TWI408448B - Mother panel and fabricating method of display panel - Google Patents

Mother panel and fabricating method of display panel Download PDF

Info

Publication number
TWI408448B
TWI408448B TW98134189A TW98134189A TWI408448B TW I408448 B TWI408448 B TW I408448B TW 98134189 A TW98134189 A TW 98134189A TW 98134189 A TW98134189 A TW 98134189A TW I408448 B TWI408448 B TW I408448B
Authority
TW
Taiwan
Prior art keywords
mother
mother substrate
panel
display panel
body portion
Prior art date
Application number
TW98134189A
Other languages
Chinese (zh)
Other versions
TW201113591A (en
Inventor
Chung Jen Ma
Yen Po Lu
Chia Ju Yang
Yu Fu Tsai
Kuang Tse Tu
Chi Hung Yang
Original Assignee
Innolux Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Innolux Corp filed Critical Innolux Corp
Priority to TW98134189A priority Critical patent/TWI408448B/en
Publication of TW201113591A publication Critical patent/TW201113591A/en
Application granted granted Critical
Publication of TWI408448B publication Critical patent/TWI408448B/en

Abstract

A mother panel for being divided into a plurality of display panels is provided. The mother panel includes a first mother substrate, a second mother substrate correspondingly disposed above the first mother substrate, and at least one first blocking structure. The first mother substrate includes a plurality of display panel regions and a peripheral region surrounding the display panel regions. The first blocking structure is disposed correspondingly to the peripheral region and is on the first mother substrate or on the second mother substrate. The first blocking structure includes a first main body and at least two flow guiding parts, wherein the flow guiding parts are connected to two sides of the first main body, and a first containing space is formed between the first main body and the flow guiding parts. The first containing space can receive the connecting sealant for binding the first mother substrate and the second mother substrate and block the entering of chemical solution for thinning the mother panel into the display panel regions.

Description

母面板及顯示面板的製作方法 Mother panel and display panel manufacturing method

本發明是有關於一種母面板(mother panel)及顯示面板的製作方法,且特別是有關於一種可控制塗膠範圍以及可防止薄化化學液的進入之母面板、及經由此母面板製作顯示面板的方法。 The present invention relates to a mother panel and a method of manufacturing the display panel, and more particularly to a mother panel capable of controlling the range of the glue application and preventing the entry of the thinned chemical liquid, and displaying the display through the mother panel The method of the panel.

顯示裝置已經成為重要的人機界面。目前的電子市場強調輕、薄、短、小的趨勢。對於行動電話、數位相機、攝錄放影機、個人數位助理等產品來說更是如此。因此,如何將顯示裝置的玻璃基板的厚度減薄,即成為重要的課題。 Display devices have become an important human-machine interface. The current electronics market emphasizes the trend of light, thin, short and small. This is especially true for products such as mobile phones, digital cameras, camcorders, and personal digital assistants. Therefore, how to reduce the thickness of the glass substrate of the display device becomes an important issue.

在製作使用於顯示裝置中的顯示面板時,一般是經由分割一個母面板而得到多個顯示面板。圖1A是習知的母面板的立體示意圖。圖1B是圖1A之母面板的俯視示意圖。請同時參照圖1A與圖1B,母面板100是由第一母基板110、第二母基板120、多個擬框膠130(dummy seal)、接合框膠140及多個密封框膠150(繪示於圖1B中)所構成。母面板100具有多個顯示面板區域102與圍繞這些顯示面板區域102的周邊區104,其中,利用密封框膠150圍繞出多個顯示面板區域102。 When a display panel used in a display device is produced, a plurality of display panels are generally obtained by dividing one mother panel. 1A is a schematic perspective view of a conventional mother panel. FIG. 1B is a top plan view of the mother panel of FIG. 1A. Referring to FIG. 1A and FIG. 1B simultaneously, the mother panel 100 is composed of a first mother substrate 110, a second mother substrate 120, a plurality of dummy seals 130, a joint frame glue 140, and a plurality of seal frame glues 150. This is shown in Figure 1B. The mother panel 100 has a plurality of display panel regions 102 and a peripheral region 104 surrounding the display panel regions 102, wherein a plurality of display panel regions 102 are surrounded by a seal sealant 150.

在母面板100的周邊區104所設置的多個擬框膠130呈一字型排列,並且支撐於第一母基板110與第二母基板120之間。接合框膠140塗佈在周邊區104,以接合第 一母基板110與第二母基板120。並且,可在第一母基板110或第二母基板120上設置對位標記160,以準確接合第一母基板110與第二母基板120,而形成母面板100。 The plurality of pseudo-frame glues 130 disposed in the peripheral region 104 of the mother panel 100 are arranged in a line shape and supported between the first mother substrate 110 and the second mother substrate 120. The joint frame glue 140 is coated on the peripheral region 104 to join the first A mother substrate 110 and a second mother substrate 120. Moreover, the alignment mark 160 may be disposed on the first mother substrate 110 or the second mother substrate 120 to accurately bond the first mother substrate 110 and the second mother substrate 120 to form the mother panel 100.

其中,位在密封框膠150外側的接合框膠140係作為密封第一母基板110和第二母基板120接合後所夾持的空間,以避免後續玻璃基板減薄製程中,蝕刻化學液的滲入。而使用擬框膠130的目的則為了控制接合框膠140的滲入範圍。 The bonding frame glue 140 located outside the sealing frame glue 150 serves as a space for sealing the first mother substrate 110 and the second mother substrate 120 after the bonding, so as to avoid etching the chemical liquid in the subsequent thinning process of the glass substrate. Infiltration. The purpose of using the quasi-frame glue 130 is to control the penetration range of the joint sealant 140.

然而,在小尺寸顯示面板的情形下,於塗佈接合框膠140時,由於接合框膠140容易經由擬框膠130而向母面板100的內部流動,而形成滲膠過深的問題。圖1C是圖1B之A區域的放大示意圖。請參照圖1C,由於可允許滲膠的空間較小,接合框膠140容易流動到位於顯示面板區域102旁的端子部106,特別是端子部106具有電子元件與線路(未繪示),因此,將造成端子部106的電子元件與線路失效,因而造成顯示面板的報廢。 However, in the case of a small-sized display panel, when the bonding of the sealant 140 is applied, since the joint sealant 140 easily flows into the interior of the mother panel 100 via the quasi-frame seal 130, a problem that the gel-penetration is too deep is formed. Fig. 1C is an enlarged schematic view of a region A of Fig. 1B. Referring to FIG. 1C, since the space for allowing the bleed is small, the joint frame glue 140 easily flows to the terminal portion 106 located beside the display panel region 102, and in particular, the terminal portion 106 has electronic components and wirings (not shown), This will cause the electronic components and wiring of the terminal portion 106 to fail, thereby causing the display panel to be scrapped.

