US20080217164A1 - Electrolytic Processing Apparatus - Google Patents
Electrolytic Processing Apparatus Download PDFInfo
- Publication number
- US20080217164A1 US20080217164A1 US10/585,739 US58573905A US2008217164A1 US 20080217164 A1 US20080217164 A1 US 20080217164A1 US 58573905 A US58573905 A US 58573905A US 2008217164 A1 US2008217164 A1 US 2008217164A1
- Authority
- US
- United States
- Prior art keywords
- electrode
- regeneration
- liquid
- ion exchanger
- electrolytic processing
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Abandoned
Abstract
An electrolytic processing apparatus (50) has feed electrodes (74) to feed a current to a substrate (W), an ion exchanger (76) brought into contact with the substrate (W), and process electrodes (72) to perform an electrolytic process on the substrate (W). The electrolytic processing apparatus (50) has an electrolytic processing liquid source to supply an electrolytic processing liquid between the substrate (W) and the ion exchanger (76), and a regeneration liquid supply source to supply a regeneration liquid to a regeneration liquid chambers (90 a , 90 b). The electrolytic processing apparatus (50) includes regeneration electrodes (84) spaced from the process electrodes (72). The feed electrode (74) has a potential higher than the process electrode (72) and the same polarity as the process electrode (72). The process electrode (72) has a potential higher than the regeneration electrode (84).
Description
- The present invention relates to an electrolytic processing apparatus, and more particularly to an electrolytic processing apparatus for processing 2 conductive material formed on a surface of a substrate such as a semiconductor wafer or removing impurities attached to the surface of the substrate.
- In recent years, there has been a growing tendency to replace aluminum or aluminum alloy as a metallic material for forming interconnection circuits on a substrate such as a semiconductor wafer with copper (Cu) having a low electric resistivity and a high electromigration resistance. Copper interconnections are generally formed by filling copper into fine recesses formed in a surface of a substrate. As methods for forming copper interconnections, there have been employed chemical vapor deposition (CVD), sputtering, and plating. In any of the methods, after a copper film is formed on substantially the entire surface of a substrate, unnecessary copper is removed by chemical mechanical polishing (CMP).
-
FIGS. 1A through 1C show an example of a process of forming a copper interconnection in a substrate W. As shown inFIG. 1A , aninsulating film 2, such as an oxide film of SiO2 or a film of low-k material, is deposited on aconductive layer 1 a on asemiconductor base 1 on which semiconductor devices have been formed. Acontact hole 3 and aninterconnection groove 4 are formed in theinsulating film 2 by lithography etching technology. Then, abarrier layer 5 made of TaN or the like is formed on theinsulating film 2, and aseed layer 7, which is used as a feeding layer for electrolytic plating, is formed on thebarrier layer 5 by sputtering, CVD, or the like. - Subsequently, as shown in
FIG. 1B , a surface of the substrate W is plated 30 with copper to fill thecontact hole 3 and theinterconnection groove 4 with copper and to form acopper film 6 on theinsulating film 2. Thereafter, the surface of the substrate W is polished by chemical mechanical polishing (CMP) to remove thecopper film 6 on theinsulating film 2 so that the surface of thecopper film 6 filled in thecontact hole 3 and theinterconnection groove 4 is made substantially even with the surface of theinsulating film 2. Thus, as shown inFIG. 1C , an interconnection comprising thecopper film 6 is formed in theinsulating layer 2. - Recently, components in various types of equipment have become finer and have required higher accuracy. As submicronic manufacturing technology has commonly been used, the properties of the materials are greatly influenced by the machining method. Under these circumstances, in a conventional mechanical machining method in which a desired portion of a workpiece is physically destroyed and removed from a surface thereof by a tool, a large number of defects may be produced by the machining, thus deteriorating the properties of the workpiece. Accordingly, it is important to perform machining without deteriorating the properties of materials.
- In copper interconnections as shown in
FIG. 1C , for example, instead of a silicon oxide film, which has heretofore been used for an insulating film, a material (low-k material) having a dielectric constant lower than that of the silicon oxide film has become employed in order to prevent signal delay caused by increased capacitance between interconnections. However, since the low-k material has a low density and a low mechanical strength, conventional processing methods such as CMP employing a mechanical effect may cause separation or mechanical breakage of the low-k material. - Some processing methods, such as chemical polishing, electrochemical machining, and electrolytic polishing, have been developed in order to solve the above problem. In contrast to the conventional physical machining methods, these methods perform a removal process or the like through a chemical dissolution reaction. Accordingly, these methods do not suffer from defects such as formation of an altered layer and dislocation due to plastic deformation, so that processing can be performed without deteriorating the properties of the materials.
- Recently, there has been developed an electrolytic processing apparatus employing an ion exchanger in an electrolytic process. As shown in
FIG. 2 , the electrolytic processing apparatus has apower supply 17, aprocess electrode 14 connected to thepower supply 17, and afeed electrode 16 connected to thepower supply 17. Theprocess electrode 14 has anion exchanger 12 a attached to a surface thereof. Thefeed electrode 16 has anion exchanger 12 b attached to a surface thereof. Aliquid 18 such as pure water or ultrapure water is supplied between theelectrodes workpiece 10 from afluid supply unit 19. Then, theworkpiece 10 is brought into contact with or close to theion exchangers electrodes process electrode 14 and thefeed electrode 16 by thepower supply 17. Thus, a surface of theworkpiece 10 is removed. - According to the electrolytic process,
water molecules 20 in theliquid 18 are dissociated intohydroxide ions 22 andhydrogen ions 24 by theion exchangers hydroxide ions 22 are supplied to the surface of theworkpiece 10 facing theprocess electrode 14. The concentration of thehydroxide ions 22 is thus increased near theworkpiece 10.Atoms 10 a in theworkpiece 10 and thehydroxide ions 22 are reacted with each other to perform removal of a surface layer of theworkpiece 10.Reactants 26 produced by the reaction are dissolved into theliquid 18 and removed from theworkpiece 10 by theliquid 18 flowing along the surface of theworkpiece 10. - For example, when a cation exchanger having a cation exchange group is used as an ion exchanger for a copper electrolytic process, copper is captured by the cation exchange group. Thus, the cation exchange group is consumed by copper. If copper consumes the cation exchange group, then a process product is deposited on the
process electrode 14 to cause short circuit between theworkpiece 10 and theprocess electrode 14. Accordingly, the electrolytic process cannot continuously be performed. When an anion exchanger having an anion exchange group is used as an ion exchanger for a copper electrolytic process, fine particles of copper oxide are produced on and attached to a surface of the ion exchanger (anion exchanger). Accordingly, the uniformity of a process rate is deteriorated. Further, the fine particles may contaminate a surface of a next substrate to be processed. - As a result, in an electrolytic process employing an ion exchanger, the amount of workpiece that can continuously be processed is so small that it is necessary to interrupt the electrolytic process and replace or regenerate the ion exchanger. When the ion exchanger is regenerated, ions captured in the ion exchanger are exchanged for hydrogen ions in a case of a cation exchanger or for hydroxide ions in a case of an anion exchanger.
