Prior art keywords
melts
alkaline
nitrite
alkaline substances
oxides
Prior art date
Application number
Other languages
English (en)
French (fr)
Publication of BE455237A publication Critical patent/BE455237A/fr

Links

Classifications

    • CCHEMISTRY; METALLURGY
    • C21METALLURGY OF IRON
    • C21DMODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING
    • C21D1/00General methods or devices for heat treatment, e.g. annealing, hardening, quenching or tempering
    • C21D1/56General methods or devices for heat treatment, e.g. annealing, hardening, quenching or tempering characterised by the quenching agents
    • C21D1/607Molten salts

Landscapes

  • Chemical & Material Sciences (AREA)
  • Engineering & Computer Science (AREA)
  • Physics & Mathematics (AREA)
  • Thermal Sciences (AREA)
  • Crystallography & Structural Chemistry (AREA)
  • Mechanical Engineering (AREA)
  • Materials Engineering (AREA)
  • Metallurgy (AREA)
  • Organic Chemistry (AREA)
  • Anti-Oxidant Or Stabilizer Compositions (AREA)
BE455237D BE455237A (enEXAMPLES)

Publications (1)

Publication Number Publication Date
BE455237A true BE455237A (enEXAMPLES)

Family

ID=109199

Family Applications (1)

Application Number Title Priority Date Filing Date
BE455237D BE455237A (enEXAMPLES)

Country Status (1)

Country Link
BE (1) BE455237A (enEXAMPLES)

Similar Documents

Publication Publication Date Title
US4174962A (en) Filled tubular article for controlled insertion into molten metal
JP2571561B2 (ja) 金属及び合金を精錬するための処理方法
BE455237A (enEXAMPLES)
RU2375462C2 (ru) Проволока для внепечной обработки металлургических расплавов
Huang et al. Effect of Ti Addition on Early-Stage Wetting Behavior Between Zn-25Sn-x Ti Solder and Cu
RU2211872C1 (ru) Алюминиево-скандиевая лигатура для производства алюминиевых и магниевых сплавов
US1997340A (en) Lithium silicon composition
Vincze et al. Examination of the eutectic modifying effect of Sr on an Al-Si-Mg-Cu alloy using various technological parameters
WO1993015238A1 (en) Method of flameproofing molten magnesium material, and alloy thereof
FR2697030A1 (fr) Procédé de production d'alliages de magnésium de haute pureté et alliage ainsi obtenu.
FR2873718A1 (fr) Procede de formation d'une couche de conversion sur un produit en alliage d'aluminium destine a etre brase
US1020512A (en) Zinc and method of purifying and improving the same.
CN1208483C (zh) 通过加钙-镁合金从熔融铅中除去铋的方法
JPH02175853A (ja) ガルバナイジング浴組成物
RU2223345C2 (ru) Способ боросилицирования стальных изделий
SU1122721A1 (ru) Флюс дл рафинировани цинковых сплавов
US3997340A (en) Method of preparing an aluminum-silicon composite
US2893114A (en) Hot working of metals
BE1007952A6 (fr) Procede d'enrichissement de poussieres siderurgiques.
SU476115A1 (ru) Сварочна проволока
SU1723174A1 (ru) Модификатор дл чугуна
BE501141A (enEXAMPLES)
US2507713A (en) Fluxing process for magnesium alloys
BE434156A (fr) Procede pour traiter les metaux et notamment ameliore leur resistance a la corrosion
SU389140A1 (enEXAMPLES)