在完成母面板100的製作後,會將母面板100浸於蝕刻化學液中,以將第一母基板110與第二母基板120的厚度減薄。圖1D是圖1B之B區域的放大示意圖。請參照圖1D,由於對位標記160與擬框膠130之間可能存在高度差,所以在第一母基板110與第二母基板120之間造成間隙170。若是將母面板100浸於蝕刻化學液CS中時,使得蝕刻化學液CS會經由間隙170而滲入母面板100內。如此一來,蝕刻化學液CS將侵蝕端子部106中的電子元件與線路,或是從母面板100的內部侵蝕第一 母基板110與第二母基板120,如此,將使得母面板100報廢。 After the fabrication of the mother panel 100 is completed, the mother panel 100 is immersed in an etching chemistry to reduce the thickness of the first mother substrate 110 and the second mother substrate 120. Fig. 1D is an enlarged schematic view of a region B of Fig. 1B. Referring to FIG. 1D , since there may be a height difference between the alignment mark 160 and the quasi-frame glue 130 , a gap 170 is formed between the first mother substrate 110 and the second mother substrate 120 . When the mother panel 100 is immersed in the etching chemical liquid CS, the etching chemical liquid CS is infiltrated into the mother panel 100 via the gap 170. In this way, the etching chemical solution CS will erode the electronic components and the wires in the terminal portion 106 or erode the first from the inside of the mother panel 100. The mother substrate 110 and the second mother substrate 120, as such, will cause the mother panel 100 to be scrapped.

有鑑於此,本發明提供一種母面板,能夠防止接合框膠滲入過深以及蝕刻化學液滲入母面板。 In view of the above, the present invention provides a mother panel capable of preventing penetration of the joint frame glue and penetration of the etching chemical liquid into the mother panel.

本發明又提供一種顯示面板的製作方法,利用上述的母面板分割成多個顯示面板,而能夠提升顯示面板的製作良率。 The present invention further provides a method for fabricating a display panel, which is divided into a plurality of display panels by using the above-described mother panel, thereby improving the production yield of the display panel.

基於上述,本發明提出一種母面板,其適於被分割成多個顯示面板,包括一第一母基板、一第二母基板以及至少一第一阻擋結構。第一母基板具有多個顯示面板區域、以及圍繞顯示面板區域的一周邊區。第二母基板對應配置於第一母基板上方。第一阻擋結構對應周邊區而配置於第一母基板或第二母基板上。第一阻擋結構包括一第一主體部以及至少二第一導流部,其中第一導流部連接於第一主體部的兩側,且第一主體部與第一導流部形成一第一容納空間。 Based on the above, the present invention provides a mother panel that is adapted to be divided into a plurality of display panels, including a first mother substrate, a second mother substrate, and at least one first blocking structure. The first mother substrate has a plurality of display panel regions and a peripheral region surrounding the display panel regions. The second mother substrate is correspondingly disposed above the first mother substrate. The first blocking structure is disposed on the first mother substrate or the second mother substrate corresponding to the peripheral region. The first blocking structure includes a first body portion and at least two first flow guiding portions, wherein the first guiding portion is connected to two sides of the first body portion, and the first body portion and the first guiding portion form a first Accommodate space.

在本發明之一實施例中,上述之第一主體部與每一第一導流部之間夾有一第一角度,且第一角度為大於等於90度且小於180度。 In an embodiment of the invention, a first angle is formed between the first body portion and each of the first flow guiding portions, and the first angle is greater than or equal to 90 degrees and less than 180 degrees.

在本發明之一實施例中,上述之母面板更包括至少二輔助導流部,每一輔助導流部分別連接於每一第一導流部,每一輔助導流部與每一第一導流部之間夾有一第二角度,且第二角度為大於180度且小於360度。 In an embodiment of the present invention, the mother panel further includes at least two auxiliary flow guiding portions, each auxiliary guiding portion is respectively connected to each of the first guiding portions, and each of the auxiliary guiding portions and each of the first guiding portions A second angle is sandwiched between the flow guiding portions, and the second angle is greater than 180 degrees and less than 360 degrees.

在本發明之一實施例中,上述之第一主體部的形狀包括V字形、半圓形或是一字形。 In an embodiment of the invention, the shape of the first body portion includes a V shape, a semicircle shape or a shape.

在本發明之一實施例中,上述之母面板更包括至少一第二阻擋結構,與第一阻擋結構為交錯配置,其中第二阻擋結構包括一第二主體部以及至少二第二導流部,第二導流部連接於第二主體部的兩側,其中第二主體部與第二導流部形成一第二容納空間。 In an embodiment of the present invention, the mother panel further includes at least one second blocking structure in a staggered configuration with the first blocking structure, wherein the second blocking structure includes a second body portion and at least two second flow guiding portions The second flow guiding portion is connected to two sides of the second body portion, wherein the second body portion and the second flow guiding portion form a second receiving space.

在本發明之一實施例中,上述之母面板更包括一接合框膠,對應周邊區而設置於第一母基板或第二母基板上,且第一容納空間適於容置接合框膠。 In an embodiment of the present invention, the mother panel further includes a joint frame glue disposed on the first mother substrate or the second mother substrate corresponding to the peripheral region, and the first receiving space is adapted to receive the joint frame glue.

在本發明之一實施例中,上述之母面板更包括至少一對位標記,對應周邊區而配置於第一母基板或第二母基板上,對位標記位於第一容納空間內。 In an embodiment of the invention, the mother panel further includes at least one pair of bit marks disposed on the first mother substrate or the second mother substrate corresponding to the peripheral region, and the alignment mark is located in the first receiving space.

在本發明之一實施例中,上述之母面板更包括多個密封框膠,設置於第一母基板或第二母基板上,每一密封框膠位於每一顯示面板區域的周圍。 In an embodiment of the invention, the mother panel further comprises a plurality of sealing frame glues disposed on the first mother substrate or the second mother substrate, each sealing frame glue being located around each display panel region.

在本發明之一實施例中,上述每一密封框膠具有一液晶注入口。 In an embodiment of the invention, each of the sealant seals has a liquid crystal injection port.

在本發明之一實施例中,上述之第一阻擋結構的材質包括熱固化膠或紫外光固化膠。 In an embodiment of the invention, the material of the first blocking structure comprises a thermosetting adhesive or an ultraviolet curing adhesive.

基於上述,本發明又提出一種顯示面板的製作方法,包括下列步驟。首先,提供一第一母基板,第一母基板具有多個顯示面板區域、以及圍繞顯示面板區域的一周邊區。再來,提供一第二母基板,對應配置於第一母基板上方。接著,對應周邊區於第一母基板或第二母 基板上形成至少一第一阻擋結構,且第一阻擋結構包括一第一主體部以及至少二第一導流部,其中第一導流部連接於第一主體部的兩側,且第一主體部與第一導流部形成一第一容納空間。繼之,接合第一母基板與第二母基板,以形成一母面板。之後,分割母面板,以形成多個顯示面板。 Based on the above, the present invention further provides a method for fabricating a display panel, including the following steps. First, a first mother substrate is provided, the first mother substrate having a plurality of display panel regions and a peripheral region surrounding the display panel region. Furthermore, a second mother substrate is provided, correspondingly disposed above the first mother substrate. Then, corresponding to the peripheral area on the first mother substrate or the second mother Forming at least one first blocking structure on the substrate, and the first blocking structure comprises a first body portion and at least two first guiding portions, wherein the first guiding portion is connected to both sides of the first body portion, and the first body The portion and the first flow guiding portion form a first receiving space. Then, the first mother substrate and the second mother substrate are bonded to form a mother panel. Thereafter, the mother panel is divided to form a plurality of display panels.

在本發明之一實施例中,上述之顯示面板的製作方法更包括形成至少二輔助導流部,每一輔助導流部分別連接於每一第一導流部,每一輔助導流部與每一第一導流部之間夾有一第二角度,且第二角度為大於等於180度且小於360度。 In an embodiment of the present invention, the method for fabricating the display panel further includes forming at least two auxiliary flow guiding portions, each auxiliary flow guiding portion being respectively connected to each of the first guiding portions, and each of the auxiliary guiding portions is A second angle is sandwiched between each of the first flow guiding portions, and the second angle is greater than or equal to 180 degrees and less than 360 degrees.

