WO2017138422A1 - 石炭成型燃料の製造方法 - Google Patents

石炭成型燃料の製造方法 Download PDF

Info

Publication number
WO2017138422A1
WO2017138422A1 PCT/JP2017/003693 JP2017003693W WO2017138422A1 WO 2017138422 A1 WO2017138422 A1 WO 2017138422A1 JP 2017003693 W JP2017003693 W JP 2017003693W WO 2017138422 A1 WO2017138422 A1 WO 2017138422A1
Authority
WO
WIPO (PCT)
Prior art keywords
coal
molded body
briquette
burr
fuel
Prior art date
Application number
PCT/JP2017/003693
Other languages
English (en)
French (fr)
Inventor
一浩 ▲虫▼合
記央 山田
宏昭 工藤
孝 本郷
隆彦 寺田
Original Assignee
宇部興産株式会社
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 宇部興産株式会社 filed Critical 宇部興産株式会社
Priority to JP2017566897A priority Critical patent/JPWO2017138422A1/ja
Publication of WO2017138422A1 publication Critical patent/WO2017138422A1/ja

Abstract

石炭粒子を成型し、成型金型の型が転写されたブリケット部およびバリ部を有し且つ前記バリ部によって連結された前記ブリケット部からなる板状成型体と、1つのブリケット部にバリ部が付着したブリケット単体を含む第1中間成型体を得る成型工程と、前記第1中間成型体を破砕して、前記板状成型体のバリ部を分割することにより前記ブリケット単体からなる第2中間成型体を得る破砕工程と、前記第2中間成型体同士を接触させ、摩擦によって前記バリ部を研磨して石炭成型燃料を得る研磨工程とを備える製造方法によって、低コストで粉化が抑制された石炭成型燃料が提供される。

