WO2020186542A1 - Procédé de fabrication d'un film d'alignement et film d'alignement - Google Patents

Procédé de fabrication d'un film d'alignement et film d'alignement Download PDF

Info

Publication number
WO2020186542A1
WO2020186542A1 PCT/CN2019/079662 CN2019079662W WO2020186542A1 WO 2020186542 A1 WO2020186542 A1 WO 2020186542A1 CN 2019079662 W CN2019079662 W CN 2019079662W WO 2020186542 A1 WO2020186542 A1 WO 2020186542A1
Authority
WO
WIPO (PCT)
Prior art keywords
area
alignment film
substrate
inkjet printing
single drop
Prior art date
Application number
PCT/CN2019/079662
Other languages
English (en)
Chinese (zh)
Inventor
赵永超
Original Assignee
深圳市华星光电半导体显示技术有限公司
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 深圳市华星光电半导体显示技术有限公司 filed Critical 深圳市华星光电半导体显示技术有限公司
Publication of WO2020186542A1 publication Critical patent/WO2020186542A1/fr

Abstract

L'invention porte sur un procédé de fabrication d'un film d'alignement et sur un film d'alignement. Le procédé de fabrication d'un film d'alignement comprend la fourniture d'un substrat ayant une première région, une deuxième région et une troisième région agencées séquentiellement dans une direction vers l'extérieur ; lors de l'éjection d'une solution de film d'alignement sur le substrat, la configuration du volume d'une seule goutte de la solution de film d'alignement projetée sur la première région pour qu'elle soit inférieure au volume d'une seule goutte de la solution de film d'alignement projetée sur la seconde région et la configuration du volume d'une seule goutte de la solution de film d'alignement projetée sur la première région pour qu'elle soit supérieure au volume d'une seule goutte de la solution de film d'alignement projetée sur la troisième région, formant ainsi, sur le substrat, un film d'alignement ayant une région de halo plus petite et une uniformité d'épaisseur élevée. L'invention peut résoudre le problème de luminosité non uniforme à la périphérie.
PCT/CN2019/079662 2019-03-18 2019-03-26 Procédé de fabrication d'un film d'alignement et film d'alignement WO2020186542A1 (fr)

Applications Claiming Priority (2)

Application Number Priority Date Filing Date Title
CN201910205041.7A CN109765730B (zh) 2019-03-18 2019-03-18 配向膜的制作方法及配向膜
CN201910205041.7 2019-03-18

Publications (1)

Publication Number Publication Date
WO2020186542A1 true WO2020186542A1 (fr) 2020-09-24

Family

ID=66459463

Family Applications (1)

Application Number Title Priority Date Filing Date
PCT/CN2019/079662 WO2020186542A1 (fr) 2019-03-18 2019-03-26 Procédé de fabrication d'un film d'alignement et film d'alignement

Country Status (2)

Country Link
CN (1) CN109765730B (fr)
WO (1) WO2020186542A1 (fr)

Families Citing this family (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN110308593B (zh) * 2019-06-12 2024-02-27 惠科股份有限公司 一种配向膜的制作方法
CN114005946B (zh) * 2021-09-06 2024-01-19 上海和辉光电股份有限公司 一种有机膜层结构及其制备方法
CN114779533A (zh) * 2022-04-11 2022-07-22 Tcl华星光电技术有限公司 配向膜及其制备方法

Citations (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN103091904A (zh) * 2013-01-25 2013-05-08 合肥京东方光电科技有限公司 一种显示面板的制作方法
US20150212373A1 (en) * 2014-01-28 2015-07-30 Japan Display Inc. Liquid crystal display device
CN106918954A (zh) * 2017-05-10 2017-07-04 京东方科技集团股份有限公司 一种配向膜制备方法、显示基板及显示面板
CN107215114A (zh) * 2016-03-21 2017-09-29 三星显示有限公司 控制膜厚度分布的喷墨印刷方法及制造显示装置的方法

