US20210379851A1 - Tire vulcanization mold and pneumatic tire - Google Patents
Tire vulcanization mold and pneumatic tire Download PDFInfo
- Publication number
- US20210379851A1 US20210379851A1 US17/411,773 US202117411773A US2021379851A1 US 20210379851 A1 US20210379851 A1 US 20210379851A1 US 202117411773 A US202117411773 A US 202117411773A US 2021379851 A1 US2021379851 A1 US 2021379851A1
- Authority
- US
- United States
- Prior art keywords
- mold
- tire
- pneumatic tire
- rubber
- fitting portion
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Abandoned
Abstract
A tire vulcanization mold including a sector mold divided into a plurality of pieces along a circumferential direction of a green tire, the sector mold configured to vulcanization mold a tread portion of the green tire into a predetermined shape, and an upper mold and a lower mold disposed on both sides of the green tire so as to sandwich the green tire therebetween in an axial direction of the green tire, the upper mold and the lower mold configured to vulcanization mold a side portion of the green tire into a predetermined shape. The sector mold has a relief groove in a vicinity of a fitting portion between the sector mold, and the upper mold and the lower mold.
Description
- The application is a Divisional of U.S. patent application Ser. No. 16/356,102, filed on Mar. 18, 2019, which is a Divisional of U.S. patent application Ser. No. 15/730,122, filed on Oct. 11, 2017, which claims priority of Japanese Patent Application No. 2016-244692 filed on Dec. 16, 2016, the content of which is incorporated herein by reference.
- The present invention relates to a tire vulcanization mold and a pneumatic tire.
- In vulcanization molding of a pneumatic tire, two kinds of molds corresponding to molded portions are generally used. One is a mold for molding a tread portion of the tire, which is called a sector mold. The other is a mold for molding a sidewall portion over a shoulder portion of the tire, which is called a side mold. The sector mold is divided into a plurality of pieces and arranged in the circumferential direction of the tire, and the side mold is arranged so as to sandwich the tire from the side. The green tire (raw tire) is subjected to vulcanization molding in a state of being closed by these two kinds of molds, and a pneumatic tire as a product is manufactured.
- For example, JP 63-66206 U discloses a pneumatic tire molded by such a sector mold and a side mold. In the pneumatic tire disclosed in JP 63-66206 U, in order to prevent the rubber from being caught by a mold during molding and to prevent the poor appearance of the tire, a protrusion is provided at the bottom of the lug groove of the tire on the side mold side.
- In the molding of the pneumatic tire disclosed in JP 63-66206 U, a protrusion is provided at the bottom of the lug groove of the tire on the side mold side. However, the position and shape of the protrusion has not been studied in detail so as to suppress rubber from flowing to the fitting portion of the molds. Therefore, there is still room for improvement in the tire vulcanization mold disclosed in JP 63-66206 U.
- An object of the present invention is to provide a tire vulcanization mold capable of suppressing a pneumatic tire from representing a poor appearance which is caused by an event in which the rubber has been caught during molding and a pneumatic tire in which such a poor appearance is suppressed.
- The tire vulcanization mold of the present invention includes a sector mold divided into a plurality of pieces along the circumferential direction of a green tire, the sector mold configured to vulcanization mold the tread portion of the green tire into a predetermined shape, and a pair of side molds disposed on respective sides of the green tire so as to sandwich the green tire therebetween in the axial direction of the green tire, for the side molds configured to vulcanization mold a side portion of the green tire into a predetermined shape, wherein the sector mold has a recess in the vicinity of a fitting portion between the sector mold, and the side molds.
- According to this configuration, when the mold is closed, the rubber of the tire can escape to the recess provided in the sector mold, so that the flow of the rubber to the fitting portion of the mold can be suppressed. Therefore, it is possible to suppress the rubber from being caught by the mold, and it is possible to suppress occurrence of the poor appearance of the pneumatic tire. In particular, the recess is provided in the sector mold instead of the side mold, thereby further suppressing the rubber from being caught. In detail, when the mold is closed, normally the sector mold moves inward in the radial direction of the tire in a state where the side mold is fixed. Therefore, the positional relationship between the side mold and the tire is fixed, and the rubber of the tire flows toward the closing sector mold. Therefore, the recess is provided in the sector mold and the rubber escapes to the recess, thereby suppressing the rubber from being caught in the fitting portion.