Description

石炭成型燃料の製造方法
 本発明は、石炭を粉砕後成型した石炭成型燃料の製造方法に関する。
 従来、特許文献1にあっては、石炭を破砕した後に乾燥、粉砕して石炭粒子を得るとともに、この石炭粒子を成型して得られた成型体としての石炭成型燃料であって、石炭粒子の平均粒子径および水分、石炭成型燃料の見掛密度を規定することで強度を確保する技術が開示されている。
WO2015/098935
 しかしながら上記特許文献1にあっては、成型後の粉化対策について有効な解決法は記載されていない。
 本発明は上記問題を解決するためになされたものであり、その目的とするところは、低コストで強度を確保し、粉化が抑制された石炭成型燃料を提供することにある。
 本発明では、石炭粒子を成型し、第1中間成型体を得る成型工程と、前記第1中間成型体を破砕して第2中間成型体を得る破砕工程と、前記第2中間成型体を研磨して石炭成型燃料を得る研磨工程とを備える石炭成型燃料の製造方法であって、前記第1中間成型体は、成型金型の型が転写されたブリケット部およびバリ部を有し、前記バリ部によって連結された前記ブリケット部からなる板状成型体と、1つのブリケット部にバリ部が付着したブリケット単体からなり、前記破砕工程では、前記板状成型体のバリ部を分割することにより前記ブリケット単体からなる第2中間成型体を得ることを特徴とする。
 本発明によれば、低コストで強度が確保され粉化が抑制された石炭成型燃料を提供できる。
実施形態1におけるプロセスフローである。 第1中間成型体(板状成型体100)、第2中間成型体200、および石炭成型燃料300を示す図である。 実施形態2におけるプロセスフローである。 回転式篩を示す図である。 石炭成型燃料300の圧壊強度を示すグラフである。 石炭成型燃料300の粉化特性を示す図である。
[実施形態1]
 図1は実施形態1におけるプロセスフロー、図2は第1中間成型体(板状成型体100)、第2中間成型体200、および石炭成型燃料300を示す図である。実施形態1における製造工程は、石炭粒子1を成型工程10で成型して第1中間成型体(板状成型体100)を得た後、破砕工程20で破砕し、研磨工程30において研磨することで石炭成型燃料300を得るものである。成型工程10では公知の手法が用いられており、粉砕された石炭をブリケットマシンやコンパクター等の成型機を用いて成型する。なお成型は1回(1段成型)のみでもよいし、一旦成型された成型体を破砕して再度成型を行ってもよい(2段成型)。公知の成型手法としては例えばWO2015/098935に記載の手法が挙げられ、WO2015/098935に記載された金型の形状、大きさおよびロール間距離等の条件は、全て本願の第1中間体の製造に適している。例えば、ブリケットの縦横の最大長が5~40mm、最大厚みが数mm(例えば2~20mm)となるようなポケットサイズ、バリ部に対応するロール間距離が数mm以下(例えば、1mm以下~2mm以下)のように設定することができる。
 本発明の成型工程10では第1中間成型体が得られる。第1中間成型体は、成型機の金型が転写されたブリケット部110とバリ部120とからなる。通常、第1中間成型体の大部分は、複数個のブリケット部110がバリ部120によって連結された板状の形状(板状成型体100)となる。成型工程10で得られる第1中間成型体には、通常、バリ部120によって連結されず1つのブリケット部110のみからなるブリケット単体200も含まれる。即ち、第1中間成型体は、通常、複数個のブリケット部とそれを連結するバリ部からなる板状成型体と、1つのブリケット部にバリ部が付着したブリケット単体200との混合物である。
 破砕工程20では、ブリケット部110を連結するバリ部120をせん断力および衝撃力によって分割し、第2中間成型体(ブリケット単体)200を得る。この破砕工程20における装置としてはハンマクラッシャ、ロールプレス、ジョークラッシャなどが用いられる。
 研磨工程30では第2中間成型体200を研磨し、バリ部120を除去して石炭成型燃料300を得る。主に第2中間成型体200同士を接触させて摩擦によりバリ部120を除去し、石炭成型燃料300の強度を向上させ、粉化を低減するものである。第2中間成型体200同士の接触に加えて、装置との接触によってバリ部120の除去が生じてもよい。研磨工程30の装置としては、第2中間成型体200同士および第2中間成型体200と装置との接触および摩擦が、バリ部が除去される程度の強度で生じるような装置であれば特に限定されない。例えば、回転式篩(トロンメル)、磨さい機、研磨機、振動ぶるいなどが用いられる。篩を用いる場合、篩下の微粉は成型工程10にリサイクルされる。篩上には石炭成型燃料300が残り、これをハンドリングする。また、バリ部の除去に磨さい機、研磨機等を用いる場合は、これらの装置による処理後に、主としてバリ部に由来する粉体および/または小粒子を篩等により除いて石炭成型燃料300を得ることが好ましい。