- Methods of regenerating an ion exchanger include immersing an ion exchanger in a chemical liquid or applying a voltage that is opposite to a voltage of an electrolytic process to an ion exchanger.
- For example, a method of immersing an ion exchanger in a chemical liquid is performed as follows. An acid chemical liquid is used when the ion exchanger comprises a cation exchanger. An alkali chemical liquid is used when the ion exchanger comprises an anion exchanger. The ion exchanger is immersed in such a chemical liquid. For example, in a case of a cation exchanger which has captured ions having a selectivity coefficient close to that of hydrogen ions, such as sodium ions, the ion exchanger can be regenerated for a considerably short period of time by immersion in an acid chemical liquid. When an ion exchanger which has captured ions having a large selectivity coefficient is regenerated by an acid or an alkali, a regeneration rate of the ion exchanger becomes considerably small.
- Further, after regeneration of the ion exchanger, the chemical liquid remains in the ion exchanger at a high concentration. Accordingly, the ion exchanger should be cleaned. Furthermore, it is necessary to treat the chemical liquid used for regeneration. Additionally, since a separate regeneration tank should be provided to store a chemical liquid for regeneration, a large space is required to install the electrolytic processing apparatus. Further, since the process should be interrupted to regenerate the ion exchanger, a throughput of the electrolytic processing apparatus is lowered.
- For example, a method of applying a voltage that is opposite to a voltage of an electrolytic process to an ion exchanger to regenerate the ion exchanger is performed as follows. After a workpiece has been processed to a certain extent, a regeneration electrode is disposed so as to face a process electrode instead of the workpiece. A voltage that is opposite to a voltage of the electrolytic process is applied to remove substances captured in the ion exchanger. In this method, it is necessary to interrupt the process to regenerate the ion exchanger. Accordingly, a throughput of the electrolytic processing apparatus is lowered.
- The present invention has been made in view of the above drawbacks. It is, therefore, an object of the present invention to provide an electrolytic processing apparatus which can continuously remove ions captured in a contact member such as an ion exchanger during processing a workpiece, and can continuously perform an electrolytic process on the workpiece while accumulation or deposition of process products is prevented in an electrode and the contact member.
- According to an aspect of the present invention, there is provided an electrolytic processing apparatus which performs an electrolytic process on a conductive material formed on a workpiece. The electrolytic processing apparatus has a feed electrode configured to feed an electric current to a conductive film formed on a workpiece, a contact member, such as an ion exchanger, configured to be brought into contact with or close to the workpiece, and a process electrode operable to perform an electrolytic process on the conductive material of the workpiece. The electrolytic processing apparatus also has an electrolytic processing liquid source configured to supply an electrolytic processing liquid between the workpiece and the contact member, a regeneration liquid chamber for immersing the process electrode in a regeneration liquid, and a regeneration liquid supply source configured to supply the regeneration liquid to the regeneration liquid chamber. The electrolytic processing apparatus includes a regeneration electrode spaced from the process electrode and a power supply operable to apply a voltage between the feed electrode, the process electrode, and the regeneration electrode. The electrolytic processing apparatus also includes a controller operable to control the voltage applied between the feed electrode, the process electrode, and the regeneration electrode so that the feed electrode has a potential higher than the process electrode and the same polarity as the process electrode, and that the process electrode has a potential higher than the regeneration electrode.
- Thus, the ion exchanger is brought into contact with or close to the workpiece while an electric current is fed to the workpiece. The electrolytic processing liquid is supplied between the workpiece and the process electrode. For example, a first voltage is applied between the process electrode and the feed electrode, and a second voltage is applied between the process electrode and the regeneration electrode. Accordingly, an electrolytic process by the process electrode and a regeneration process of the ion exchanger by the regeneration electrode can be performed simultaneously. A first voltage may be applied between the feed electrode and the regeneration electrode, and a second voltage may be applied between the process electrode and the regeneration electrode. Alternatively, a first voltage may be applied between the feed electrode and the process electrode, and a second voltage may be applied between the feed electrode and the regeneration electrode.
- The electrolytic processing apparatus may include an insulation member disposed between the contact member (ion exchanger) and the process electrode. The insulation member has liquid permeability. With this arrangement, ionic process products or ionic impurities captured in the ion exchanger during processing can be moved through the insulation member toward the process electrode by electrophoresis and dissolved in the regeneration liquid. The ionic process products or ionic impurities are discharged to the exterior of the system by the flow of the regeneration liquid or moved toward the regeneration electrode by electrophoresis using the power supply and deposited on the regeneration electrode. Thus, even if deposition occurs on the process electrode, the deposition does not reach the ion exchanger. Accordingly, no short circuits are caused between the process electrode and the workpiece.
- It is desirable that the electrolytic processing liquid comprises ultrapure water, pure water, a liquid having an electric conductivity of 500 μS/cm or less, or an electrolytic solution. For example, ultrapure water has an electric conductivity of 0.1 μS/cm or less. In this case, the electric conductivity is represented as a converted value at 1 atm and 25° C. This also holds true in the following examples. For example, pure water has an electric conductivity of 10 μS/cm or less. Thus, with pure water, preferably ultrapure water, a clean electrolytic process can be achieved while no impurities remain on a surface of the workpiece. Accordingly, subsequent processes of cleaning the surface of the workpiece and treating a waste liquid can be simplified.