在本發明之一實施例中,上述之第一主體部的形狀包括V字形、半圓形或是一字形。 In an embodiment of the invention, the shape of the first body portion includes a V shape, a semicircle shape or a shape.

在本發明之一實施例中,上述之顯示面板的製作方法更包括形成至少一第二阻擋結構,與第一阻擋結構為交錯配置,其中第二阻擋結構包括一第二主體部以及至少二第二導流部,第二導流部連接於第二主體部的兩側,其中第二主體部與第二導流部形成一第二容納空間。 In an embodiment of the present invention, the method for fabricating the display panel further includes forming at least one second blocking structure in a staggered configuration with the first blocking structure, wherein the second blocking structure includes a second body portion and at least two The second flow guiding portion is connected to two sides of the second body portion, wherein the second body portion and the second flow guiding portion form a second receiving space.

在本發明之一實施例中,上述之接合第一母基板與第二母基板的方法包括對應周邊區於第一母基板或第二母基板上形成一接合框膠,以接合第一母基板與第二母基板,其中,第一容納空間內適於容置接合框膠。 In an embodiment of the invention, the method for bonding the first mother substrate and the second mother substrate comprises forming a bonding frame glue on the first mother substrate or the second mother substrate corresponding to the peripheral region to bond the first mother substrate. And the second mother substrate, wherein the first receiving space is adapted to receive the bonding frame glue.

在本發明之一實施例中,於接合第一母基板與第二母基板之前,更包括對應周邊區而於第一母基板或第二母基板上形成至少一對位標記,且對位標記位於第一容 納空間內。 In an embodiment of the present invention, before the first mother substrate and the second mother substrate are joined, at least a pair of bit marks are formed on the first mother substrate or the second mother substrate, and the alignment mark is formed corresponding to the peripheral region. Located in the first capacity Within the nano space.

在本發明之一實施例中,上述之顯示面板的製作方法更包括於第一母基板或第二母基板上形成多個密封框膠,每一密封框膠位於每一顯示面板區域的周圍。 In an embodiment of the present invention, the method for manufacturing the display panel further includes forming a plurality of sealing frame glues on the first mother substrate or the second mother substrate, each sealing frame glue being located around each display panel region.

在本發明之一實施例中,上述每一密封框膠具有一液晶注入口。 In an embodiment of the invention, each of the sealant seals has a liquid crystal injection port.

在本發明之一實施例中,在形成母面板之後且於分割母面板之前,更包括將母面板浸於一化學液中而進行一薄化製程,化學液適於被第一阻擋結構阻擋,且滲入母面板中的化學液適於容置於第一容納空間中。 In an embodiment of the present invention, after forming the mother panel and before dividing the mother panel, the method further comprises: immersing the mother panel in a chemical liquid to perform a thinning process, and the chemical liquid is adapted to be blocked by the first barrier structure. And the chemical liquid infiltrated into the mother panel is adapted to be accommodated in the first receiving space.

在本發明之一實施例中,顯示面板的製作方法更包括於每一顯示面板中注入一液晶層。 In an embodiment of the invention, the method for fabricating the display panel further includes injecting a liquid crystal layer into each of the display panels.

在本發明之一實施例中,上述之第一阻擋結構的材質包括熱固化膠或紫外光固化膠。 In an embodiment of the invention, the material of the first blocking structure comprises a thermosetting adhesive or an ultraviolet curing adhesive.

本發明之母面板採用配置於母基板之周邊區上的阻擋結構,而阻擋結構具有主體部以及導流部,且主體部與導流部形成一容納空間。因此,阻擋結構能夠延緩接合框膠的滲膠速度,以防止接合框膠滲入母面板。此外,阻擋結構也能夠阻擋用於薄化製程的化學液進入母面板內部,以避免化學液侵蝕母面板的內部。因此,利用上述的母面板所製得的顯示面板具有較佳的製作良率。 The mother panel of the present invention adopts a blocking structure disposed on a peripheral area of the mother substrate, and the blocking structure has a main body portion and a flow guiding portion, and the main body portion and the flow guiding portion form a receiving space. Therefore, the barrier structure can delay the penetration speed of the joint sealant to prevent the joint frame glue from penetrating into the mother panel. In addition, the barrier structure can also block the chemical liquid used for the thinning process from entering the interior of the mother panel to prevent the chemical liquid from eroding the interior of the mother panel. Therefore, the display panel produced by using the above-described mother panel has a better manufacturing yield.

為讓本發明之上述和其他目的、特徵和優點能更明顯易懂,下文特舉較佳實施例,並配合所附圖式,作詳細說明如下。 The above and other objects, features and advantages of the present invention will become more <RTIgt;

本發明的母面板可應用於各種平面顯示面板的製作,諸如液晶顯示面板、有機電激發光顯示面板、電漿顯示面板等。並且,本發明的母面板特別適合應用在需要進行薄化製程的平面顯示面板中,利用第一阻擋結構即可有效地控制滲膠範圍與防止化學液進入母面板中。以下舉數個實施例進行說明,並非用以限定本發明的實施形態。 The mother panel of the present invention can be applied to the fabrication of various flat display panels, such as liquid crystal display panels, organic electroluminescent display panels, plasma display panels, and the like. Moreover, the mother panel of the present invention is particularly suitable for use in a flat display panel that requires a thinning process, and the first barrier structure can be used to effectively control the range of penetration and prevent chemical liquid from entering the mother panel. The following examples are given to illustrate and not to limit the embodiments of the invention.

圖2A是本發明較佳實施例的一種母面板的立體示意圖。圖2B為圖2A的母面板的俯視示意圖。請共同參照圖2A與圖2B,母面板200適於被分割成多個顯示面板DP,此母面板200包括一第一母基板210、一第二母基板220以及至少一第一阻擋結構230。第一母基板210具有多個顯示面板區域212、以及圍繞顯示面板區域212的一周邊區214。第二母基板220對應配置於第一母基板210上方。第一阻擋結構230對應周邊區214而配置於第一母基板210或第二母基板220上。第一阻擋結構230包括一第一主體部230a以及至少二第一導流部230b,第一導流部230b連接於第一主體部230a的兩側,且第一主體部230a與第一導流部230b形成第一容納空間S1。 2A is a perspective view of a mother panel in accordance with a preferred embodiment of the present invention. 2B is a top plan view of the mother panel of FIG. 2A. Referring to FIG. 2A and FIG. 2B together, the mother panel 200 is adapted to be divided into a plurality of display panels DP. The mother panel 200 includes a first mother substrate 210, a second mother substrate 220, and at least one first blocking structure 230. The first mother substrate 210 has a plurality of display panel regions 212 and a peripheral region 214 surrounding the display panel region 212. The second mother substrate 220 is disposed above the first mother substrate 210 . The first blocking structure 230 is disposed on the first mother substrate 210 or the second mother substrate 220 corresponding to the peripheral region 214. The first blocking structure 230 includes a first body portion 230a and at least two first guiding portions 230b. The first guiding portion 230b is connected to two sides of the first body portion 230a, and the first body portion 230a and the first guiding portion The portion 230b forms the first accommodation space S1.

