A method of iron ore concentration in which as iron ore the impounded rejects of iron ore and/or impounded substandard iron ores are used, and as an useful component in concentrated raw material hematite is used, in the case, then extracted raw material is used for forming a slurry that is subjected to screening, the resulting oversize product of size-class above 1 mm is forwarded to a dump, and the undersize product is subjected to classification in a hydrocyclone, which discharge with particle size -003 mm is forwarded to the dump and sands of grain size 0.03 mm are concentrated at the first stage of hydraulic gravity concentration, for example, in a conical separator, and the resulting sands are forwarded for hydraulic gravity concentration, for example, in a spiral separator, and the discharge is forwarded for the second stage of hydraulic gravity concentration - recleaning, for example, in the conical separator, which discharge is forwarded to the dump, and the sands as well as the sands of the first stage of hydraulic gravity separation in the separator are forwarded to hydraulic gravity concentration, for example, in the spiral separator, and then three technological flows are obtained: one of them – the discharge is forwarded to the dump, another flow - the intermediate product containing particles of enriched hematite is forwarded for re-classification in the hydrocyclone, and the third flow - hematite concentrate - is forwarded to condensation and dehydration.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
UAU201009218U UA54229U (en) | 2010-07-22 | 2010-07-22 | method of iron ore concentration |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
UAU201009218U UA54229U (en) | 2010-07-22 | 2010-07-22 | method of iron ore concentration |
Publications (1)
Publication Number | Publication Date |
---|---|
UA54229U true UA54229U (en) | 2010-10-25 |
Family
ID=50740607
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
UAU201009218U UA54229U (en) | 2010-07-22 | 2010-07-22 | method of iron ore concentration |
Country Status (1)
Country | Link |
---|---|
UA (1) | UA54229U (en) |
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
RU2540173C2 (en) * | 2012-10-29 | 2015-02-10 | Руслан Петрович Цыплаков | Iron-ore raw material benefication method |
-
2010
- 2010-07-22 UA UAU201009218U patent/UA54229U/en unknown
Cited By (1)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
RU2540173C2 (en) * | 2012-10-29 | 2015-02-10 | Руслан Петрович Цыплаков | Iron-ore raw material benefication method |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
CN105312148B (en) | Beneficiation and enrichment method suitable for associated scheelite in molybdenite flotation tailings | |
CN101664715B (en) | Ore-dressing technique capable of effectively improving comprehensive utilization rate of mine resources | |
PH12019502827A1 (en) | Beneficiation of values from ores with a heap leach process | |
Tripathy et al. | Characterisation and separation studies of Indian chromite beneficiation plant tailing | |
RU2533792C2 (en) | Method of obtaining of bulk concentrate from ferruginous quartzites | |
RU2432207C1 (en) | Method of dressing composite iron ores | |
CN106311441B (en) | Vanadium titano-magnetite multi-metallic minerals separation beneficiation method | |
RU2388544C1 (en) | Procedure for production of collective concentrate out of mixed fine ingrained iron ore | |
Xiao et al. | The liberation effect of magnetite fine ground by vertical stirred mill and ball mill | |
CN106733107A (en) | low-grade iron ore beneficiation method | |
Nunna et al. | Beneficiation strategies for removal of silica and alumina from low-grade hematite-goethite iron ores | |
CN107638950A (en) | A kind of flotation method of nonferrous metal ores | |
Rosa et al. | Comparing ball and vertical mills performance: An industrial case study | |
AU2011308090B2 (en) | A method of sorting ore | |
RU2290999C2 (en) | Method for concentration of iron ores | |
UA54229U (en) | method of iron ore concentration | |
RU2751185C1 (en) | Method for increasing quality of magnetite concentrates | |
RU2457035C1 (en) | Method of dressing iron-bearing ores | |
RU2010147675A (en) | METHOD FOR ENRICHMENT OF IRON RAW MATERIALS | |
RU2540173C2 (en) | Iron-ore raw material benefication method | |
CN108405179A (en) | A kind of method of magnetic separation-roasting-magnetic separation process recycling magnetic tailing | |
CN111013809A (en) | Mineral processing technology for separating, grinding, sorting, upgrading and tailing reducing of lava ore | |
Mohanty et al. | High intensity magnetic separation of iron ore slime and its limitations | |
Maharaj et al. | The effect of the design of a secondary grinding circuit on platinum flotation from a UG-2 ore | |
Opalev et al. | Substantiation of Energy-Saving Technology for Ferruginous Quartzites Processing Using Magnetic-Gravity Processing Methods |