- For example, an additive such as a surface active agent may be added into pure water or ultrapure water to adjust the electric conductivity at 500 μS/cm or less, preferably 50 μS/cm or less, more preferably 0.1 μS/cm or less. Thus, when an additive which serves to prevent ions from being locally concentrated is added, ions are prevented from being locally concentrated. For example, the electrolytic solution may comprise a solution of a neutral salt such as NaCl or Na2SO4, a solution of an acid such as HCl or H2SO4, or a solution of an alkali such as ammonia. The electrolytic solution can be selectively used according to the properties of the workpiece.
- The electrolytic processing apparatus may include a diaphragm disposed between the contact member and the insulation member so as to separate the electrolytic processing liquid and the regeneration liquid. The diaphragm may comprise an ion exchange film. With such an arrangement, the regeneration liquid can comprise a different liquid than the electrolytic processing liquid. Accordingly, a liquid which is unlikely to cause deposition or accumulation of process products or impurities can be used as the regeneration liquid.
- It is desirable that the diaphragm comprises a cation exchanger when the contact member comprises a cation exchanger. It is also desirable that the diaphragm comprises an anion exchanger when the contact member comprises an anion exchanger. At that time, positive ions in the contact member of the cation exchanger pass through the cation exchanger of the diaphragm and reach the regeneration liquid. The positive ions are dissolved in the regeneration liquid and removed. Similarly, negative ions in the contact member of the anion exchanger pass through the anion exchanger of the diaphragm and reach the regeneration liquid. The negative ions are dissolved in the regeneration liquid and removed.
- The controller may be operable to control potentials of the feed electrode, the process electrode, and the regeneration electrode, or currents flowing through the feed electrode, the process electrode, and the regeneration electrode. The current flowing through the feed electrode exerts a great influence on a processing rate, and the current flowing through the process electrode exerts a great influence on a tendency unlikely to cause deposition or accumulation of process products or impurities. Accordingly, by controlling the current flowing through the feed electrode and the current flowing through the process electrode, it is possible to control a processing rate or a tendency unlikely to cause deposition or accumulation of process products or impurities.
- For example, a tendency unlikely to cause deposition or accumulation of process products or impurities will be described below. When copper is processed while the feed electrode serves as an anode and the process electrode serves as a cathode, deposits accumulate on the process electrode in several minutes. Thus, a short circuit occurs between the process electrode and the feed electrode. Accordingly, it becomes impossible to continue the electrolytic process. However, when the process electrode serves as an anode (which is the same polarity as the feed electrode), an electrolytic process can be continued for at least several hours without any short circuit between the process electrode and the feed electrode. The anode is defined as an electrode from which positive charges flow toward the electrolytic processing liquid. The cathode is defined as an electrode into which positive charges flow from the electrolytic processing liquid. Accordingly, it is important that a current flows through the process electrode in a fixed direction continuously during processing. Specifically, it is important to maintain the polarity of the process electrode (so as to have the same polarity as the feed electrode). Thus, it is desirable to control a current or a voltage at a constant value to maintain the polarity of the process electrode.
- In this case, it is desirable that the current flowing through the process electrode is controlled so as to be equal to 1 to 30% of the current flowing through the feed electrode or the regeneration electrode. As a larger current flows through the process electrode, deposition of impurities can be prevented more effectively. Usually, 1 to 30% of the current flowing through the feed electrode or the regeneration electrode is sufficient for the current flowing through the process electrode. In consideration of consumed energy and process cost, it is desirable that the current flowing through the process electrode is in a range of 1 to 10%, preferably 1 to 3% of the current flowing through the feed electrode or the regeneration electrode.
- According to the present invention, process products can readily and immediately be removed from the contact member such as an ion exchanger during an electrolytic process. It is possible to prevent accumulation or deposition of process products within the electrode and the contact member. Accordingly, it is possible to reduce or eliminate a period of time during which the electrolytic process is interrupted to regenerate the contact member. Thus, the efficiency of the electrolytic processing apparatus can be improved.
- The above and other objects, features, and advantages of the present invention will be apparent from the following description when taken in conjunction with the accompanying drawings which illustrate preferred embodiments of the present invention by way of example.
-
FIGS. 1A through 1C are diagrams showing an example of a process of forming a copper interconnection in a substrate; -
FIG. 2 is a schematic view showing a principle of an electrolytic process employing an ion exchanger; -
FIG. 3 is a vertical cross-sectional view showing an electrolytic processing apparatus according to an embodiment of the present invention; -
FIG. 4 is a partial enlarged view of the electrolytic processing apparatus shown inFIG. 3 ; -
FIG. 5A is a circuit diagram showing electric connection in the electrolytic processing apparatus shown inFIGS. 3 and 4 ; and -
FIGS. 5B and 5C are circuit diagrams showing variations of the electric connection shown inFIG. 5A . - An electrolytic processing apparatus according to an embodiment of the present invention will be described below with reference to
FIGS. 3 through 5C . Like or corresponding parts are denoted by like or corresponding reference numerals throughout drawings, and will not be described below repetitively. In the following description, a substrate is processed as a workpiece by an electrolytic processing apparatus. However, the present invention is applicable to any workpiece other than a substrate. -
FIG. 3 is a vertical cross-sectional view showing anelectrolytic processing apparatus 50 according to an embodiment of the present invention. Theelectrolytic processing apparatus 50 has anarm 52 extending in a horizontal direction, asubstrate holder 54 attached to a free end of thearm 52, and a circular electrode table 56 disposed below thesubstrate holder 54. Thearm 52 is movable in a vertical direction and swingable in a horizontal direction. Thesubstrate holder 54 attracts and holds a workpiece W such as a substrate in a state such that the substrate W faces downward (in a face-down manner). - The
electrolytic processing apparatus 50 also has aswing shaft 62 coupled to aswing motor 60. Thearm 52 is attached to an upper end of theswing shaft 62. Thus, when theswing motor 60 is driven, thearm 52 is swung in the horizontal direction so as to pivot about theswing shaft 62. Theswing shaft 62 is coupled to aball screw 64 extending in the vertical direction. The ball screw 64 is connected to avertical movement motor 66. Thus, when thevertical movement motor 66 is driven, theswing shaft 62 is moved vertically together with thearm 52. - The
substrate holder 54 is coupled to arotation motor 68 mounted on thearm 52. Therotation motor 68 serves as a first driving mechanism for moving the substrate W held by thesubstrate holder 54 and the electrode table 56 relative to each other. Thus, when therotation motor 68 is driven, thesubstrate holder 54 is rotated. Further, since thearm 52 is vertically movable and horizontally swingable as described above, thesubstrate holder 54 is movable in the vertical direction and swingable in the horizontal direction together with thearm 52. - The