請繼續參照圖2A與圖2B,在一較佳實施例中,第一主體部230a與每一第一導流部230b之間夾有一第一角度θ 1,且第一角度θ 1為大於等於90度且小於180度。如圖2B所示,第一主體部230a的形狀例如是一字形且第一角度θ 1等於90度,因此第一阻擋結構230可 呈ㄇ字形。第一阻擋結構230的材質包括熱固化膠或紫外光固化膠。 2A and 2B, in a preferred embodiment, a first angle θ 1 is sandwiched between the first body portion 230a and each of the first flow guiding portions 230b, and the first angle θ 1 is greater than or equal to 90 degrees and less than 180 degrees. As shown in FIG. 2B, the shape of the first body portion 230a is, for example, a shape and the first angle θ 1 is equal to 90 degrees, so the first blocking structure 230 can be It is in a glyph shape. The material of the first blocking structure 230 includes a thermosetting adhesive or an ultraviolet curing adhesive.

請繼續參照圖2A與圖2B,母面板200更包括一接合框膠240,對應周邊區214而設置於第一母基板210或第二母基板220上,且第一容納空間S1適於容置接合框膠240。換句話說,利用接合框膠240來接合第一母基板210與第二母基板220,且接合框膠240的範圍會因為接合而擴張。另外,母面板200更包括多個密封框膠250,設置於第一母基板210或第二母基板220上,每一密封框膠250位於每一顯示面板區域212的周圍。值得注意的是,第一阻擋結構230可以控制滲膠的速度與範圍。圖2C是圖2B之C區域的放大示意圖。請參照圖2C,由於第一阻擋結構230具有第一導流部230b,所以第一阻擋結構230可以延緩接合框膠240的滲膠速度、且限制接合框膠240的滲膠範圍。如此一來,可防止接合框膠240流動到顯示面板區域212旁的端子部206上,所以端子部206的電子元件(未繪示)與線路(未繪示)不會受到損壞。 2A and 2B, the mother panel 200 further includes a bonding frame 240 disposed on the first mother substrate 210 or the second mother substrate 220 corresponding to the peripheral region 214, and the first receiving space S1 is adapted to be accommodated. The frame glue 240 is joined. In other words, the first mother substrate 210 and the second mother substrate 220 are bonded by the joint sealant 240, and the extent of the joint sealant 240 is expanded by the joint. In addition, the mother panel 200 further includes a plurality of sealing frame glues 250 disposed on the first mother substrate 210 or the second mother substrate 220 , and each sealing frame glue 250 is located around each display panel region 212 . It is worth noting that the first blocking structure 230 can control the speed and range of the bleed. 2C is an enlarged schematic view of a region C of FIG. 2B. Referring to FIG. 2C , since the first blocking structure 230 has the first guiding portion 230 b , the first blocking structure 230 can delay the bleeding speed of the bonding frame glue 240 and limit the penetration range of the bonding frame glue 240 . In this way, the bonding frame filler 240 can be prevented from flowing to the terminal portion 206 beside the display panel region 212, so that the electronic components (not shown) of the terminal portion 206 and the wires (not shown) are not damaged.

請同時參照圖2A與圖2B,母面板200可更包括至少一對位標記260,對應周邊區214而配置於第一母基板210或第二母基板220上,且對位標記260位於第一容納空間S1內。值得注意的是,對位標記260與第一阻擋結構230之間可能會有高度差,此高度差可能導致第一母基板210與第二母基板220之間產生間隙。如此一來,在後續的薄化製程中,化學液很容易滲入母面板200中 而侵蝕內部元件。 Referring to FIG. 2A and FIG. 2B simultaneously, the mother panel 200 may further include at least one pair of bit marks 260 disposed on the first mother substrate 210 or the second mother substrate 220 corresponding to the peripheral region 214, and the alignment mark 260 is located at the first position. The accommodation space S1. It should be noted that there may be a height difference between the alignment mark 260 and the first barrier structure 230, which may cause a gap between the first mother substrate 210 and the second mother substrate 220. In this way, in the subsequent thinning process, the chemical liquid easily penetrates into the mother panel 200. And eroding internal components.

圖2D是圖2B之D區域的放大示意圖。請參照圖2D,於本實施例中,對位標記260位於第一容納空間S1內且被第一阻擋結構230所圍繞。亦即,即使化學液CS從間隙270進入母面板200,第一阻擋結構230仍然能夠有效地擋住化學液CS,使化學液CS容置於第一容納空間S1中。也就是說,在將母面板200浸於化學液CS中的薄化製程中,第一阻擋結構230可有效防止母面板200的內部元件受到化學液CS的破壞。 2D is an enlarged schematic view of a region D of FIG. 2B. Referring to FIG. 2D , in the embodiment, the alignment mark 260 is located in the first receiving space S1 and surrounded by the first blocking structure 230 . That is, even if the chemical liquid CS enters the mother panel 200 from the gap 270, the first barrier structure 230 can effectively block the chemical liquid CS, so that the chemical liquid CS is accommodated in the first accommodation space S1. That is, in the thinning process of immersing the mother panel 200 in the chemical liquid CS, the first barrier structure 230 can effectively prevent the internal components of the mother panel 200 from being damaged by the chemical liquid CS.

圖3A~圖3C為本發明較佳實施例的數種第一阻擋結構的示意圖。請先參照圖3A,此第一阻擋結構232與如圖2A~2B所繪示的第一阻擋結構230類似,相同的構件以相同的標號表示,在此不予以重述。如圖3A所示,此第一阻擋結構232更包括至少二輔助導流部230c,每一輔助導流部230c分別連接於每一第一導流部230b,每一輔助導流部230c與每一第一導流部230b之間夾有一第二角度θ 2,且第二角度θ 2為大於180度且小於360度。輔助導流部230c能夠進一步將接合框膠240或化學液CS導流至相反於顯示面板區域212的方向,進而防止接合框膠240或化學液CS滲入母面板200中。 3A-3C are schematic views of several first blocking structures in accordance with a preferred embodiment of the present invention. Referring to FIG. 3A, the first blocking structure 232 is similar to the first blocking structure 230 shown in FIGS. 2A-2B, and the same components are denoted by the same reference numerals and will not be described again. As shown in FIG. 3A, the first blocking structure 232 further includes at least two auxiliary guiding portions 230c. Each of the auxiliary guiding portions 230c is respectively connected to each of the first guiding portions 230b, and each of the auxiliary guiding portions 230c and each A first angle θ 2 is sandwiched between the first flow guiding portions 230b, and the second angle θ 2 is greater than 180 degrees and less than 360 degrees. The auxiliary flow guiding portion 230c can further guide the bonding frame rubber 240 or the chemical liquid CS to a direction opposite to the display panel region 212, thereby preventing the bonding of the sealant 240 or the chemical liquid CS from penetrating into the mother panel 200.

請再參照圖3B,此第一阻擋結構234與如圖2A~2B所繪示的第一阻擋結構230類似,相同的構件以相同的標號表示,在此不予以重述。特別是,在此實施例中,第一主體部230a的形狀為V字型。 Referring to FIG. 3B, the first blocking structure 234 is similar to the first blocking structure 230 shown in FIGS. 2A-2B, and the same components are denoted by the same reference numerals and will not be described again. In particular, in this embodiment, the shape of the first body portion 230a is V-shaped.