- The recess may have a depth of 0.3 mm or more and 0.5 mm or less.
- According to this configuration, the depth of the recess is defined, thereby further suppressing the rubber from being caught, and ensuring the releasability of the mold. Specifically, the depth of the recess is 0.3 mm or more, whereby the rubber in an amount necessary for suppressing the rubber from being caught can escape into the recess. Further, the depth of the recess is 0.5 mm or less, thereby preventing the rubber from deeply entering the recess. Therefore, it is possible to prevent the rubber from becoming difficult to be released from the mold when the mold is opened, that is, it is possible to ensure releasability of the mold.
- The recess may be provided away from the fitting portion by a distance of 0.5 mm or more and 0.8 mm or less.
- According to this configuration, the distance between the recess and the fitting portion is defined, thereby preventing durability of the mold from deteriorating and further suppressing the rubber from being caught. In detail, the recess is 0.5 mm or more away from the fitting portion, whereby the thickness of the sector mold in the vicinity of the fitting portion can be sufficiently ensured. Therefore, it is possible to prevent durability of the sector mold from deteriorating. Since the sector mold contacts the side mold at the fitting portion, and the sector mold is subjected to receive impact upon every molding, it is very effective to be able to prevent durability in the vicinity of the fitting portion of the sector mold from deteriorating. In addition, the recess is provided within a distance of 0.8 mm from the fitting portion, whereby the flow of the rubber to the fitting portion can be suppressed more reliably. If the recess is provided extremely far from the fitting portion, the recess does not affect the flow of the rubber toward the fitting portion, and the effect of suppressing the rubber from being caught at the fitting portion cannot be provided.
- The sector mold may be provided with a projection for forming a lug groove on an outer circumferential surface of the green tire, and the recess may be provided away from the projection by a distance of 0.5 mm or more and 0.8 mm or less.
- According to this configuration, the distance between the recess and the projection is defined, thereby preventing durability of the tire to be manufactured from deteriorating, and sufficiently ensuring an area for arranging the recess in the mold. In detail, the recess is 0.5 mm or more away from the projection, thereby preventing a ridge line from being formed in the vicinity of the lug groove of the tire to be manufactured. If the recess is provided extremely close to the projection, a ridge line is formed in the vicinity of the lug groove in the tire. In that case, since the lug groove and the ridge line form a protruding and recessed relation, the abrasion rate of the tire is increased. Therefore, by preventing the formation of the recess extremely close to the projection, it is possible to prevent the abrasion resistance of the tire from deteriorating, that is, deterioration of the durability of the pneumatic tire can be prevented. If the recess is provided extremely far from the projection, that is, if the recess is provided extremely close to the fitting portion, the area for providing the recess between the fitting portion and the projection is decreased. Therefore, the recess is provided within a distance of 0.8 mm from the projection, whereby the sufficient area for arranging the recess in the mold can be ensured.
- The recesses may be a plurality of grooves in a mesh shape extending in a direction intersecting with both a circumferential direction and a radial direction of the green tire. The recesses may be grooves extending annularly in a circumferential direction of the green tire.
- According to this configuration, the recess is provided so as to extend in a direction intersecting with the flow direction of the rubber (radial direction of the tire) to the fitting portion. Therefore, when the rubber flows to the fitting portion, the rubber stretches across the recess, so that the rubber can reliably escape to the recess. Therefore, the flow of the rubber to the fitting portion can be suppressed, and it is possible to prevent the rubber from being caught. In particular, when the recess is provided in a mesh shape, the rubber can escape in various directions, and it is possible to more reliably suppress the rubber from being caught. Particularly, when the recess is provided in the circumferential direction of the tire, since the recess can be formed by lathe machining or the like, it is easy to process the recess.
- The pneumatic tire according to the present invention includes a protrusion-shaped mold fitting mark located between a tread portion and a side portion, and a protrusion-shaped molding mark provided in the vicinity of and outside of the mold fitting mark.
