TW201918370A - Cationic aqueous solution used in the manufacture method to prevent the packaging material is contaminated ink - Google Patents

Cationic aqueous solution used in the manufacture method to prevent the packaging material is contaminated ink Download PDF

Info

Publication number
TW201918370A
TW201918370A TW106138029A TW106138029A TW201918370A TW 201918370 A TW201918370 A TW 201918370A TW 106138029 A TW106138029 A TW 106138029A TW 106138029 A TW106138029 A TW 106138029A TW 201918370 A TW201918370 A TW 201918370A
Authority
TW
Taiwan
Prior art keywords
ink
layer
substrate
aqueous solution
forming
Prior art date
Application number
TW106138029A
Other languages
Chinese (zh)
Inventor
林紫綺
Original Assignee
林紫綺
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 林紫綺 filed Critical 林紫綺
Priority to TW106138029A priority Critical patent/TW201918370A/en
Publication of TW201918370A publication Critical patent/TW201918370A/en

Abstract

The present invention discloses a cationic aqueous solution used in the manufacture method to prevent the packaging material is contaminated ink, it includes the following steps: providing a material base, forming an ink layer, forming an primer layer, and forming a film layer. With the implementation of the present invention, not only it can be manufactured without ink contamination of the packaging materials, but also to achieve effective insulation ink layer. Thus contamination is perfectly stopped and the safety of drinking or eating is completely ensured.

Description

陽離子水性溶液製造防止墨料汙染包裝材料之方法Method for manufacturing cationic aqueous solution to prevent ink from contaminating packaging material

本發明為一種陽離子水性溶液製造防止墨料汙染包裝材料之方法,特別是一種應用於食品包裝容器,其使用陽離子水性溶液作為介面層之陽離子水性溶液製造防止墨料汙染包裝材料之方法。The invention relates to a method for manufacturing a cationic aqueous solution for preventing ink contamination of a packaging material, in particular to a food packaging container, which uses a cationic aqueous solution as a cationic aqueous solution of an interface layer to manufacture a method for preventing ink from contaminating a packaging material.

一般市面上現有的容器,尤其是印製有墨料的紙杯結構,因要求成本之控管,不論是使用黑白或彩色墨料,其使用的包裝材料之品質參差不齊,很難確保其使用之安全無虞或不會產生汙染。此外,目前使用量甚大的紙杯,其印製的墨料大多不經覆蓋,經常直接暴露而接觸使用者,甚至汙染到所盛裝的內容物,非常容易造成使用者飲用或食用的安全疑慮。Generally, the existing containers on the market, especially the paper cup structure printed with ink, are required to control the cost. Whether using black and white or colored ink, the quality of the packaging materials used is uneven, and it is difficult to ensure the use thereof. Safe or flawless. In addition, paper cups that are currently used in large quantities are mostly uncovered, often exposed directly to the user, and even contaminated with the contents of the contents, which are very likely to cause safety concerns for the user to drink or eat.

再者,目前對於使用墨料的法律規範尚未臻齊全,且時下使用的墨料又大多仍含有或多或少的有毒物質,使用者在使用容器或是紙杯時所受到的毒物汙染之風險,實際上大大超出一般人的想像。Furthermore, the current legal regulations for the use of inks are not yet complete, and most of the inks currently used still contain more or less toxic substances, and the risk of toxic contamination of users when using containers or paper cups. In fact, it is much larger than the imagination of the average person.

另一方面,包裝材料、容器或紙杯的運送或儲存,為了減少其占用體積,通常又皆以互套或堆疊方式為之,如此包裝材料、容器或紙杯所印製的高結合性墨料層之墨料,又會以接觸方式,汙染到互套或堆疊的其他包裝材料、容器或紙杯。On the other hand, the transportation or storage of packaging materials, containers or paper cups, in order to reduce their occupation volume, is usually in the form of mutual or stacked, so that the high-combination ink layer printed on the packaging material, container or paper cup The ink will be contaminated by other means of packaging, containers or paper cups in a mutual contact or stack.