請再參照圖3C,此第一阻擋結構236的第一主體部 230a的形狀為半圓形。由於V字形或半圓形的構形具有更佳的導流以及容納流體的特性,因此可達到更好的防止接合框膠240或化學液CS滲入母面板200中的效果。 Referring to FIG. 3C again, the first body portion of the first blocking structure 236 The shape of 230a is semicircular. Since the V-shaped or semi-circular configuration has better conductance and fluid-containing characteristics, it is possible to achieve better prevention of the penetration of the joint sealant 240 or the chemical liquid CS into the mother panel 200.

此外,由於V字形或半圓形的構形具有導流以及容納的特性,第一阻擋結構(未繪示)的形狀也可以是V字形或半圓形。 In addition, the shape of the first barrier structure (not shown) may also be V-shaped or semi-circular due to the V-shaped or semi-circular configuration having the characteristics of conduction and accommodation.

圖4為本發明較佳實施例的另一種母面板的俯視示意圖。請參照圖4,此母面板300與圖2A、圖2B中所繪示之母面板200相似,相同的構件以相同的標號表示。特別是,在本實施例中,母面板300更包括至少一第二阻擋結構280,第二阻擋結構280包括一第二主體部280a以及至少二第二導流部280b,第二導流部280b連接於第二主體部280a的兩側,其中第二主體部280a與第二導流部280b形成一第二容納空間S2。 4 is a top plan view of another mother panel in accordance with a preferred embodiment of the present invention. Referring to FIG. 4, the mother panel 300 is similar to the mother panel 200 illustrated in FIGS. 2A and 2B, and the same components are denoted by the same reference numerals. In particular, in the embodiment, the mother panel 300 further includes at least one second blocking structure 280. The second blocking structure 280 includes a second body portion 280a and at least two second guiding portions 280b, and the second guiding portion 280b. It is connected to two sides of the second body portion 280a, wherein the second body portion 280a and the second flow guiding portion 280b form a second receiving space S2.

值得注意的是,第二阻擋結構280與第一阻擋結構230為交錯配置,這樣的配置可以促使接合框膠240與化學液(未繪示)朝向水平方向流動,以減緩上述兩者朝向顯示面板區域212的垂直流動速度。值得注意的是,第一阻擋結構230與第二阻擋結構280的構形可以不同。換言之,第一阻擋結構230與第二阻擋結構280可以是圖2A以及圖3A~圖3C或其他合適形狀的阻擋結構的組合,本發明並不加以限定。 It should be noted that the second blocking structure 280 and the first blocking structure 230 are in a staggered configuration. Such a configuration may cause the bonding glue 240 and the chemical liquid (not shown) to flow in a horizontal direction to slow the two toward the display panel. The vertical flow velocity of region 212. It should be noted that the configuration of the first blocking structure 230 and the second blocking structure 280 may be different. In other words, the first blocking structure 230 and the second blocking structure 280 may be a combination of the blocking structure of FIG. 2A and FIG. 3A to FIG. 3C or other suitable shapes, which is not limited by the present invention.

請再參照圖2A~圖2C,當母面板200是用以製作液晶顯示面板時,可使每一密封框膠250具有一液晶注入口(未繪示),當母基板200被分割成多個顯示面板DP 後,即可透過液晶注入口對於顯示面板DP進行液晶注入,而完成液晶顯示面板的製作。也就是說,雖然在圖式中是以使用液晶滴入(one drop fill,ODF)方式製作的母面板200為例,但本發明之母面板200也適於使用傳統液晶注入等其他方式來製作。 Referring to FIG. 2A to FIG. 2C, when the mother panel 200 is used to fabricate the liquid crystal display panel, each sealing frame adhesive 250 can have a liquid crystal injection port (not shown) when the mother substrate 200 is divided into a plurality of layers. Display panel DP After that, liquid crystal injection can be performed on the display panel DP through the liquid crystal injection port to complete the fabrication of the liquid crystal display panel. That is, although the mother panel 200 fabricated by using a one drop fill (ODF) method is exemplified in the drawings, the mother panel 200 of the present invention is also suitable for being fabricated by other methods such as conventional liquid crystal injection. .

下文將介紹以上述實施例之母面板200來製作顯示面板DP的方法。並且,此處是以液晶顯示面板為例而進行說明,母面板200並不僅限於液晶顯示面板的製作。 A method of manufacturing the display panel DP using the mother panel 200 of the above embodiment will be described below. Here, the liquid crystal display panel will be described as an example, and the mother panel 200 is not limited to the production of the liquid crystal display panel.

圖5是本發明較佳實施例的一種顯示面板的製作方法流程圖。請同時參照圖2A、圖2B以及圖5,首先,進行步驟S500,提供一第一母基板210,第一母基板210具有多個顯示面板區域212、以及圍繞顯示面板區域212的一周邊區214。此第一母基板210的材質可以是玻璃基板,並且第一母基板210可以是薄膜電晶體陣列基板。 FIG. 5 is a flow chart of a method for fabricating a display panel according to a preferred embodiment of the present invention. Referring to FIG. 2A, FIG. 2B and FIG. 5 simultaneously, first, step S500 is performed to provide a first mother substrate 210 having a plurality of display panel regions 212 and a peripheral region 214 surrounding the display panel region 212. The material of the first mother substrate 210 may be a glass substrate, and the first mother substrate 210 may be a thin film transistor array substrate.

請再參照圖2A、圖2B以及圖5,接著,進行步驟S502,提供一第二母基板220,對應配置於第一母基板210上方。此第二母基板220的材質可以是玻璃基板,並且第二母基板220可以是彩色濾光基板。 Referring to FIG. 2A, FIG. 2B and FIG. 5 again, step S502 is performed to provide a second mother substrate 220 corresponding to the first mother substrate 210. The material of the second mother substrate 220 may be a glass substrate, and the second mother substrate 220 may be a color filter substrate.

請繼續參照圖2A、圖2B以及圖5,然後,進行步驟S504,對應周邊區214於第一母基板210或第二母基板220上形成至少一第一阻擋結構230,且第一阻擋結構230包括一第一主體部230a以及至少二第一導流部230b,其中第一導流部230b連接於第一主體部230a的兩側,且第一主體部230a與第一導流部230b形成一第一容納空間S1。在此實施例中,第一阻擋結構230是形成於第一 母基板210上。特別是,如圖4所示,還可形成至少一第二阻擋結構280,與第一阻擋結構230為交錯配置。關於第一阻擋結構230與第二阻擋結構280的詳細結構已經陳述如上,各種實施的形態也如圖2A~圖4所示,在此即不予以重述。 Continuing to refer to FIG. 2A, FIG. 2B and FIG. 5, and then performing step S504, forming at least one first blocking structure 230 on the first mother substrate 210 or the second mother substrate 220 corresponding to the peripheral region 214, and the first blocking structure 230 The first body portion 230a and the at least two first flow guiding portions 230b are included, wherein the first guiding portion 230b is connected to two sides of the first body portion 230a, and the first body portion 230a forms a first portion with the first guiding portion 230b. The first accommodation space S1. In this embodiment, the first blocking structure 230 is formed in the first On the mother substrate 210. In particular, as shown in FIG. 4, at least one second barrier structure 280 may also be formed, which is in a staggered configuration with the first barrier structure 230. The detailed structure of the first blocking structure 230 and the second blocking structure 280 has been described above, and the various embodiments are also shown in FIGS. 2A to 4, and will not be repeated here.