- According to this configuration, the pneumatic tire is manufactured using the mold having said recess, thereby suppressing the rubber from being caught. Thus, occurrence of poor appearance of the pneumatic tire is suppressed. Therefore, the aesthetic appearance of the tire is maintained. Here, the vicinity of and the outside of the mold fitting mark refer to a range within, for example, 0.8 mm from the mold fitting mark on the radially outer side of the pneumatic tire.
- According to the present invention, it is possible to suppress the rubber from being caught during molding in the tire vulcanization mold, and it is possible to maintain the aesthetic appearance of the pneumatic tire.
- The foregoing and the other features of the present invention will become apparent from the following description and drawings of an illustrative embodiment of the invention in which:
-
FIG. 1 is a partial sectional view of a vulcanization molding machine equipped with a tire vulcanization mold according to an embodiment of the present invention; -
FIG. 2A is an enlarged view of a fitting portion of the tire vulcanization mold ofFIG. 1 ; -
FIG. 2B is a front view of a recess ofFIG. 2A ; -
FIGS. 3A to 3F are partial sectional views showing a clamping operation of the tire vulcanization mold ofFIG. 1 ; -
FIG. 4 is a cross-sectional perspective view of a pneumatic tire manufactured by the tire vulcanization mold ofFIG. 1 ; and -
FIG. 5 is a front view of a recess showing a modification fromFIG. 2B . - Hereinafter, embodiments of the present invention will be described with reference to the accompanying drawings.
-
FIG. 1 shows a state in which atire vulcanization mold 2 according to the present embodiment is attached to avulcanization molding machine 1. Thetire vulcanization mold 2 is attached via a container 6 between anupper plate 3 and anupper platen 4 of thevulcanization molding machine 1, and a lower platen 5. - The
upper plate 3 is fixed to the lower end of a lifting cylinder 7. A liftingrod 8 is disposed at the center of the lifting cylinder 7. Theupper platen 4 is fixed to the lower end of the liftingrod 8. The lifting cylinder 7 and the liftingrod 8 are moved up and down by a driving device (not shown). Theupper plate 3 and theupper platen 4 are configured to be able to move up and down independently. Aflow path 4 a is formed in theupper platen 4. The temperature can be adjusted by the flow of a heat exchange medium (for example, oil) in theflow path 4 a. - As with the
upper platen 4, aflow path 5 a in which the heat exchange medium flows is formed in the lower platen 5. Adjusting the temperature of the heat exchange medium allows thetire vulcanization mold 2 to have a desired vulcanization temperature through theupper platen 4 and the lower platen 5. Abladder unit 9 is disposed at the center of the lower platen 5. - In the
bladder unit 9, abladder 13 is attached to anupper clamp 11 and alower clamp 12 which are fixed to a verticallymovable support shaft 10. Air is supplied to and discharged from a space surrounded by theupper clamp 11, thelower clamp 12, and thebladder 13 by a supply/exhaust device (not shown). Thebladder 13 is inflated toward its outer circumference side by the supply of air, and supports a green tire GT from the inside. Here, the green tire GT indicates a raw tire before being subjected to vulcanization molding. - A container 6 includes a
segment 14, ajacket ring 15, anupper container plate 16, and alower container plate 17. - The
segment 14 is screwed to asector mold 20 of thetire vulcanization mold 2 described later at each of respective pieces. In the present embodiment, thesegment 14 is consisted of nine pieces, and thesector mold 20 is also consisted of nine pieces. The inner surface of thesegment 14 is disposed along the outer surface of thesector mold 20, and its outer surface is constituted by an inclined surface (outer peripheral conical surface) gradually expanding toward the outer diameter side in going downward. Thesegment 14 is reciprocably supported in the radial direction by anupper slide 18. - A