electrolytic processing apparatus 50 includes ahollow motor 70 disposed below the electrode table 56. Thehollow motor 70 serves as a second driving mechanism for moving the substrate W and the electrode table 56 relative to each other. Thus, when thehollow motor 70 is driven, the substrate W and the electrode table 56 make a scroll movement or a translational rotation movement. - The electrode table 56 includes
process electrodes 72,feed electrodes 74, and an insulator (not shown) disposed around theprocess electrodes 72 and thefeed electrodes 74. For example, theprocess electrodes 72 and thefeed electrodes 74 may have a sectorial shape. Theprocess electrodes 72 and thefeed electrodes 74 are embedded alternately in the electrode table 56 in a manner such that (upper) surfaces of theelectrodes electrodes ion exchanger 76. When theprocess electrodes 72 and thefeed electrodes 74 are divided along a circumferential direction of the electrode table 56 and alternately arranged in the electrode table 56, it is possible to eliminate a fixed portion for feeding an electric current to a conductive film of the substrate W (workpiece). Thus, it is possible to process the entire surface of the substrate W. In the present embodiment, the electrode table 56 including theprocess electrodes 72 and thefeed electrodes 74 has a diameter slightly larger than the diameter of the substrate W held by thesubstrate holder 54. Since the electrode table 56 makes a scroll movement, the entire surface of the substrate W is subjected to an electrolytic process. - For example, the
ion exchanger 76 on the electrode table 56 may be formed of a nonwoven fabric having an anion exchange function or a cation exchange function. Preferably, the cation exchanger has a strongly acidic cation exchange group (e.g., sulfonic acid group). Alternatively, the cation exchanger may have a weakly acidic cation exchange group (e.g., carboxyl group). Preferably, the anion exchanger has a strongly basic anion exchange group (e.g., quaternary ammonium group). Alternatively, the anion exchanger may have a weakly basic anion exchange group (e.g., tertiary or lower ammonium group). - For example, a nonwoven fabric having a strongly basic anion exchange function can be prepared as follows. Graft chains are introduced into a polyolefin nonwoven fabric having a fiber diameter of 20 to 50 μm and a porosity of about 90% with the use of radiation-induced graft polymerization, which comprises gamma irradiation and graft polymerization. Then, the introduced graft chains are aminated to introduce a quaternary ammonium group to thereby form a nonwoven fabric having a strongly basic anion exchange function. The capacity of the introduced ion exchange group is determined according to the amount of graft chains introduced. The graft polymerization may be conducted by the use of a monomer such as acrylic acid, styrene, glycidyl methacrylate, sodium styrenesulfonate, or chloromethylstyrene. The amount of the graft chains can be controlled by adjusting the monomer concentration, the reaction temperature, and the reaction time. A graft ratio, which is a ratio of the weight of a material after graft polymerization to the weight thereof before the graft polymerization, can be increased to about 500% at maximum. The exchange capacity of the ion exchange group introduced by graft polymerization can be increased to about 5 meq/g at maximum.
- For example, a nonwoven fabric having a strongly acidic cation exchange function can be prepared as follows. Graft chains are introduced into a polyolefin nonwoven fabric having a fiber diameter of 20 to 50 μm and a porosity of about 90% with the use of radiation-induced graft polymerization, which comprises gamma irradiation and graft polymerization. Then, the introduced graft chains are treated with heated sulfuric acid to introduce a sulfonic acid group to thereby form a nonwoven fabric having a strongly acidic cation exchange function. Such a nonwoven fabric can have a graft ratio of about 500% at maximum. The exchange capacity of the ion exchange group introduced by graft polymerization can be increased to about 5 meq/g at maximum.
- The
ion exchanger 76 may be formed of polyolefin such as polyethylene or polypropylene, or any other organic polymers. Further, theion exchanger 76 may be in the form of a woven fabric, a sheet, a porous material, short fibers, a net, or the like. In a case of the graft polymerization of polyethylene or polypropylene, a radioactive ray (γ-ray or electron beam) may be applied to a material for pre-irradiation to generate a radical so that the radical reacts with a monomer. In this case, it is possible to produce uniform graft chains which have fewer impurities. Alternatively, a material may be impregnated with a monomer and irradiated with a radioactive ray (γ-ray, electron beam, or ultraviolet ray) for simultaneous irradiation to perform a radical polymerization. In this method, the uniformity of graft chains may be lowered, but can be applied to almost all materials. - Thus, when the
ion exchanger 76 is formed of a nonwoven fabric having an anion exchange function or a cation exchange function, the water permeability can be provided so that a liquid, such as pure water, ultrapure water, or an electrolytic solution, can move within the nonwoven fabric without any interruption. Accordingly, ion exchange reaction is readily performed between ions in liquid phase and an ion exchange group in theion exchanger 76. - If the
ion exchanger 76 is formed of a material having only one of an anion exchange function and a cation exchange function, types of materials that can be subjected to an electrolytic process are limited. Further, impurities are likely to be produced by its polarity. Accordingly, theion exchanger 76 may have a structure in which cation exchangers having a cation exchange function and anion exchangers having an anion exchange function are concentrically arranged. Alternatively, anion exchangers having an anion exchange function and cation exchangers having an anion exchange function may be piled on each other. Further, anion exchangers and cation exchangers may be formed into sectorial shapes and disposed alternately in a circumferential direction. Furthermore, theion exchanger 76 may have both of an anion exchange function and a cation exchange function. Such an ion exchanger may include an amphoteric ion exchanger having anion exchange groups and cation exchange groups which are distributed in a desired manner, a bipolar ion exchanger having anion exchange groups and cation exchange groups in the form of layers, and a mosaic ion exchanger having portions containing anion exchange groups and portions containing cation exchange groups in parallel in a thickness direction. It is possible to selectively use an ion exchanger having an anion exchange function or an ion exchanger having a cation exchange function according to the material to be processed. -
FIG. 4 is a partial enlarged view of theelectrolytic processing apparatus 50 shown inFIG. 3 . As shown inFIG. 4 , the electrode table 56 has a through-hole 56 a defined at a central portion thereof and an electrolytic processingliquid supply pipe 78 for supplying an electrolytic processing liquid, such as pure water, preferably ultrapure water, to the through-hole 56 a. The electrolytic processingliquid supply pipe 78 extends through a hollow portion of thehollow motor 70. The through-hole 56 a is connected through the electrolytic processingliquid supply pipe 78 to an electrolytic processingliquid supply source 80. Thus, the electrolytic processing liquid is supplied through the through-hole 56 a to an upper surface of the electrode table 56 and is then supplied through theion exchanger 76 having water absorbing properties to the entire surface of the substrate W. - For example, pure water has an electric conductivity of 10 μS/cm or less, and ultrapure water has an electric conductivity of 0.1 μS/cm or less. A liquid having an electric conductivity of 500 μS/cm or less, or various electrolytic solutions may be used instead of pure water. By supplying such a liquid during processing, unstableness of the process, which is caused by process products or gas dissolution, can be eliminated so as to achieve a uniform process with high reproducibility.