另外,還可以於第一母基板210或第二母基板220上(本實施例是形成於第一母基板210上)形成多個密封框膠250,每一密封框膠250位於每一顯示面板區域212的周圍,且每一密封框膠250例如是具有一液晶注入口(未繪示)。 In addition, a plurality of sealing frame glues 250 may be formed on the first mother substrate 210 or the second mother substrate 220 (the present embodiment is formed on the first mother substrate 210), and each sealing frame glue 250 is located on each display panel. Around the region 212, each sealant 250 has, for example, a liquid crystal injection port (not shown).

請再參照圖2A、圖2B以及圖5,而後,進行步驟S506,接合第一母基板210與第二母基板220,以形成一母面板200。在一較佳實施例中,接合第一母基板210與第二母基板220的方法例如是對應周邊區214於第一母基板210或第二母基板220上形成一接合框膠240,以接合第一母基板210與第二母基板220,其中,第一容納空間S1內適於容置接合框膠240。 Referring to FIG. 2A, FIG. 2B and FIG. 5 again, step S506 is performed to bond the first mother substrate 210 and the second mother substrate 220 to form a mother panel 200. In a preferred embodiment, the method of bonding the first mother substrate 210 and the second mother substrate 220 is, for example, forming a bonding frame 240 on the first mother substrate 210 or the second mother substrate 220 corresponding to the peripheral region 214 to be bonded. The first mother substrate 210 and the second mother substrate 220 are adapted to receive the bonding frame glue 240 in the first receiving space S1.

特別是,為了使第一母基板210與第二母基板220之間的對位更為準確,於接合第一母基板210與第二母基板220(步驟S506)之前,更包括對應周邊區214而於第一母基板210或第二母基板220上形成至少一對位標記260,且對位標記260位於第一容納空間S1內。 In particular, in order to make the alignment between the first mother substrate 210 and the second mother substrate 220 more accurate, before the first mother substrate 210 and the second mother substrate 220 are joined (step S506), the corresponding peripheral region 214 is further included. At least a pair of bit marks 260 are formed on the first mother substrate 210 or the second mother substrate 220, and the alignment marks 260 are located in the first housing space S1.

值得注意的是,在利用接合框膠240接合第一母基板210、第二母基板220時,藉由第一阻擋結構230、第二阻擋結構280的設置而延緩接合框膠240的滲膠速 度,且可限制接合框膠240的滲膠範圍。如此,可防止接合框膠240滲入到端子部206中。 It is to be noted that, when the first mother substrate 210 and the second mother substrate 220 are joined by the bonding glue 240, the speed of the glue of the bonding frame 240 is delayed by the arrangement of the first blocking structure 230 and the second blocking structure 280. Degree, and can limit the penetration range of the joint seal 240. In this way, the joint sealant 240 can be prevented from penetrating into the terminal portion 206.

請繼續參照圖2A、圖2B以及圖5,繼之,進行步驟S508,分割母面板200,以形成多個顯示面板DP。分割母面板200的方式例如是習知的雷射切割,或是其他適合的切割方式。 2A, 2B, and 5, next, step S508 is performed to divide the mother panel 200 to form a plurality of display panels DP. The manner in which the mother panel 200 is divided is, for example, a conventional laser cutting or other suitable cutting method.

值得一提的是,如圖2D所示,為了使顯示面板DP符合輕薄的需求,會在形成母面板200(步驟S506)之後且於分割母面板200(步驟S508)之前,將母面板200浸於一化學液CS中以進行一薄化製程,化學液CS適於被第一阻擋結構230阻擋,且滲入母面板200中的化學液CS適於容置於第一容納空間S1中。 It is worth mentioning that, as shown in FIG. 2D, in order to meet the light and thin requirements of the display panel DP, the mother panel 200 is dipped after the mother panel 200 is formed (step S506) and before the mother panel 200 is divided (step S508). In a chemical solution CS to perform a thinning process, the chemical liquid CS is adapted to be blocked by the first barrier structure 230, and the chemical liquid CS penetrating into the mother panel 200 is adapted to be accommodated in the first accommodation space S1.

更詳細而言,即使化學液CS通過間隙270而進入母面板200,第一阻擋結構230可阻擋化學液CS,可防止母面板200受到化學液CS的破壞,進而能提升顯示面板的製作良率。 In more detail, even if the chemical liquid CS enters the mother panel 200 through the gap 270, the first barrier structure 230 can block the chemical liquid CS, which can prevent the mother panel 200 from being damaged by the chemical liquid CS, thereby improving the manufacturing yield of the display panel. .

在將母面板200分割成多個顯示面板DP後,可利用密封框膠250的液晶注入口(未繪示),於每一顯示面板DP中注入一液晶層(未繪示),而完成液晶顯示面板的製作。另外,第一阻擋結構230的材質包括熱固化膠或紫外光固化膠,並且,第一阻擋結構230的材質可與接合框膠240、對位標記260以及密封框膠250相同,因此,製作第一阻擋結構230、第二阻擋結構280與現有製程相容,不會造成生產成本的大幅增加。 After the mother panel 200 is divided into a plurality of display panels DP, a liquid crystal injection port (not shown) of the sealant 250 can be used to inject a liquid crystal layer (not shown) into each display panel DP to complete the liquid crystal. The production of the display panel. In addition, the material of the first blocking structure 230 includes a thermosetting adhesive or an ultraviolet curing adhesive, and the material of the first blocking structure 230 can be the same as that of the bonding frame glue 240, the alignment mark 260, and the sealing frame glue 250. A barrier structure 230 and a second barrier structure 280 are compatible with existing processes and do not cause a substantial increase in production costs.

綜上所述,本發明的母面板及顯示面板的製作方法 至少具有以下優點: In summary, the mother panel and the display panel of the present invention At least have the following advantages:

母面板具有阻擋結構以及由阻擋結構所構成的容納空間,阻擋結構可以延緩接合框膠的滲膠速度以及限制其滲膠範圍,因此,可以避免接合框膠滲入顯示面板區域而影響元件的性能。此外,阻擋結構可以阻擋且容納用於薄化母面板的化學液,以避免母面板的內部受到化學液的破壞,進而能提升顯示面板的製作良率。再者,製作阻擋結構與現有的顯示面板製程相容,不會造成生產成本的大幅增加。 The mother panel has a blocking structure and an accommodating space formed by the blocking structure. The blocking structure can delay the bleed speed of the joint framing and limit the bleed range thereof. Therefore, it is possible to prevent the joint splicer from infiltrating into the display panel area and affecting the performance of the component. In addition, the barrier structure can block and accommodate the chemical liquid used to thin the mother panel to prevent the interior of the mother panel from being damaged by the chemical liquid, thereby improving the production yield of the display panel. Moreover, the fabrication of the barrier structure is compatible with existing display panel processes and does not result in a substantial increase in production costs.

雖然本發明已以較佳實施例揭露如上,然其並非用以限定本發明,任何熟習此技藝者,在不脫離本發明之精神和範圍內,當可作些許之更動與潤飾,因此本發明之保護範圍當視後附之申請專利範圍所界定者為準。 While the present invention has been described in its preferred embodiments, the present invention is not intended to limit the invention, and the present invention may be modified and modified without departing from the spirit and scope of the invention. The scope of protection is subject to the definition of the scope of the patent application.

