ATE77658T1 - Verschleissfestes gusseisen mit hohem phosphorgehalt. - Google Patents

Verschleissfestes gusseisen mit hohem phosphorgehalt.

Info

Publication number
ATE77658T1
ATE77658T1 AT88870003T AT88870003T ATE77658T1 AT E77658 T1 ATE77658 T1 AT E77658T1 AT 88870003 T AT88870003 T AT 88870003T AT 88870003 T AT88870003 T AT 88870003T AT E77658 T1 ATE77658 T1 AT E77658T1
Authority
AT
Austria
Prior art keywords
cast iron
phosphorus content
high phosphorus
wear resistant
resistant cast
Prior art date
Application number
AT88870003T
Other languages
English (en)
Inventor
Herman Dehon
Original Assignee
Abex Rail Sa
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Family has litigation
First worldwide family litigation filed litigation Critical https://patents.darts-ip.com/?family=3882504&utm_source=google_patent&utm_medium=platform_link&utm_campaign=public_patent_search&patent=ATE77658(T1) "Global patent litigation dataset” by Darts-ip is licensed under a Creative Commons Attribution 4.0 International License.
Application filed by Abex Rail Sa filed Critical Abex Rail Sa
Application granted granted Critical
Publication of ATE77658T1 publication Critical patent/ATE77658T1/de

Links

Classifications

    • CCHEMISTRY; METALLURGY
    • C22METALLURGY; FERROUS OR NON-FERROUS ALLOYS; TREATMENT OF ALLOYS OR NON-FERROUS METALS
    • C22CALLOYS
    • C22C37/00Cast-iron alloys

Landscapes

  • Chemical & Material Sciences (AREA)
  • Engineering & Computer Science (AREA)
  • Materials Engineering (AREA)
  • Mechanical Engineering (AREA)
  • Metallurgy (AREA)
  • Organic Chemistry (AREA)
  • Refinement Of Pig-Iron, Manufacture Of Cast Iron, And Steel Manufacture Other Than In Revolving Furnaces (AREA)
  • Braking Arrangements (AREA)
  • Meat, Egg Or Seafood Products (AREA)
  • Lubricants (AREA)
AT88870003T 1987-02-05 1988-01-14 Verschleissfestes gusseisen mit hohem phosphorgehalt. ATE77658T1 (de)

Applications Claiming Priority (2)

Application Number Priority Date Filing Date Title
BE8700085A BE1000292A3 (fr) 1987-02-05 1987-02-05 Fonte a haute teneur en phosphore resistant a l'usure.
EP88870003A EP0277931B2 (de) 1987-02-05 1988-01-14 Verschleissfestes Gusseisen mit hohem Phosphorgehalt

Publications (1)

Publication Number Publication Date
ATE77658T1 true ATE77658T1 (de) 1992-07-15

Family

ID=3882504

Family Applications (1)

Application Number Title Priority Date Filing Date
AT88870003T ATE77658T1 (de) 1987-02-05 1988-01-14 Verschleissfestes gusseisen mit hohem phosphorgehalt.

Country Status (8)

Country Link
EP (1) EP0277931B2 (de)
AT (1) ATE77658T1 (de)
BE (1) BE1000292A3 (de)
DE (1) DE3872262T2 (de)
DK (1) DK173189B1 (de)
ES (1) ES2032602T5 (de)
GR (2) GR3005698T3 (de)
NO (1) NO170989C (de)

Families Citing this family (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
KR0130481B1 (ko) * 1993-02-03 1998-04-10 가나이 쯔도무 엘리베이터용 비상정지장치 및 엘리베이터
ES2321664T3 (es) * 2007-03-07 2009-06-09 Eisenwerk Arnstadt Gmbh Hierro colado para la produccion de piezas componentes para dispositivos de frenos de friccion y procedimiento para la produccion del hierro colado.
DE102015007229A1 (de) 2015-06-03 2016-12-08 Anstatt Schienenfahrzeuge-Kraftwerksanlagenbau Gmbh Metallurgisches Recycling von Rest-, Anfall- und Abfallstoffen