- A liquid having an electric conductivity of 500 μS/cm or less (e.g., an electrolytic solution in which an electrolyte is added into pure water or ultrapure water) can be used instead of pure water or ultrapure water. The use of the electrolytic solution can reduce an electric resistance and hence electric power consumption. The electrolytic solution may comprise a solution of a neutral salt such as NaCl or Na2SO4, a solution of an acid such as HCl or H2SO4, or a solution of an alkali such as ammonia. The electrolytic solution can be selectively used according to the properties of the workpiece. When the electrolytic solution is used, it is desirable to form a slight gap between the substrate W and the
ion exchanger 76 so that the substrate W is not brought into contact with theion exchanger 76. - Further, instead of pure water or ultrapure water, there may be used a liquid in which a surface active agent is added into pure water or ultrapure water so as to have an electric conductivity of 500 μS/cm or less, preferably 50 μS/cm or less, more preferably 0.1 μS/cm or less (a resistivity of 10 MΩ·cm or less). By adding a surface active agent into pure water or ultrapure water, a uniform layer can be formed at an interface between the substrate W and the
ion exchanger 76 to moderately inhibit ion migration. Thus, concentrated ion exchange (metal dissolution) can be moderated so as to enhance flatness of the surface of the substrate W. The concentration of the surface active agent is preferably 100 ppm or less. If the liquid has an excessively high electric conductivity, a current efficiency and a processing rate are lowered. The use of the liquid having an electric conductivity of 500 ES/cm or less, preferably 50 μS/cm or less, more preferably 0.1 μS/cm or less, can provide a desired processing rate. - In the present embodiment, a plurality of
sectorial electrodes FIG. 3 , theelectrodes power supply 58, respectively. The electrodes connected to the cathode of thepower supply 58 serve as process electrodes while the electrodes connected to the anode of thepower supply 58 serve as feed electrodes. This is because an electrolytic process is performed on the cathode side in a case of copper. Depending upon a material to be processed, the electrodes connected to the cathode may serve as feed electrodes while the electrodes connected to the anode may serve as process electrodes. Specifically, when the material to be processed is copper, molybdenum, or iron, an electrolytic process is performed on the cathode side. Accordingly, the electrodes connected to the cathode of thepower source 58 serve as the process electrodes while the electrodes connected to the anode serve as the feed electrodes. When the material to be processed is aluminum or silicon, an electrolytic process is performed on the anode side. Accordingly, the electrodes connected to the anode serve as the process electrodes while the electrodes connected to the cathode serve as the feed electrodes. - Generally, oxidation or dissolution of the
process electrodes 72 and thefeed electrodes 74 problematically occurs due to an electrolytic reaction. Accordingly, it is desirable that the electrodes are made of carbon, a noble metal that is relatively inactive, a conductive oxide, or a conductive ceramics, rather than metal or metal compound, which has widely been used for electrodes. For example, in order to produce a noble metal-based electrode, a titanium electrode may be plated or coated with platinum or iridium and then sintered at a high temperature to stabilize and strengthen the electrode. Generally, inorganic raw materials are subjected to heat treatment to produce ceramics products. Ceramics products having various properties are produced from various raw materials including oxides, carbides, and nitrides of metals and nonmetals. Some ceramics have an electric conductivity. When an electrode is oxidized, the electric resistance of the electrode is increased to thereby cause an increase of an applied voltage. However, by protecting the surface of an electrode with a non-oxidative material such as platinum or with a conductive oxide such as an iridium oxide, the electric resistance of the electrode can be prevented from being increased due to oxidation of the electrode. - When the
ion exchanger 76 has a cation exchange group to perform a copper electrolytic process, copper occupies most of ion exchange groups in the ion exchanger (cation exchanger) 76 after the electrolytic process. Accordingly, a process efficiency is lowered when a next substrate is processed. Alternatively, process products are deposited on theprocess electrodes 72 to cause a short circuit between the substrate W and theprocess electrodes 72. Thus, it is difficult to continuously perform an electrolytic process. Further, whenion exchanger 76 has an anion exchange group to perform a copper electrolytic process, fine particles of copper oxides are produced on and attached to a surface of the ion exchanger (anion exchanger) 76. Accordingly, the fine particles of copper oxides may contaminate a surface of a next substrate. In the present embodiment, a cation exchanger is used as theion exchanger 76 and regenerated at a location between theprocess electrodes 72 and the substrate W in the following manner. - As shown in
FIG. 4 , each of theprocess electrodes 72 is housed in arecess 56 b formed in the electrode table 56, and each of thefeed electrodes 74 is housed in arecess 56 c formed in the electrode table 56. Therecess 56 b which houses theprocess electrode 72 has a depth greater than that of therecess 56 c which houses thefeed electrode 74.Regeneration electrode 84 for regenerating theion exchanger 76 is disposed at a bottom of therecess 56 b. - The
recess 56 b has an upper opening covered with adiaphragm 86. Further, aninsulation member 88 is disposed on an upper surface of theprocess electrode 72. Each of theinsulation member 88 and theprocess electrode 72 has liquid permeability. In the present embodiment, theprocess electrode 72 is formed of an electrode having a large number of meshes, which serve as through-holes. As shown inFIG. 4 , thediaphragm 86 is spaced from theinsulation member 88 so as to form aregeneration liquid chamber 90 a between theprocess electrode 72 and thediaphragm 86. Theregeneration electrode 84 is spaced from theprocess electrode 72 so as to form aregeneration liquid chamber 90 b between theprocess electrode 72 and theregeneration electrode 84. - The
regeneration liquid chambers liquid supply passage 56 d, which extends through the electrode table 56. The regenerationliquid supply passage 56 d is connected through a regenerationliquid supply pipe 92, which extends through the hollow portion of thehollow motor 70, to a regenerationliquid supply source 94. Peripheral portions of theregeneration liquid chambers liquid discharge passages 56 e. The regenerationliquid discharge passages 56 e extend in the horizontal direction and open at peripheral edges of the electrode table 56. - With such an arrangement, a regeneration liquid is supplied through the regeneration