jacket ring 15 has a hollow cylindrical shape. The upper end surface of thejacket ring 15 is fixed to theupper plate 3, and thejacket ring 15 moves up and down according to the lifting action of the lifting cylinder 7. The inner surface of thejacket ring 15 is constituted by an inner peripheral conical surface inclined toward the outer diameter side so as to gradually enlarge its diameter in going toward the lower end of thejacket ring 15. The inner peripheral conical surface of thejacket ring 15 and the outer peripheral conical surface of thesegment 14 slide along the conical surface so as not to be away from each other (for example, by a configuration like a tenon and a dovetail groove). As a result, when thejacket ring 15 descends, the outer peripheral conical surface of thesegment 14 is pressed by the inner peripheral conical surface of thejacket ring 15, and it is possible to move thesegment 14 expanding toward the outer diameter side into a state in which the pieces of thesegment 14 are annularly continuously disposed on the inner diameter side. - The
upper slide 18 is fixed to the undersurface of theupper container plate 16 on the outer peripheral side thereof, and anupper mold 21, which will be described later, is fixed to the undersurface of theupper container plate 16 on the inner peripheral side thereof. Theupper container plate 16 itself is fixed to the undersurface of theupper platen 4. As a result, when the liftingrod 8 moves up and down, theupper mold 21 and the segment 14 (including thesector mold 20 fixed to the segment 14) move up and down together with theupper platen 4 and theupper container plate 16. - The
lower slide 19 is fixed to the top surface of thelower container plate 17 on the outer peripheral side thereof, and alower mold 22, which will be described later, is fixed to the top surface of thelower container plate 17 on the inner peripheral side thereof. On thelower slide 19, thesegment 14 is placed at the time of mold clamping and is supported slidably in the radial direction. Thelower container plate 17 itself is fixed to the top surface of the lower platen 5. - The
tire vulcanization mold 2 includes thesector mold 20, the upper mold (side mold) 21, and the lower mold (side mold) 22. - The
sector mold 20 is a mold for vulcanization molding the tread portion of the tire into a predetermined shape. Thesector mold 20 is made of an aluminum alloy and is divided into a plurality of pieces in the circumferential direction of the tire (nine divisions in this case), and the pieces are continuously disposed in a ring shape in a state where the pieces are moved to the inner diameter side. -
FIG. 2A is an enlarged view of a portion surrounded by a circle C inFIG. 1 , that is,FIG. 2A is an enlarged view of a fitting portion between thesector mold 20 and the upper mold 21 (or the lower mold 22). InFIG. 1 , there are two portions surrounded by a circle C. Since each enlarged view of the two portions differs only in orientation and is identical in shape, the two portions are shown inFIG. 2A by one figure. Hereinafter, the term “fitting portion” refers to a fitting portion between thesector mold 20 and the upper mold 21 (or the lower mold 22). The fitting portion has a recessed shape and has a shape like an open beak. This recessed shape can suppress the rubber from being caught in the fitting portion when the mold is closed. Thesector mold 20 is provided with aprojection 20 a for forming a lug groove on the tire surface in order to improve driveability of the tire to be manufactured and a relief groove (recess) 20 b for suppressing the rubber from being caught. - The
relief groove 20 b is provided at a position, for example, 0.5 mm away from the fitting portion (W1=0.5 mm) and is provided at a position, for example, 0.5 mm away from theprojection 20 a (W2=0.5 mm). A plurality ofrelief grooves 20 b is provided, and in this embodiment, threerelief grooves 20 b are provided. Therelief groove 20 b has, for example, an R portion having a radius of about 1.0 mm with respect to the surface of thesector mold 20. The interval between therelief grooves 20 b is, for example, about 1.0 mm (W3=1.0 mm). As also shown inFIG. 2B seen from the direction of the arrow A inFIG. 2A , therelief groove 20 b of the present embodiment extends in the circumferential direction of the tire, and the sectional shape thereof is a triangular shape. The depth of the relief groove is, for example, about 0.4 mm (D=0.4 mm). InFIG. 2B , in order to clearly show the position of therelief groove 20 b, marking is schematically indicated by oblique lines with respect to therelief groove 20 b. - The
relief groove 20 b has a preferable range of position and shape. Therelief groove 20 b is preferably provided at a position 0.5 mm to 0.8 mm away from the fitting portion, that is, the width W1 preferably satisfies 0.5 mm≅W1≤0.8 mm. Further, therelief groove 20 b is preferably provided at a position 0.5 mm to 0.8 mm away from theprojection 20 a, that is, the width W2 preferably satisfies 0.5 mm≤W2≤0.8 mm. The interval between therelief grooves 20 b is preferably 0.7 mm to 1.3 mm, that is, the width W3 preferably satisfies 0.7 mm≤W3≤1.3 mm. Further, the depth of therelief groove 20 b is preferably 0.3 mm to 0.5 mm, that is, the depth D is preferably 0.3 mm≤D≤0.5 mm. - While the cross-sectional shape of the