 石炭成型燃料300は、破砕工程20および研磨工程30にて、成型体に含まれる低強度の箇所が除去されているため、ハンドリング時に生じる粉末の量が第2中間成型体200と比べ非常に少なく、既設の石炭ハンドリング設備にて、石炭と同様の運用が可能である。また、石炭成型燃料300は、高密度のため(比表面積が小さいため)、第2中間成型体200と比べ酸化反応による自然発熱リスクも軽減されている。
[実施形態2]
 図3は実施形態2におけるプロセスフローである。実施形態2では、図4に示す回転式篩(トロンメル)31を用いて破砕工程20と研磨工程30を同時に行う。即ち、第1中間成型体(板状成型体100)が粉砕された第2中間成型体200は、同一工程において(通常、外部に取り出されることなく)、引き続き研磨されて石炭成型燃料300となる。図4では省略されているが、回転式篩31の外周には網が設けられて篩となっている。篩下の微粉は実施形態1と同様に成型工程10に戻される。実施形態2においても、実施形態1と同様の効果が得られる。
 図5は実施形態1および/または実施形態2により得られた石炭成型燃料300の圧壊強度を示すグラフである。JIS Z8841-1993(造粒物の強度試験方法)に記載の「3.1圧壊強度試験方法」に基づき測定した。図5横軸のaは正の定数である。破砕前の第1中間成型体100よりも、破砕および研磨した後の石炭成型燃料300(歩留まり82.9%および76.5%)のほうが強度が高くなっている。
 図6は石炭成型燃料300の粉化特性を示す図である。縦軸は第1中間成型体(板状成型体100)および石炭成型燃料300を2mm篩で分級した際の篩下残分である。第1中間成型体(板状成型体100)よりも、破砕、研磨によりバリ部120が除去された石炭成型燃料300のほうが粉化しにくいことが示される。
 本出願の主要な開示事項は次のとおりである。
(1) 石炭粒子を成型し、第1中間成型体を得る成型工程と、
 前記第1中間成型体を破砕して第2中間成型体を得る破砕工程と、
 前記第2中間成型体を研磨して石炭成型燃料を得る研磨工程と
を備える石炭成型燃料の製造方法であって、
 前記第1中間成型体は、成型金型の型が転写されたブリケット部およびバリ部を有し、前記バリ部によって連結された前記ブリケット部からなる板状成型体と、1つのブリケット部にバリ部が付着したブリケット単体を含み、
 前記破砕工程では、前記板状成型体のバリ部を分割することにより前記ブリケット単体からなる第2中間成型体を得ること
を特徴とする石炭成型燃料の製造方法。
(2) 前記破砕工程では、せん断力と衝撃力により前記バリ部を分割すること
を特徴とする上記(1)に記載の石炭成型燃料の製造方法。
(3) 前記研磨工程では、前記第2中間成型体同士の接触による摩擦によって前記バリ部を研磨することを特徴とする上記(1)または(2)に記載の石炭成型燃料の製造方法。
(4) 前記破砕工程の後に前記研磨工程が行われることを特徴とする上記(1)~(3)のいずれか1項に記載の石炭成型燃料の製造方法。
(5) 前記破砕工程と前記研磨工程は同時に行われることを特徴とする上記(1)~(3)のいずれか1項に記載の石炭成型燃料の製造方法。
 この出願は、2016年2月9日に出願された日本特許出願特願2016-022911を基礎とする優先権を主張し、その開示の全てをここに取り込む。
1 石炭粒子
10 成型工程
20 破砕工程
30 研磨工程
31 回転式篩
100 第1中間成型体(板状成型体)
110 ブリケット部
120 バリ部
200 第2中間成型体(ブリケット単体)
300 石炭成型燃料

Claims (4)

  1.  石炭粒子を成型し、成型金型の型が転写されたブリケット部およびバリ部を有し且つ前記バリ部によって連結された前記ブリケット部からなる板状成型体と、1つのブリケット部にバリ部が付着したブリケット単体を含む第1中間成型体を得る成型工程と、
     前記第1中間成型体を破砕して、前記板状成型体のバリ部を分割することにより前記ブリケット単体からなる第2中間成型体を得る破砕工程と、
     前記第2中間成型体同士を接触させ、摩擦によって前記バリ部を研磨して石炭成型燃料を得る研磨工程と
    を備えることを特徴とする石炭成型燃料の製造方法。
  2.  前記破砕工程では、せん断力と衝撃力により前記バリ部を分割すること
    を特徴とする請求項1に記載の石炭成型燃料の製造方法。
  3.  前記破砕工程の後に前記研磨工程が行われること
    を特徴とする請求項2に記載の石炭成型燃料の製造方法。
  4.  前記破砕工程と前記研磨工程は同時に行われること
    を特徴とする請求項1ないし請求項3のいずれか1項に記載の石炭成型燃料の製造方法。
PCT/JP2017/003693 2016-02-09 2017-02-02 石炭成型燃料の製造方法 WO2017138422A1 (ja)