liquid supply passage 56 d into theregeneration liquid chambers regeneration liquid chambers process electrode 72 and theinsulation member 88 in the regeneration liquid. The regeneration liquid flows in one direction within theregeneration liquid chambers liquid discharge passages 56 e to the exterior of the electrode table 56. - As described above, the
process electrode 72 is formed of an electrode having a large number of meshes which serve as through-holes. Accordingly, process products in the form of ions (ionic impurities) which have been produced from theion exchanger 76 pass through the meshes (through-holes) in theprocess electrode 72 into theregeneration liquid chamber 90 b. - Preferably, the regeneration liquid to be supplied into the
regeneration liquid chambers ion exchanger 76. Specifically, the regeneration liquid serves to discharge ions that have moved from theion exchanger 76 and passed through thediaphragm 86 and theprocess electrode 72 to the exterior of the electrode table 56 by the liquid flow. Thus, when the regeneration liquid comprises a liquid that has a high electric conductivity (dielectric constant) and is unlikely to generate insoluble compounds by reaction with ions that have been removed from theion exchanger 76, the electric resistance of the regeneration liquid can be lowered so as to reduce the electric power consumption in theregeneration liquid chambers ion exchanger 76 and from being attached to thediaphragm 86. The regeneration liquid is selectively used according to types of ionic impurities to be removed. For example, when an ion exchanger that has been used for a copper electrolytic process is regenerated, the regeneration liquid may comprise sulfuric acid having a concentration of at least 1 wt %. - It is desirable that the
diaphragm 86, which is disposed below theion exchanger 76, does not interfere with movement of ionic impurities to be removed from theion exchanger 76. Further, it is desirable that thediaphragm 86 can prevent a regeneration liquid (including ions therein) flowing through theregeneration liquid chamber 90 a between thediaphragm 86 and theinsulation member 88 from permeating thediaphragm 86 into theion exchanger 76. Materials that can meet such requirements include a membranous ion exchanger such as Nafion™ (by DuPont). Such an ion exchanger allows anions or cations to selectively permeate thediaphragm 86. Further, since the ion exchanger is membranous, the regeneration liquid is prevented from flowing from theregeneration liquid chamber 90 a into theion exchanger 76. - In the present embodiment, the
diaphragm 86 comprises an ion exchanger having the same ion exchange group as theion exchanger 76, i.e. a cation exchanger. Accordingly, the diaphragm (ion exchanger) 86 can allow only ions from the ion exchanger (cation exchanger) 76 to permeate thediaphragm 86. The ions in the regeneration liquid flowing through theregeneration liquid chamber 90 a are prevented from permeating the diaphragm (ion exchanger) 86 into theion exchanger 76. If theion exchanger 76 comprises an anion exchanger having an anion exchange group, it is desirable to use an anion exchanger as the diaphragm (ion exchanger) 86. - The
insulation member 88 having liquid permeability should be insoluble in the regeneration liquid. In the present embodiment, theinsulation member 88 comprises a fluorocarbon resin sheet having a thickness of about 0.1 mm, which has a large number of holes having a diameter of about 2 mm. Process products are deposited on theprocess electrode 72 and subsequently deposited in theion exchanger 76. Specifically, the process products extend through theion exchanger 76 and reach the substrate W to cause a short circuit between theprocess electrode 72 and the substrate W. In the case where theinsulation member 88 having liquid permeability is disposed between theprocess electrode 72 and theion exchanger 76, even if deposition occurs on theprocess electrode 72, the deposition does not reach theion exchanger 76. Accordingly, a short circuit is not caused between theprocess electrode 72 and the substrate W. - In the present embodiment, the
feed electrodes 74 are connected to the anode of thepower supply 58, and theprocess electrodes 72 are connected to the cathode of thepower supply 58. Thepower supply 58 supplies a process voltage between thefeed electrodes 74 and theprocess electrodes 72. Theprocess electrodes 72 and theregeneration electrodes 84 are connected through the control box (not shown) to the anode and the cathode of apower supply 96, respectively. Thepower supply 96 supplies a regeneration voltage between theprocess electrode 72 and theregeneration electrode 84. - The control box (see
FIG. 3 ) connected to thepower supply 58 and the control box (not shown) connected to thepower supply 96 adjust a process voltage and a regeneration voltage so that a potential of thefeed electrode 74 is higher than that of theprocess electrode 72, and the potential of theprocess electrode 72 is higher than that of theregeneration electrode 84. The control boxes also adjust the process voltage and the regeneration voltage so that thefeed electrode 74 has the same polarity as theprocess electrode 72. In the present embodiment, the polarities of thefeed electrode 74 and theprocess electrode 72 are anodic. Specifically, positive charges flow from thefeed electrode 74 and theprocess electrode 72 into an electrolytic processing liquid. Accordingly, process products (ions) which accumulate on theion exchanger 76 can continuously be discharged. As a result, the electrolytic process can be continued for a long term. - In the present embodiment, the
feed electrode 74, theprocess electrode 72, and theregeneration electrode 84 are electrically connected in series. The control boxes independently control a current flowing through thefeed electrode 74, a current flowing through theprocess electrode 72, a current flowing through theregeneration electrode 84, a potential of thefeed electrode 74, a potential of theprocess electrode 72, and a potential of theregeneration electrode 84. Thus, ionic impurities can be discharged from theion exchanger 76 during the electrolytic process. Accordingly, the electrolytic process can continuously be performed. Particularly, it is desirable to control a current flowing through theprocess electrode 72 so as to be equal to 1 to 30% of a current flowing through thefeed electrode 74 or theregeneration electrode 84. - In the present embodiment, as shown in
