformação magnética pulsante. | |
BR0100222A (pt) | Martelada de impacto duplo a laser | |
BR0304631A (pt) | Dispositivo em uma coluna de processo de engenharia | |
SE0100251D0 (sv) | Verktygshållare | |
ES2187906T3 (es) | Portaequipajes para un vehiculo automovil equipado con una baja fija. | |
FR2779154B1 (fr) | Procede d'amplification d'au moins une sequence nucleotidique particuliere et amorces de mise en oeuvre | |
BR9912925A (pt) | Método para unir um elo de corrente articulada | |
EA200500005A1 (ru) | Способ лечения повреждения, вызванного реперфузией после ишемии, с использованием антагонистов рецептора аденозина | |
DE60115310D1 (de) | Vorrichtung zur Trennung der Befestigungspunkte, die zwei Ränder einer Schnittlinie verbinden | |
IT1319671B1 (it) | Processo per la preparazione di (s)-n,n'-bis(2-idrossi-1-(idrossimetil)etil)-5-((2-idrossi-1-ossopropil)ammino) | |
PT1128929E (pt) | Processo e dispositivo para o fabrico de placas metalicas soldadas | |
FI20031135A (fi) | Jousikuormitettu kiilamainen pääteliitin, jossa on elementit yhteen kytkemiseksi ja johdinpitimen leukojen siirtymisen estämiseksi | |
SE9900794L (sv) | Verktyg | |
ES2269065T3 (es) | Herramienta con arranque de virutas. | |
PE20000487A1 (es) | Un metodo para aumentar la longitud de una sarta de perforacion, de un elemento de sarta de perforacion y de un miembro de acoplamiento | |
ITMC20020011A1 (it) | Metodo e relativo impianto per l'incisione laser di lastre o cilindricalcografici. | |
SE0100250L (sv) | Verktygshållare | |
RU2221914C2 (ru) | Способ разделки рельс |
Legal Events
Date | Code | Title | Description |
---|---|---|---|
B09A | Decision: intention to grant [chapter 9.1 patent gazette] | ||
B16A | Patent or certificate of addition of invention granted [chapter 16.1 patent gazette] |
Free format text: PRAZO DE VALIDADE: 20 (VINTE) ANOS CONTADOS A PARTIR DE 29/09/2000, OBSERVADAS AS CONDICOES LEGAIS. |
|
B24C | Patent annual fee: request for for restoration |
Free format text: REFERENTE A 8A, 9A, 10A E 11A ANUIDADE(S). |
|
B24H | Lapse because of non-payment of annual fees (definitively: art 78 iv lpi) | ||
B24F | Patent annual fee: publication cancelled |
Free format text: ANULADA A PUBLICACAO CODIGO 24.8 NA RPI NO 2258 DE 15/04/2014 POR TER SIDO INDEVIDA. |
|
B21F | Lapse acc. art. 78, item iv - on non-payment of the annual fees in time |
Free format text: REFERENTE AS 8A, 9A, 10A E 11A ANUIDADES. |
|
B24J | Lapse because of non-payment of annual fees (definitively: art 78 iv lpi, resolution 113/2013 art. 12) |
Free format text: EM VIRTUDE DA EXTINCAO PUBLICADA NA RPI 2606 DE 15-12-2020 E CONSIDERANDO AUSENCIA DE MANIFESTACAO DENTRO DOS PRAZOS LEGAIS, INFORMO QUE CABE SER MANTIDA A EXTINCAO DA PATENTE E SEUS CERTIFICADOS, CONFORME O DISPOSTO NO ARTIGO 12, DA RESOLUCAO 113/2013. |