Family Cites Families (8)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US1527165A (en) * 1923-03-28 1925-02-24 Bauer Bros Co Alloy
US1690352A (en) * 1927-06-11 1928-11-06 Harry M Williams Heat-resisting alloy
US3193383A (en) * 1962-11-14 1965-07-06 Union Carbide Corp Iron base alloy
FR1528123A (fr) * 1966-05-09 1968-06-07 Albright & Wilson Mfg Ltd Alliages de fer à haute teneur en phosphore
GB1238646A (de) * 1967-07-07 1971-07-07
JPS516608B1 (de) * 1971-04-05 1976-03-01
GB1411216A (en) * 1971-07-13 1975-10-22 Albright & Wilson Casting iron alloys
US4352416A (en) * 1977-01-18 1982-10-05 Abex Corp. Cast iron railroad brake shoes

Also Published As

Publication number Publication date
ES2032602T5 (es) 2000-12-16
EP0277931B2 (de) 2000-08-30
GR3034788T3 (en) 2001-02-28
DE3872262D1 (de) 1992-07-30
GR3005698T3 (de) 1993-06-07
NO170989C (no) 1993-01-06
DK173189B1 (da) 2000-03-13
EP0277931A2 (de) 1988-08-10
NO170989B (no) 1992-09-28
NO880496D0 (no) 1988-02-04
DK56488D0 (da) 1988-02-04
BE1000292A3 (fr) 1988-10-11
DE3872262T2 (de) 1992-12-03
EP0277931A3 (en) 1988-09-07
DK56488A (da) 1988-08-06
EP0277931B1 (de) 1992-06-24
ES2032602T3 (es) 1993-02-16
NO880496L (no) 1988-08-08

Similar Documents

Publication Publication Date Title
ATE77658T1 (de) Verschleissfestes gusseisen mit hohem phosphorgehalt.
DE3862767D1 (de) Gusseisen zur fertigung von bremstrommeln.
ATE14455T1 (de) Verfahren zur herstellung von gusseisen mit vermicular-graphit und nach diesem verfahren hergestelltes gusseisen.
Dehon Wear-resistant cast iron with a high phosphorus content
FR2564342B1 (fr) Masselotte d'alimentation pour la production de pieces de fonderie en fonte de fer, notamment
JPS5582829A (en) Brake disc and its manufacturing method
Muradov et al. Improvement of the Wear Resistance of Cast Iron for Manufacturing Parts Used in Refrigerators
SE8701615L (sv) Kokillomroerare
ATE70858T1 (de) Kupferlegierung.
Melamed Effects of the Chemical Composition on Properties of H. S. Cast Iron Pipes Produced by Semicontinuous Casting
Szatmari The Properties of Gray Cast Iron Produced by Continuous Casting
BR8400402A (pt) Maquina de lingotamento continuo para ferro ligas ou ferro fundido
Riposan et al. Contributions to the study of vermicular graphite cast irons
ATE31081T1 (de) Verfahren zur herstellung von mit bor legierten staehlen.
GB1432176A (en) Cast-iron for making brake shoes
FR2388617A1 (fr) Procede de coulee de matieres metalliques fondues
Hummer Assessment of Shrinkage Tendency of Ductile Iron Melts by Reference to Cooling and Dilatation Curves
Rudyuk et al. Structure Formation and Characteristics of Copper-Containing Nodular Cast Irons
FR2562187B1 (fr) Indicateur d'usure, de preference pour plaquettes de frein a disque
Komatsu The Effect of Silicon Content on the Fracture Toughness of Ferritic Spheroidal Graphite Cast Iron
Lekakh et al. The Oxygen Activity in the Liquid Irons and Their Deoxidation
Petrichenko et al. High-Strength Cast Iron Castings Production in Lined Chill Molds With Nodularizing Treatment in the Mold
Henning Alloy Selection for Cupola Melting.--II
Orths Quality Owing to Reliability
Wolfsgruber Experiences With Long-Time Innoculants for Induction Melting of Cast Iron

Legal Events

Date Code Title Description
UEP Publication of translation of european patent specification
UEP Publication of translation of european patent specification
EELA Cancelled due to lapse of time