relief groove 20 b is preferably a triangular shape, it may be any shape, such as a semicircular shape or a trapezoidal shape, for example. The significance of the preferable range of the position and the shape of therelief groove 20 b will be described later. - As shown in
FIG. 1 , theupper mold 21 and thelower mold 22 are molds for vulcanization molding the side portions of the tire into a predetermined shape. - The
upper mold 21 is formed in an annular shape, and anupper bead ring 23 is fixed to the inner periphery of theupper mold 21. Theupper mold 21 is fixed to theupper container plate 16, and moves up and down as the liftingrod 8 moves up and down. When theupper mold 21 descends, theupper bead ring 23 can hold down the bead portion of the green tire GT. Thereby, a sidewall portion and a bead portion of the tire are formed by the lower inner surface of theupper mold 21 and the undersurface of theupper bead ring 23. - As with the
upper mold 21, thelower mold 22 is formed in an annular shape, and alower bead ring 24 is fixed to the inner peripheral portion of thelower mold 22. -
FIGS. 3A to 3F are partial cross-sectional views showing the mold clamping operation of thetire vulcanization mold 2 of the present embodiment. In the present embodiment, the green tire GT is set in thevulcanization molding machine 1 equipped with thetire vulcanization mold 2 having the above-described configuration. After closing the mold, and the mold is clamped, the vulcanization molding of the green tire GT is performed. - In the mold open state shown in
FIG. 3A , the green tire GT is placed on thelower mold 22 so that the axial direction of the green tire GT directs upward and downward. At this time, the bead portion of the green tire GT on the lower side is aligned with thelower bead ring 24. - As shown in
FIG. 3B , air is then supplied into thebladder 13 to inflate thebladder 13 and hold the inner surface of the green tire GT on the outer surface of thebladder 13. As a result, the green tire GT is supported by thelower bead ring 24 and thebladder 13, and is in a non-contact state with thelower mold 22. - As shown in
FIG. 3C , theupper mold 21 and thesector mold 20 are subsequently lowered by the liftingrod 8 and the lifting cylinder 7. Then, theupper bead ring 23 comes into contact with the bead portion positioned at the upper side of the green tire GT. - As shown in
FIGS. 3D and 3E , subsequently, after the green tire GT is pressed and deformed via the bead portion, theupper mold 21 comes into contact with the green tire GT. When theupper mold 21 descends to the mold clamping completion position, the green tire GT is sandwiched between theupper mold 21 and thelower mold 22. - As shown in
FIG. 3F , the descent by the lifting cylinder 7 is continued even after theupper mold 21 has descended to the mold clamping completion position, and thejacket ring 15 is downwardly moved together with theupper plate 3. As a result, the inner peripheral conical surface of thejacket ring 15 presses the outer peripheral conical surface of thesegment 14. Then, thesector mold 20 fixed to thesegment 14 moves toward the inner diameter side. - The vulcanization molding is performed after the mold clamping is completed as shown in
FIGS. 3A to 3F . After completion of the molding, when thetire vulcanization mold 2 is opened by the reverse motion, the green tire GT becomes a pneumatic tire as a product. -
FIG. 4 shows the pneumatic tire AT manufactured as described above. The pneumatic tire AT includes an annular and linear moldfitting mark 30 formed by a fitting portion between thesector mold 20 and the upper mold 21 (or the lower mold 22), and a protrusion-shaped relief groove mark (molding mark) 31 provided in the vicinity of and the outside of the moldfitting mark 30. Here, the vicinity of and the outside of the moldfitting mark 30 refer to a range within, for example, 0.8 mm from the moldfitting mark 30 on the radially outer side of the pneumatic tire AT. Therelief groove mark 31 is provided between the moldfitting mark 30 and thelug groove 32 in the radial direction of the pneumatic tire AT. InFIG. 4 , three streaks of relief groove marks 31 are shown corresponding to the number of therelief grooves 20 b inFIG. 2B . The number of the relief groove marks 31 to be formed is the same as the number of therelief grooves 20 b. In addition, therelief groove mark 31 has a cross-sectional shape corresponding to that of therelief groove 20 b. Therefore, for example, therelief groove mark 31 formed from therelief groove 20 b with the triangular cross section of this embodiment have a chevron cross-sectional shape. In this way, therelief groove mark 31 is formed corresponding to therelief groove 20 b with respect to dimensions, positions, etc. in addition to the cross-sectional shape. - According to the present embodiment, when the