100、200、300‧‧‧母面板 100, 200, 300‧‧ ‧ mother panel

102、212‧‧‧顯示面板區域 102, 212‧‧‧ display panel area

104、214‧‧‧周邊區 104, 214‧‧‧ surrounding area

106、206‧‧‧端子部 106, 206‧‧‧ Terminals

110、210‧‧‧第一母基板 110, 210‧‧‧ first mother substrate

120、220‧‧‧第二母基板 120, 220‧‧‧ second mother substrate

130‧‧‧擬框膠 130‧‧‧

140、240‧‧‧接合框膠 140, 240‧‧‧ joint frame glue

150、250‧‧‧密封框膠 150, 250‧‧‧ Sealing frame glue

160、260‧‧‧對位標記 160, 260‧‧‧ alignment mark

170、270‧‧‧間隙 170, 270‧ ‧ gap

230、232、234、236‧‧‧第一阻擋結構 230, 232, 234, 236‧‧‧ first barrier structure

230a‧‧‧第一主體部 230a‧‧‧First Main Body

230b‧‧‧第一導流部 230b‧‧‧First Drainage Department

230c‧‧‧輔助導流部 230c‧‧Auxiliary diversion

240‧‧‧接合框膠 240‧‧‧Joint frame glue

280‧‧‧第二阻擋結構 280‧‧‧second barrier structure

280a‧‧‧第二主體部 280a‧‧‧Second Main Body

280b‧‧‧第二導流部 280b‧‧‧Second diversion

CS‧‧‧化學液 CS‧‧‧Chemical fluid

DP‧‧‧顯示面板 DP‧‧‧ display panel

S1‧‧‧第一容納空間 S1‧‧‧First accommodation space

S2‧‧‧第二容納空間 S2‧‧‧Second accommodation space

θ 1‧‧‧第一角度 θ 1‧‧‧ first angle

θ 2‧‧‧第二角度 θ 2‧‧‧second angle

S500~S508‧‧‧步驟 S500~S508‧‧‧Steps

圖1A是習知的母面板的立體示意圖。 1A is a schematic perspective view of a conventional mother panel.

圖1B是圖1A之母面板的俯視示意圖。 FIG. 1B is a top plan view of the mother panel of FIG. 1A.

圖1C是圖1B之A區域的放大示意圖。 Fig. 1C is an enlarged schematic view of a region A of Fig. 1B.

圖1D是圖1B之B區域的放大示意圖。 Fig. 1D is an enlarged schematic view of a region B of Fig. 1B.

圖2A是本發明較佳實施例的一種母面板的立體示意圖。 2A is a perspective view of a mother panel in accordance with a preferred embodiment of the present invention.

圖2B為圖2A的母面板的俯視示意圖。 2B is a top plan view of the mother panel of FIG. 2A.

圖2C是圖2B之C區域的放大示意圖。 2C is an enlarged schematic view of a region C of FIG. 2B.

圖2D是圖2B之D區域的放大示意圖。 2D is an enlarged schematic view of a region D of FIG. 2B.

圖3A~圖3C為本發明較佳實施例的數種第一阻擋 結構的示意圖。 3A-3C are several first blocks of a preferred embodiment of the present invention Schematic diagram of the structure.

圖4為本發明較佳實施例的另一種母面板的俯視示意圖。 4 is a top plan view of another mother panel in accordance with a preferred embodiment of the present invention.

圖5是本發明較佳實施例的一種顯示面板的製作方法流程圖。 FIG. 5 is a flow chart of a method for fabricating a display panel according to a preferred embodiment of the present invention.

200‧‧‧母面板 200‧‧‧ mother panel

210‧‧‧第一母基板 210‧‧‧First mother substrate

212‧‧‧顯示面板區域 212‧‧‧Display panel area

214‧‧‧周邊區 214‧‧‧The surrounding area

230‧‧‧第一阻擋結構 230‧‧‧First barrier structure

230a‧‧‧第一主體部 230a‧‧‧First Main Body

230b‧‧‧第一導流部 230b‧‧‧First Drainage Department

240‧‧‧接合框膠 240‧‧‧Joint frame glue

250‧‧‧密封框膠 250‧‧‧ Sealing frame glue

260‧‧‧對位標記 260‧‧‧ alignment mark

DP‧‧‧顯示面板 DP‧‧‧ display panel

S1‧‧‧第一容納空間 S1‧‧‧First accommodation space

θ 1‧‧‧第一角度 θ 1‧‧‧ first angle

Claims (22)