有鑑於此,必須儘速發明設計出一種防止墨料汙染包裝材料之方法,不但可以保留包裝材料的方便與易於量產的特性,又可以有效隔離墨料,避免墨料對使用者或內容物造成汙染,進而能成為包裝材料、容器、紙杯及其廣大應用產業,一個重要的創新與進步。In view of this, it is necessary to invent the design of a method for preventing the ink from contaminating the packaging material as soon as possible, not only to preserve the convenience and mass production characteristics of the packaging material, but also to effectively isolate the ink material and avoid the ink material to the user or the contents. It causes pollution and can become an important innovation and progress in packaging materials, containers, paper cups and their application industries.

本發明係要解決如何使墨料不會對容器中的內容物或與墨料接觸的其他容器造成汙染,以保護使用者之飲用或食用的衛生及安全之功效。The present invention is directed to how to prevent the ink from contaminating the contents of the container or other containers in contact with the ink to protect the user's health and safety from drinking or eating.

本發明提供一種陽離子水性溶液製造防止墨料汙染包裝材料之方法,其包括下列步驟:提供基材,其係提供一基材,做為防墨料汙染包裝材料的基底;形成墨料層,其係將一墨料層形成於基材之至少一表面;形成介面層,其係將一陽離子水性溶液之介面層(Primer Layer)形成於墨料層上;以及形成淋膜層,其係將一淋膜層形成於基材或介面層上。The invention provides a method for manufacturing a cationic aqueous solution for preventing ink from contaminating a packaging material, comprising the steps of: providing a substrate, which is provided as a substrate for preventing ink from contaminating the packaging material; forming an ink layer, Forming an ink layer on at least one surface of the substrate; forming an interface layer for forming a cationic layer of a cationic aqueous solution on the ink layer; and forming a coating layer, which is a The coating layer is formed on the substrate or interface layer.

藉由本發明的實施,至少可以達到下列進步功效: 一、 製造成本增加甚少,且大量生產容易。 二、 隔離墨料,避免產生包裝材料或容器之相互汙染。 三、 避免墨料汙染使用者或內容物,確保包裝材料或容器之使用衛生及安全。With the implementation of the present invention, at least the following advancements can be achieved: 1. Manufacturing costs are increased little, and mass production is easy. Second, the ink is isolated to avoid mutual contamination of the packaging materials or containers. 3. Avoid ink contamination of users or contents, and ensure the use of packaging materials or containers is hygienic and safe.

為了使任何熟習相關技藝者了解本發明之技術內容並據以實施,且根據本說明書所揭露之內容、申請專利範圍及圖式,任何熟習相關技藝者可輕易地理解本發明相關之目的及優點,因此將在實施方式中詳細敘述本發明之詳細特徵以及優點。In order to make those skilled in the art understand the technical content of the present invention and implement it, and according to the disclosure, the patent scope and the drawings, the related objects and advantages of the present invention can be easily understood by those skilled in the art. The detailed features and advantages of the present invention will be described in detail in the embodiments.

請參考如第1圖所示,本實施例為一種陽離子水性溶液製造防止墨料汙染包裝材料之方法100,其包括:提供基材(步驟S10);形成墨料層(步驟S20);形成介面層 (步驟S30);以及形成淋膜層(步驟S40)。其主要藉由乙烯亞胺水性聚合物含有胺基的聚合物,又其為高陽離子性為極性基團,因此能與聚悕鯨(polyolefin)類材料產生鍵結,藉此以產生良好介面處理的效果。Please refer to FIG. 1 , which is a method 100 for preparing a cationic aqueous solution to prevent ink contamination of a packaging material, comprising: providing a substrate (step S10); forming an ink layer (step S20); forming an interface a layer (step S30); and forming a lamination layer (step S40). It mainly uses an amine-based polymer of an ethyleneimine aqueous polymer, which is a highly cationic group, and thus can bond with a poly-type material, thereby producing a good interface treatment. Effect.