tire vulcanization mold 2 is closed, the rubber of the tire can escape to therelief groove 20 b provided in thesector mold 20. Thus, it is possible to suppress the rubber from flowing to the fitting portion of thetire vulcanization mold 2. Therefore, it is possible to suppress the rubber from being caught by thetire vulcanization mold 2 and the poor appearance of the pneumatic tire can be prevented. Particularly, therecess 20 b is provided in thesector mold 20 instead of the upper mold 21 (or the lower mold 22), thereby further suppressing the rubber from being caught. In detail, when thetire vulcanization mold 2 is closed as described above, thesector mold 20 moves inward in the radial direction of the tire while the upper mold 21 (or the lower mold 22) is fixed. Since the positional relationship between the upper mold 21 (or the lower mold 22) and the tire is fixed, the rubber of the tire flows toward the closingsector mold 20. Therefore, therecess 20 b is provided in thesector mold 20, and the rubber escapes to therecess 20 b, thereby suppressing the rubber from being caught in the fitting portion. - The depth of the
relief groove 20 b is defined, thereby preventing the rubber from being caught, and ensuring releasability of thetire vulcanization mold 2. Specifically, therelief groove 20 b has a depth of 0.3 mm or more, whereby the rubber in an amount necessary for suppressing the rubber from being caught can escape. Further, therelief groove 20 b has a depth of 0.5 mm or less, thereby preventing the rubber from deeply entering into therelief groove 20 b and becoming difficult to be released from thetire vulcanization mold 2 when themold 2 is opened. - The distance W1 between the
relief groove 20 b and the fitting portion is defined, thereby preventing durability of thetire vulcanization mold 2 from deteriorating, and the rubber from being caught. In detail, therelief groove 20 b is 0.5 mm or more away from the fitting portion, whereby a sufficient thickness of thesector mold 20 in the vicinity of the fitting portion can be ensured. Therefore, it is possible to prevent durability of thesector mold 20 from deteriorating. Since thesector mold 20 comes into contact with theside molds sector mold 20 in the vicinity of the fitting portion from deteriorating. In addition, therelief groove 20 b is provided within a distance of 0.8 mm from the fitting portion, thereby more reliably suppressing the rubber from flowing to the fitting portion. If therelief groove 20 b is provided extremely far from the fitting portion, the flow of the rubber toward the fitting portion cannot be suppressed, and it is impossible to provide the effect of preventing rubber from being caught in the fitting portion. - Further, the distance W2 between the
relief groove 20 b and theprojection 20 a is defined, thereby preventing durability of the tire to be manufactured from deteriorating, and sufficiently ensuring the area for arranging therelief groove 20 b. Specifically, therelief groove 20 b is 0.5 mm or more away from theprojection 20 a, thereby preventing a ridge line from being formed in the vicinity of the lug groove of the tire to be manufactured. If therelief groove 20 b is provided extremely close to theprojection 20 a, the ridge line is formed in the vicinity of the lug groove in the tire. In that case, since the lug groove and the ridge line form a protruding and recessed relation, the abrasion rate of the tire is increased. Therefore, by preventing the formation of therelief groove 20 b extremely close to theprojection 20 a, it is possible to prevent the abrasion resistance of the tire from deteriorating, that is, deterioration of durability of the pneumatic tire can be prevented. If therelief groove 20 b is provided extremely far from theprojection 20 a, that is, if therelief groove 20 b is provided extremely close to the fitting portion, the area for providing therelief groove 20 b between the fitting portion and theprojection 20 a is decreased. Therefore, therelief groove 20 b is provided within a distance of 0.8 mm from theprojection 20 a, whereby the sufficient area for arranging therelief groove 20 b in the mold can be ensured. - Further, a