FIG. 5A , thefeed electrode 74, theprocess electrode 72, and theregeneration electrode 96 are electrically connected in series to thepower supply 58 and thepower supply 96. However, connection of the electrodes and the power supplies is not limited to the illustrated example. As shown inFIG. 5B , for example, thefeed electrode 74 may be connected to an anode of a first power supply 97 a while theregeneration electrode 84 may be connected to a cathode of the first power supply 97 a. Theprocess electrode 72 may be connected to an anode of asecond power supply 97 b while theregeneration electrode 84 may be connected to a cathode of thesecond power supply 97 b. Alternatively, as shown inFIG. 5C , thefeed electrode 74 may be connected to an anode of afirst power supply 98 a while theregeneration electrode 84 may be connected to a cathode of thefirst power supply 98 a. Thefeed electrode 74 may be connected to an anode of asecond power supply 98 b while theprocess electrode 72 may be connected to a cathode of thesecond power supply 98 b. According to connections shown inFIGS. 5B and 5C , a potential of theprocess electrode 72 can accurately be set and controlled by accurately controlling a voltage of thesecond power supply - Further, when the
process electrode 72 is disposed close to theion exchanger 76 so that theprocess electrode 72 has the same potential as theion exchanger 76, variations of an electric field can be prevented so as to reduce an adverse influence from deposits or air bubbles. In order to uniformly perform an electrolytic process and a regeneration process, the surface of the substrate W, theprocess electrode 72, and theregeneration electrode 84 are preferably disposed in parallel to each other. It is desirable that thewhole ion exchanger 76 has a uniform thickness. - There will be described substrate processing (an electrolytic process and a regeneration process) employing the
electrolytic processing apparatus 50. First, thesubstrate holder 54 of theelectrolytic processing apparatus 50 attracts and holds a substrate W. Thearm 52 is swung to move thesubstrate holder 54 holding the substrate W to an electrolytic process position located right above the electrode table 56. Then, thevertical movement motor 66 is driven to lower thesubstrate holder 54. Thus, the substrate W held by thesubstrate holder 54 is brought into contact with or close to a surface of theion exchanger 76 attached to the upper surface of the electrode table 56. - At that time, the
rotation motor 68 is driven to rotate the substrate W. Simultaneously, thehollow motor 70 is driven so that the electrode table 56 makes a scroll movement. An electrolytic processing liquid such as pure water or ultrapure water is supplied from the through-hole 56 a in the electrode table 56 to the upper surface of the electrode table 56. Thus, a space between theprocess electrode 72, thefeed electrode 74, and the substrate W is filled with pure water, ultrapure water, a liquid of 500 μS/cm or less, or an electrolytic solution. Thepower supply 58 applies a process voltage between theprocess electrode 72 and thefeed electrode 74. Thus, hydrogen ions or hydroxide ions generated by theion exchanger 76 perform an electrolytic process on a conductive film (e.g., acopper film 6 shown inFIG. 1B ) formed on a surface of the substrate W at the process electrode (cathode). Since theelectrolytic processing apparatus 50 is configured so that the electrolytic processing liquid such as pure water or ultrapure water flows through theion exchanger 76, an efficient electrolytic process can be achieved. - At that time, a regeneration liquid for the
ion exchanger 76 is supplied through the regenerationliquid supply passage 56 d in the electrode table 56 into theregeneration liquid chambers regeneration liquid chambers process electrode 72 and theinsulation member 88 in the regeneration liquid. The regeneration liquid flows through theregeneration liquid chambers liquid discharge passages 56 e to the exterior of the electrode table 56. - Accordingly, ions in the
ion exchanger 76 are moved toward theprocess electrode 72 by ion exchange reaction employing theion exchanger 76 as a solid electrolyte. The ions in theion exchanger 76 pass through thediaphragm 86 into theregeneration liquid chamber 90 a. The ions moved to theregeneration liquid chamber 90 a are discharged to the exterior of the electrode table 56 by the regeneration liquid flowing through theregeneration liquid chamber 90 a. Thus, theion exchanger 76 is regenerated. At that time, when a cation exchanger is used as theion exchanger 76, cations captured in theion exchanger 76 are moved through thediaphragm 86 into theregeneration liquid chamber 90 a. When an anion exchanger is used as theion exchanger 76, anions captured in theion exchanger 76 are moved through thediaphragm 86 into theregeneration liquid chamber 90 a. - Further, a regeneration voltage is applied between the
process electrode 72 and theregeneration electrode 84 during processing by thepower supply 96 to force a current to flow between theprocess electrode 72 and theregeneration electrode 84. Thus, ionic process products (ionic impurities) accumulating in theion exchanger 76 can be moved through theprocess electrode 72 into theregeneration liquid chamber 90 b. The ions moved to theregeneration liquid chamber 90 b are discharged to the exterior of the electrode table 56 by the regeneration liquid supplied to theregeneration liquid chamber 90 b or deposited on theregeneration electrode 84. Thus, theion exchanger 76 can be regenerated. - As described above, since the
diaphragm 86 comprises an ion exchanger having the same ion exchange group as theion exchanger 76, the diaphragm (ion exchanger) 86 is prevented from inhibiting movement of ionic impurities in theion exchanger 76 through the diaphragm (ion exchanger) 86. Thus, electric power consumption can be reduced. Further, the regeneration liquid (including ions therein) flowing between thediaphragm 86 and theprocess electrode 72 is prevented from permeating thediaphragm 86 into theion exchanger 76. Thus, re-contamination of theion exchanger 76 can be prevented after the regeneration. Furthermore, since the regeneration liquid supplied between thediaphragm 86 and theprocess electrode 72 has a high electric conductivity and is unlikely to generate insoluble compounds by reaction with ions removed from theion exchanger 76, the electric power consumption in the regeneration section can be reduced by a lowered electric resistance of the regeneration liquid. Additionally, insoluble compounds (by-products) produced by reaction with ionic impurities can be prevented from being attached to thediaphragm 86. Accordingly, the electric resistance can be prevented from being varied between theprocess electrode 72 and thefeed electrode 74. Thus, difficulties in control can be eliminated. - After completion of the electrolytic process, electrical connection is interrupted between the