如第1圖及第2圖所示,提供基材(步驟S10),其係準備一基底材質,做為製造防墨料汙染包裝材料的基底,使用之基材10可以選擇為一紙板或一高分子板材。As shown in FIGS. 1 and 2, a substrate is provided (step S10), which is a substrate material prepared as a substrate for manufacturing an ink-repellent packaging material, and the substrate 10 used may be selected as a cardboard or a substrate. Polymer sheet.

當所述之基材10,其材質選擇為紙質基材10,此時,由陽離子水性溶液製造防止墨料汙染包裝材料之方法S100製造之防墨料汙染包裝材料所形成的容器,可以是一紙杯、一紙碗或一紙盒。When the substrate 10 is made of a paper substrate 10, the container formed by the ink-repellent packaging material manufactured by the method S100 for preventing the ink from contaminating the packaging material from the cationic aqueous solution may be a container. Paper cup, a paper bowl or a paper box.

另一方面,當基材10之材質選擇為高分子材質,則所使用之高分子材質,可選擇較易取得且成本控制較佳的塑膠或矽膠材質。On the other hand, when the material of the substrate 10 is selected as a polymer material, the polymer material used can be selected from a plastic or silicone material which is relatively easy to obtain and has a cost control.

如第1圖及第3圖所示,形成墨料層(步驟S20),其係於基材10之至少一表面形成一墨料層20,且墨料層20可以是形成於整個基材10的表面,或僅形成於基材10表面的一部份。As shown in FIGS. 1 and 3, an ink layer is formed (step S20), which is formed on at least one surface of the substrate 10 to form an ink layer 20, and the ink layer 20 may be formed on the entire substrate 10. The surface, or only a portion of the surface of the substrate 10 is formed.

如第6A圖至第8B圖所示,墨料層20係可以形成於基材10之至少一表面。而墨料層20可以為水性的墨料層20、油性的墨料層20、固體的墨料層20,或者是綜合性的墨料層20。As shown in FIGS. 6A to 8B, the ink layer 20 may be formed on at least one surface of the substrate 10. The ink layer 20 may be an aqueous ink layer 20, an oily ink layer 20, a solid ink layer 20, or a comprehensive ink layer 20.

如第1圖及第4A圖所示,形成介面層(步驟S30),其係將一陽離子水性溶液之介面層30(Primer Layer)形成於墨料層20上,所述介面層30係可以為總固含量5%~50%之乙烯亞胺水性聚合物所形成,又乙烯亞胺水性聚合物中可以含有1%~25%之含有胺基的聚合物。As shown in FIG. 1 and FIG. 4A, an interface layer is formed (step S30), in which an interface layer 30 of a cationic aqueous solution is formed on the ink layer 20, and the interface layer 30 can be The ethyleneimine aqueous polymer is formed by a total solid content of 5% to 50%, and the ethyleneimine aqueous polymer may contain 1% to 25% of an amine group-containing polymer.

接著,請參考如第1圖及第4B圖所示,形成淋膜層(步驟S40),其係將一淋膜層40附著於基材10或介面層30上。Next, referring to FIGS. 1 and 4B, a coating layer is formed (step S40), and a coating layer 40 is attached to the substrate 10 or the interface layer 30.

於基材10之表面形成有墨料層20時,因為墨料層20有時不易與淋膜層40黏附,因此,在覆蓋形成淋膜層40之前,先於墨料層20上形成一層與淋膜層40及墨料層20都容易黏附的介面層30,可以確保淋膜層40之穩固附著。When the ink layer 20 is formed on the surface of the substrate 10, since the ink layer 20 sometimes does not easily adhere to the coating layer 40, a layer is formed on the ink layer 20 before covering the coating layer 40. The interface layer 30, which is easy to adhere to both the coating layer 40 and the ink layer 20, ensures the stable adhesion of the coating layer 40.