relief groove 20 b is provided so as to extend in a direction (circumferential direction of the tire) intersecting with the flow direction of the rubber (radial direction of the tire) to the fitting portion. Therefore, when the rubber flows into the fitting portion, it stretches across therelief groove 20 b, so that the rubber can reliably escape to therelief groove 20 b. Therefore, the flow of the rubber to the fitting portion can be suppressed, and it is possible to prevent the rubber from being caught. In particular, when therelief groove 20 b is provided in the circumferential direction of the tire, it is easy to process therelief groove 20 b. - As described above, in the pneumatic tire AT (see
FIG. 4 ), since the biting of rubber during molding is suppressed, occurrence of poor appearance of the pneumatic tire AT is suppressed. Therefore, the aesthetic appearance of the tire is maintained. -
FIG. 5 shows a modification corresponding toFIG. 2B of the above embodiment. A plurality ofrelief grooves 20 b of this modification extend in a direction intersecting with both the circumferential direction and the radial direction of the green tire GT, that is, therelief grooves 20 b are provided in a mesh shape. Therelief grooves 20 b of the present modification extend so as to intersect with each of the circumferential direction and the radial direction at an angle of 45 degrees. Therelief grooves 20 b may intersect with each of the circumferential direction and the radial direction at an angle other than 45 degrees. - According to the present modification, when the
relief groove 20 b is provided in a mesh shape (including a knurl shape), the rubber can escape in various directions, and it is possible to more reliably suppress the rubber from being caught. - The form of the
relief groove 20 b is not limited to parallel streaks extending along the circumferential direction of the tire shown inFIG. 2B and a mesh shape which intersects with both the circumferential direction and the radial direction of the tire shown inFIG. 4 . For example, the form of therelief groove 20 b may be parallel streaks which intersect with the radial direction of the tire. - Although the specific embodiments of the present invention and its modifications have been described above, the present invention is not limited to the above-described embodiments, and various modifications can be made within the scope of the present invention. For example, an appropriate combination of descriptions of individual embodiments may be one embodiment of the present invention.
Claims (8)
1. A pneumatic tire comprising:
a protrusion-shaped mold fitting mark located between a tread portion and a side portion; and
a protrusion-shaped molding mark provided in a vicinity of and outside on the mold fitting mark,
wherein the molding mark is a plurality of protrusions in a mesh shape extending in a direction intersecting with both a circumferential direction and a radial direction.
2. The pneumatic tire according to claim 1 , wherein the molding mark has a height of 0.3 mm or more and 0.5 mm or less.
3. The pneumatic tire according to claim 1 , wherein the molding mark is provided away from the mold fitting mark by a distance of 0.5 mm or more and 0.8 mm or less.
4. The pneumatic tire according to claim 2 , wherein the molding mark is provided away from the mold fitting mark by a distance of 0.5 mm or more and 0.8 mm or less.
5. The pneumatic tire according to claim 1 ,
wherein a lug groove is provided on an outer surface of the pneumatic tire, and
wherein the molding mark is provided away from the lug by a distance of 0.5 mm or more and 0.8 mm or less.
6. The pneumatic tire according to claim 2 ,
wherein a lug groove is provided on an outer surface of the pneumatic tire, and
wherein the molding mark is provided away from the lug by a distance of 0.5 mm or more and 0.8 mm or less.
7. The pneumatic tire according to claim 3 ,
wherein a lug groove is provided on an outer surface of the pneumatic tire, and
wherein the molding mark is provided away from the lug by a distance of 0.5 mm or more and 0.8 mm or less.
8. The pneumatic tire according to claim 4 ,
wherein a lug groove is provided on an outer surface of the pneumatic tire, and
wherein the molding mark is provided away from the lug by a distance of 0.5 mm or more and 0.8 mm or less.