Family Cites Families (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP4148021B2 (ja) * 2003-05-20 2008-09-10 セイコーエプソン株式会社 配向膜の液滴吐出方法、電気光学パネルの製造方法、電子機器の製造方法、プログラム及び配向膜の液滴吐出装置
JP4609472B2 (ja) * 2007-10-03 2011-01-12 セイコーエプソン株式会社 液滴吐出装置およびその製造方法
CN203012303U (zh) * 2012-08-01 2013-06-19 北京京东方光电科技有限公司 一种新型转印板
CN103149739B (zh) * 2013-03-05 2015-09-02 合肥京东方光电科技有限公司 取向膜制备方法及系统
KR20190018267A (ko) * 2017-08-14 2019-02-22 주식회사 대호무역상사 외곽부 망점 약화 방지판 설계 방법

Patent Citations (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN103091904A (zh) * 2013-01-25 2013-05-08 合肥京东方光电科技有限公司 一种显示面板的制作方法
US20150212373A1 (en) * 2014-01-28 2015-07-30 Japan Display Inc. Liquid crystal display device
CN107215114A (zh) * 2016-03-21 2017-09-29 三星显示有限公司 控制膜厚度分布的喷墨印刷方法及制造显示装置的方法
CN106918954A (zh) * 2017-05-10 2017-07-04 京东方科技集团股份有限公司 一种配向膜制备方法、显示基板及显示面板

Also Published As

Publication number Publication date
CN109765730A (zh) 2019-05-17
CN109765730B (zh) 2020-08-04

Similar Documents

Publication Publication Date Title
JP2001117105A (ja) 液晶表示装置の製造方法
WO2020186542A1 (fr) Procédé de fabrication d'un film d'alignement et film d'alignement
WO2017173672A1 (fr) Panneau d'affichage à cristaux liquides et procédé de traitement de cellule associé
US9346248B2 (en) Liquid crystal sealant forming device and display panel assembly apparatus using the same
CN105457843A (zh) 光阻涂布装置及光阻涂布方法
CN108803125A (zh) 液晶面板及其制作方法
US6738124B2 (en) Method for fabricating liquid crystal display panel
US10203563B2 (en) Forming methods of liquid crystal layers, liquid crystal panels, and liquid crystal dripping devices
WO2014029147A1 (fr) Procédé pour revêtir un panneau d'affichage à cristaux liquides avec du polyimide
WO2020082718A1 (fr) Procédé de fabrication d'agent d'étanchéité et panneau d'affichage
WO2019100485A1 (fr) Substrat de film couleur, écran d'affichage et procédé de préparation de substrat de film couleur
WO2020186561A1 (fr) Procédé de fabrication de panneau d'affichage à cristaux liquides
US20130141677A1 (en) LCD, LCD Substrate and LCD Manufacturing Method
WO2020019469A1 (fr) Panneau d'affichage à cristaux liquides et son procédé de fabrication
US9144134B2 (en) Method for coating polyimide on liquid crystal display panel
KR101777134B1 (ko) 액정 표시 패널의 제조방법
KR20040077072A (ko) 액정표시소자의 배향막 형성장치 및 이를 이용한 배향막형성방법
WO2016061834A1 (fr) Procédé et appareil permettant l'application d'un revêtement de polyimide
KR100919204B1 (ko) 액정표시소자의 배향막 형성장치 및 이를 이용한 배향막형성방법
KR101127835B1 (ko) 액정 적하 장치 및 이를 이용한 액정 적하 방법
US11592714B2 (en) Method of coating polyimide film and method of fabricating display panel using same
US20210333644A1 (en) Display panel and manufacturing method for display panel
KR101671173B1 (ko) 액정표시장치용 액정분사장치 및 이를 이용한 액정층 형성방법
US20130300964A1 (en) Liquid Crystal Display Device and Manufacturing Method Thereof
KR20040079142A (ko) 액정표시장치 및 그 제조방법

Legal Events

Date Code Title Description
121 Ep: the epo has been informed by wipo that ep was designated in this application

Ref document number: 19919942

Country of ref document: EP

Kind code of ref document: A1

NENP Non-entry into the national phase

Ref country code: DE

122 Ep: pct application non-entry in european phase

Ref document number: 19919942

Country of ref document: EP

Kind code of ref document: A1