如第4A圖、第4B圖、以及第6A圖至第8B圖所示,淋膜層40附著於覆蓋墨料層20的介面層30上,可以有效遮蔽墨料層20,避免了墨料層20直接與使用者或其他物體產生接觸,可以避免墨料層20所使用的墨料汙染使用者或其他物體而產生不良影響。As shown in FIG. 4A, FIG. 4B, and FIGS. 6A to 8B, the coating layer 40 is attached to the interface layer 30 covering the ink layer 20, which can effectively shield the ink layer 20 and avoid the ink layer. 20 Direct contact with a user or other object can prevent the ink used in the ink layer 20 from contaminating the user or other objects and adversely affecting them.

至於形成淋膜層(步驟S40)所使用之淋膜層40,可以是由高分子材料所形成,而使用之高分子材料,則係可以為聚丙烯(PP)、聚氯乙烯(PVC)、聚乙烯(PE)、低密度聚乙烯 (LDPE)、高密度聚乙烯(HDPE)、聚苯乙烯(PS)、丙烯腈-丁二烯-苯乙烯共聚合物(ABS)、聚醯胺樹脂(Nylon)、聚酯樹脂(PET)或乙烯-醋酸乙烯共聚物(EVA樹脂)。The coating layer 40 used to form the coating layer (step S40) may be formed of a polymer material, and the polymer material used may be polypropylene (PP) or polyvinyl chloride (PVC). Polyethylene (PE), low density polyethylene (LDPE), high density polyethylene (HDPE), polystyrene (PS), acrylonitrile-butadiene-styrene copolymer (ABS), polyamine resin ( Nylon), polyester resin (PET) or ethylene-vinyl acetate copolymer (EVA resin).

再者,如第5圖至第8B圖所示,製造方法S200,係為陽離子水性溶液製造防止墨料汙染包裝材料之方法S100進一步包括一形成容器(步驟S50)之步驟,其係以防墨料汙染包裝材料形成一防墨料汙染容器100、防墨料汙染容器200或防墨料汙染容器300,而其中防墨料汙染容器100、防墨料汙染容器200或防墨料汙染容器300可以為杯體、碗體或盒體。Furthermore, as shown in FIGS. 5 to 8B, the manufacturing method S200 is a method for producing a cationic aqueous solution to prevent ink contamination of the packaging material. The method S100 further includes a step of forming a container (step S50), which is protected against ink. The pollution-contaminated packaging material forms an ink-repellent-contaminated container 100, an ink-repellent-contaminated container 200, or an ink-repellent-contaminated container 300, wherein the ink-repellent-contaminated container 100, the ink-repellent-contaminated container 200, or the ink-repellent-contaminated container 300 can be It is a cup, bowl or box.

如第6A圖及第6B圖所示之防墨料汙染容器100實施例,係僅基材10之外表面形成有墨料層20。如第7A圖及第7B圖所示之防墨料汙染容器200實施例,係基材10之外表面及內表面皆形成有墨料層20。而如第8A圖及第8B圖所示之防墨料汙染容器300實施例,則係基材10之外表面、內表面及內底面皆形成有墨料層20。As an example of the ink repellent container 100 shown in FIGS. 6A and 6B, only the outer layer 10 of the substrate 10 is formed with the ink layer 20. As an embodiment of the ink repellent container 200 shown in FIGS. 7A and 7B, the ink layer 20 is formed on both the outer surface and the inner surface of the substrate 10. Further, as in the embodiment of the ink repellent container 300 shown in FIGS. 8A and 8B, the ink layer 20 is formed on the outer surface, the inner surface, and the inner bottom surface of the substrate 10.

如第6A圖至第8B圖所示,不論是直接於基材10表面或是介面層30之上,防墨料汙染容器100、防墨料汙染容器200或防墨料汙染容器300內部或外部之表面層皆為淋膜層40。As shown in FIGS. 6A to 8B, the ink repellent contamination container 100, the ink repellent contamination container 200, or the ink repellent contamination container 300 may be internal or external, either directly on the surface of the substrate 10 or above the interface layer 30. The surface layers are all the coating layer 40.