一種母面板,適於被分割成多個顯示面板,該母面板包括:一第一母基板,具有多個顯示面板區域、以及圍繞該些顯示面板區域的一周邊區;一第二母基板,對應配置於該第一母基板上方;至少一第一阻擋結構,對應該周邊區而配置於該第一母基板或該第二母基板上,該第一阻擋結構包括:一第一主體部;以及至少二第一導流部,連接於該第一主體部的兩側,其中該第一主體部與該些第一導流部形成一第一容納空間,該第一容納空間朝向該第一母基板或該第二母基板外側。 A mother panel is adapted to be divided into a plurality of display panels, the mother panel comprising: a first mother substrate having a plurality of display panel regions and a peripheral region surrounding the display panel regions; a second mother substrate corresponding to Disposed on the first mother substrate; at least one first blocking structure is disposed on the first mother substrate or the second mother substrate corresponding to the peripheral region, the first blocking structure comprising: a first body portion; The at least two first flow guiding portions are connected to the two sides of the first main body portion, wherein the first main body portion and the first flow guiding portions form a first receiving space, the first receiving space facing the first female portion The substrate or the outside of the second mother substrate. 如申請專利範圍第1項所述之母面板,其中該第一主體部與每一該些第一導流部之間夾有一第一角度,且該第一角度為大於等於90度且小於180度。 The mother panel of claim 1, wherein the first body portion and each of the first flow guiding portions have a first angle, and the first angle is greater than or equal to 90 degrees and less than 180 degrees. degree. 如申請專利範圍第2項所述之母面板,更包括至少二輔助導流部,分別連接於每一該些第一導流部,每一該些輔助導流部與每一該些第一導流部之間夾有一第二角度,且該第二角度為大於180度且小於360度。 The mother panel of claim 2, further comprising at least two auxiliary guiding portions respectively connected to each of the first guiding portions, each of the auxiliary guiding portions and each of the first guiding portions A second angle is sandwiched between the flow guiding portions, and the second angle is greater than 180 degrees and less than 360 degrees. 如申請專利範圍第1項所述之母面板,其中該第一主體部的形狀包括V字形、半圓形或是一字形。 The mother panel of claim 1, wherein the shape of the first body portion comprises a V shape, a semicircle shape or a shape. 如申請專利範圍第1項所述之母面板,更包括至少一第二阻擋結構,與該第一阻擋結構為交錯配置,其中該第二阻擋結構包括: 一第二主體部;以及至少二第二導流部,連接於該第二主體部的兩側,其中該第二主體部與該些第二導流部形成一第二容納空間。 The mother panel of claim 1, further comprising at least one second blocking structure in a staggered configuration with the first blocking structure, wherein the second blocking structure comprises: a second body portion; and at least two second flow guiding portions are connected to the two sides of the second body portion, wherein the second body portion and the second flow guiding portions form a second receiving space. 如申請專利範圍第1項所述之母面板,更包括一接合框膠,對應該周邊區而設置於該第一母基板或該第二母基板上,且該第一容納空間適於容置該接合框膠。 The mother panel of claim 1, further comprising a joint frame glue disposed on the first mother substrate or the second mother substrate corresponding to the peripheral region, and the first receiving space is adapted to be received The joint frame glue. 如申請專利範圍第1項所述之母面板,更包括至少一對位標記,對應該周邊區而配置於該第一母基板或該第二母基板上,該對位標記位於該第一容納空間內。 The mother panel of claim 1, further comprising at least one pair of bit marks disposed on the first mother substrate or the second mother substrate corresponding to the peripheral area, the alignment mark being located in the first receiving Within the space. 如申請專利範圍第1項所述之母面板,更包括多個密封框膠,設置於該第一母基板或該第二母基板上,每一該些密封框膠位於每一該些顯示面板區域的周圍。 The mother panel of claim 1, further comprising a plurality of sealing frame glues disposed on the first mother substrate or the second mother substrate, each of the sealing frame glues being located on each of the display panels Around the area. 如申請專利範圍第8項所述之母面板,其中每一該些密封框膠具有一液晶注入口。 The mother panel of claim 8, wherein each of the seal seals has a liquid crystal injection port. 如申請專利範圍第1項所述之母面板,其中該第一阻擋結構的材質包括熱固化膠或紫外光固化膠。 The mother panel of claim 1, wherein the material of the first barrier structure comprises a thermosetting adhesive or an ultraviolet curing adhesive. 一種顯示面板的製作方法,包括:提供一第一母基板,該第一母基板具有多個顯示面板區域、以及圍繞該些顯示面板區域的一周邊區;提供一第二母基板,對應配置於該第一母基板上方;對應該周邊區於該第一母基板或該第二母基板上形成至少一第一阻擋結構,且該第一阻擋結構包括一第一主體部以及至少二第一導流部,連接於該第一主體部的兩側,其中該第一主體部與該些第一導流部形成一第一 容納空間,該第一容納空間朝向該第一母基板或該第二母基板外側;接合該第一母基板與該第二母基板,以形成一母面板;以及分割該母面板,以形成多個顯示面板。 A method for manufacturing a display panel, comprising: providing a first mother substrate, the first mother substrate having a plurality of display panel regions, and a peripheral region surrounding the display panel regions; providing a second mother substrate corresponding to the Forming at least a first blocking structure on the first mother substrate or the second mother substrate corresponding to the peripheral region, and the first blocking structure includes a first body portion and at least two first channels Connected to the two sides of the first body portion, wherein the first body portion and the first flow guiding portions form a first The first receiving space faces the outer side of the first mother substrate or the second mother substrate; the first mother substrate and the second mother substrate are joined to form a mother panel; and the mother panel is divided to form a plurality of Display panels. 如申請專利範圍第11項所述之顯示面板的製作方法,其中該第一主體部與每一該些第一導流部之間夾有一第一角度,且該第一角度為大於等於90度且小於180度。 The method of manufacturing the display panel of claim 11, wherein the first body portion and each of the first flow guiding portions have a first angle, and the first angle is greater than or equal to 90 degrees. And less than 180 degrees. 如申請專利範圍第12項所述之顯示面板的製作方法,更包括形成至少二輔助導流部,分別連接於每一該些第一導流部,每一該些輔助導流部與每一該些第一導流部之間夾有一第二角度,且該第二角度為大於等於180度且小於360度。 The method for manufacturing a display panel according to claim 12, further comprising forming at least two auxiliary flow guiding portions respectively connected to each of the first flow guiding portions, each of the auxiliary guiding portions and each A second angle is sandwiched between the first flow guiding portions, and the second angle is greater than or equal to 180 degrees and less than 360 degrees. 如申請專利範圍第11項所述之顯示面板的製作方法,其中該第一主體部的形狀包括V字形、半圓形或是一字形。 The method of manufacturing the display panel according to claim 11, wherein the shape of the first body portion comprises a V shape, a semicircle shape or a shape. 如申請專利範圍第11項所述之顯示面板的製作方法,更包括形成至少一第二阻擋結構,與該第一阻擋結構為交錯配置,其中該第二阻擋結構包括:一第二主體部;以及至少二第二導流部,連接於該第二主體部的兩側,其中該第二主體部與該些第二導流部形成一第二容納空間。 The method of manufacturing the display panel of claim 11, further comprising forming at least one second blocking structure in a staggered configuration with the first blocking structure, wherein the second blocking structure comprises: a second body portion; And at least two second flow guiding portions are connected to the two sides of the second body portion, wherein the second body portion and the second flow guiding portions form a second receiving space. 如申請專利範圍第11項所述之顯示面板的製作方法,其中,接合該第一母基板與該第二母基板的方法 包括:對應該周邊區於該第一母基板或該第二母基板上形成一接合框膠,以接合該第一母基板與該第二母基板,其中,該第一容納空間內適於容置該接合框膠。 The method for fabricating a display panel according to claim 11, wherein the method of bonding the first mother substrate and the second mother substrate The method includes: forming a bonding frame glue on the first mother substrate or the second mother substrate corresponding to the peripheral region to bond the first mother substrate and the second mother substrate, wherein the first receiving space is suitable for receiving Place the joint frame glue. 如申請專利範圍第11項所述之顯示面板的製作方法,其中,於接合該第一母基板與該第二母基板之前,更包括對應該周邊區而於該第一母基板或該第二母基板上形成至少一對位標記,且該對位標記位於該第一容納空間內。 The method for manufacturing a display panel according to claim 11, wherein before the bonding the first mother substrate and the second mother substrate, the corresponding peripheral region is included in the first mother substrate or the second At least one pair of bit marks is formed on the mother substrate, and the alignment mark is located in the first receiving space. 如申請專利範圍第11項所述之顯示面板的製作方法,更包括於該第一母基板或該第二母基板上形成多個密封框膠,每一該些密封框膠位於每一該些顯示面板區域的周圍。 The method of manufacturing the display panel of claim 11, further comprising forming a plurality of sealing frame glues on the first mother substrate or the second mother substrate, each of the sealing frame glues being located in each of the plurality of sealing frames. Shows the area around the panel area. 如申請專利範圍第18項所述之顯示面板的製作方法,其中每一該些密封框膠具有一液晶注入口。 The method for manufacturing a display panel according to claim 18, wherein each of the seal seals has a liquid crystal injection port. 如申請專利範圍第11項所述之顯示面板的製作方法,在形成該母面板之後且於分割該母面板之前,更包括將該母面板浸於一化學液中而進行一薄化製程,該化學液適於被該第一阻擋結構阻擋,且滲入該母面板中的該化學液適於容置於該第一容納空間中。 The method for manufacturing a display panel according to claim 11, after forming the mother panel and before dividing the mother panel, further comprising immersing the mother panel in a chemical liquid to perform a thinning process. The chemical liquid is adapted to be blocked by the first barrier structure, and the chemical liquid penetrating into the mother panel is adapted to be received in the first receiving space. 如申請專利範圍第11項所述之顯示面板的製作方法,更包括於每一該些顯示面板中注入一液晶層。 The method for fabricating a display panel according to claim 11, further comprising injecting a liquid crystal layer into each of the display panels. 如申請專利範圍第11項所述之顯示面板的製作方法,其中該第一阻擋結構的材質包括熱固化膠或紫外光固化膠。 The manufacturing method of the display panel of claim 11, wherein the material of the first barrier structure comprises a thermosetting adhesive or an ultraviolet curing adhesive.
TW98134189A 2009-10-08 2009-10-08 Mother panel and fabricating method of display panel TWI408448B (en)