power supply 58, theprocess electrode 72, and thefeed electrode 74, and between thepower supply 96, theprocess electrode 72, and theregeneration electrode 84. Further, the rotation of thesubstrate holder 54 and the scroll movement of the electrode table 56 are stopped. Then, thesubstrate holder 54 is raised, and thearm 52 is moved to transfer the substrate W that has been subjected to the electrolytic process into a subsequent process. - As described above, in the present embodiment, pure water, preferably ultrapure water is supplied between the electrode table 56 and the substrate W. When an electrolytic process is performed with pure water or ultrapure water, which contains no electrolytes, it is possible to prevent excessive impurities such as electrolytes from being attached onto or remaining on a surface of the substrate W. Further, copper ions dissolved by the electrolytic process can immediately be captured by the
ion exchanger 76 through the ion exchange reaction. Accordingly, dissolved copper ions are prevented from being deposited on other portions of the substrate W and from oxidized and converted into fine particles which would contaminate the surface of the substrate W. - Ultrapure water has a large specific resistance, and a current is unlikely to flow through ultrapure water. Accordingly, in order to reduce an electric resistance, the electrode and the workpiece are disposed at nearest positions, or an ion exchanger is disposed between the electrode and the workpiece. With the above electrolytic solution, the electric resistance can further be reduced, and thus the electric power consumption can be reduced. In the process using an electrolytic solution, the workpiece is processed at an area that is slightly larger than the process electrode. However, with a combination of ultrapure water and an ion exchanger, since a current hardly flows through ultrapure water, the workpiece is processed only at an area that faces the process electrode and the ion exchanger.
- If a process voltage and a current density are increased in order to increase a processing rate, electric charge may occur in a case of a large electric resistance between the electrode and the substrate (workpiece). Such electric charge causes pitching on a surface of the workpiece, thereby making it difficult to maintain uniformity or planarization of the surface of the workpiece. However, when the
ion exchanger 76 is brought into contact with the substrate W, the electric resistance is so small that electric charge can be prevented from being caused. - In the present embodiment, the feed electrodes serve as an anode to process copper. However, when the feed electrodes are configured to serve as a cathode, a removal process of aluminum or silicon can be performed. In this case, the feed electrodes and the process electrodes are configured to have the same polarity. Specifically, when the process electrodes are configured to serve as a cathode, into which positive charges flow from an electrolytic processing liquid, ionic process products accumulating on the
ion exchanger 76 can continuously be discharged. Accordingly, an electrolytic process can be continued for a long term. - Further, in the above embodiment, the electrode table 56 makes a scroll movement while the substrate W is rotated. The electrode table 56 and the substrate W can make any movement as long as they move relative to each other. For example, one of the electrode table 56 and the substrate W may be rotated, or both of them may be rotated. In the above embodiment, the
substrate holder 54 attracts and holds the substrate W in a state such that the surface of the substrate W faces downward (in a face-down manner). However, the substrate W may be held in a state such that the surface of the substrate W faces upward (in a face-up manner). - Although certain preferred embodiments of the present invention have been shown and described in detail, it should be understood that various changes and modifications may be made therein without departing from the scope of the appended claims.
- The present invention is suitable for use in an electrolytic processing apparatus for processing a conductive material formed on a surface of a substrate such as a semiconductor wafer or removing impurities attached to the surface of the substrate.
Claims (8)
1. An electrolytic processing apparatus comprising:
a feed electrode configured to feed an electric current to a conductive material formed on a workpiece;
a contact member configured to be brought into contact with or close to the workpiece;
a process electrode operable to perform an electrolytic process on the conductive material formed on the workpiece;
an electrolytic processing liquid source operable to supply an electrolytic processing liquid between the workpiece and said contact member;
a regeneration liquid chamber configured to immerse said process electrode in a regeneration liquid;
a regeneration liquid supply source operable to supply the regeneration liquid to said regeneration liquid chamber;
a regeneration electrode spaced from said process electrode;
a power supply operable to apply a voltage between said feed electrode, said process electrode, and said regeneration electrode; and
a controller operable to control the voltage applied between said feed electrode, said process electrode, and said regeneration electrode so that said feed electrode has a potential higher than said process electrode and the same polarity as said process electrode, and that said process electrode has a potential higher than said regeneration electrode.
2. The electrolytic processing apparatus as recited in claim 1 , further comprising an insulation member disposed between said contact member and said process electrode, said insulation member having liquid permeability.
3. The electrolytic processing apparatus as recited in claim 2 , further comprising a diaphragm disposed between said contact member and said insulation member so as to separate the electrolytic processing liquid and said regeneration liquid.
4. The electrolytic processing apparatus as recited in claim 3 , wherein said diaphragm comprises an ion exchange film.
5. The electrolytic processing apparatus as recited in claim 1 , wherein said contact member comprises an ion exchanger.
6. The electrolytic processing apparatus as recited in claim 1 , wherein said process electrode has liquid permeability.
7. The electrolytic processing apparatus as recited in claim 1 , wherein said controller is operable to control potentials of said feed electrode, said process electrode, and said regeneration electrode, or currents flowing through said feed electrode, said process electrode, and said regeneration electrode.
8. The electrolytic processing apparatus as recited in claim 7 , wherein said controller is operable to control the current flowing through said process electrode so as to be equal to 1 to 30% of the current flowing through said feed electrode or said regeneration electrode.