綜上所述,具有淋膜層40的防墨料汙染容器100、防墨料汙染容器200或防墨料汙染容器300,皆使用介面層30使墨料層20之上可以確實附著淋膜層40,而能使淋膜層40同時能附著於基材10及墨料層20之上,以淋膜層40有效隔離墨料層20中之墨料,達到防止墨料汙染之功效,而能確保使用衛生與避免接觸墨料中有毒物質之可能。In summary, the ink repellent contaminated container 100 having the coating layer 40, the ink repellent contaminating container 200 or the ink repellent contaminating container 300 all use the interfacial layer 30 to allow the laminating layer to adhere to the ink layer 20 40, the coating layer 40 can be attached to the substrate 10 and the ink layer 20 at the same time, and the coating layer 40 effectively isolates the ink in the ink layer 20 to achieve the effect of preventing ink contamination. Ensure hygiene and avoid the possibility of exposure to toxic substances in the ink.

惟上述各實施例係用以說明本發明之特點,其目的在使熟習該技術者能瞭解本發明之內容並據以實施,而非限定本發明之專利範圍,故凡其他未脫離本發明所揭示之精神而完成之等效修飾或修改,仍應包含在以下所述之申請專利範圍中。The embodiments are described to illustrate the features of the present invention, and the purpose of the present invention is to enable those skilled in the art to understand the present invention and to implement the present invention without limiting the scope of the present invention. Equivalent modifications or modifications made by the spirit of the disclosure should still be included in the scope of the claims described below.

S100‧‧‧陽離子水性溶液製造防止墨料汙染包裝材料之方法S100‧‧‧Method for manufacturing cationic aqueous solution to prevent ink from contaminating packaging materials

S10‧‧‧提供基材S10‧‧‧ providing substrate

S20‧‧‧形成墨料層S20‧‧‧Ink layer

S30‧‧‧形成介面層S30‧‧‧ forming interface layer

S40‧‧‧形成淋膜層S40‧‧‧ forming a laminar layer

S200‧‧‧製造方法S200‧‧‧Manufacturing method

S50‧‧‧形成容器S50‧‧‧ forming a container

10‧‧‧基材10‧‧‧Substrate

20‧‧‧墨料層20‧‧‧Ink layer

30‧‧‧介面層30‧‧‧Interface

40‧‧‧淋膜層40‧‧‧Layer layer

100‧‧‧防墨料汙染容器100‧‧‧Ink-contaminated container

200‧‧‧防墨料汙染容器200‧‧‧Anti-ink pollution container

300‧‧‧防墨料汙染容器300‧‧‧Ink-contaminated container

[第1圖]為本發明實施例之一種陽離子水性溶液製造防止墨料汙染包裝材料之方法之流程步驟圖; [第2圖]為本發明實施例之一種基材的示意圖; [第3圖]為本發明實施例之一種基材上形成墨料層之示意圖; [第4A圖]為本發明實施例之一種基材上形成墨料層及淋膜層之示意圖; [第4B圖]為本發明實施例之一種形成淋膜層之示意圖; [第5圖]為本發明方法實施例進一步包含一形成容器之步驟之流程步驟圖; [第6A圖]為本發明方法實施例所製造之容器的立體示意圖; [第6B圖]為第6A圖實施例之立體縱剖視示意圖; [第7A圖]為本發明方法實施例所製造之另一種容器的縱剖視示意圖; [第7B圖]為第7A圖實施例之局部放大圖; [第8A圖]為本發明方法實施例所製造之又一種容器的剖視示意圖;以及 [第8B圖]為第8A圖實施例之局部放大圖。[FIG. 1] FIG. 1 is a flow chart showing a method for manufacturing a cationic aqueous solution to prevent ink from contaminating a packaging material; FIG. 2 is a schematic view showing a substrate according to an embodiment of the present invention; A schematic view of forming an ink layer on a substrate according to an embodiment of the present invention; [FIG. 4A] is a schematic view showing formation of an ink layer and a coating layer on a substrate according to an embodiment of the present invention; [FIG. 4B] A schematic diagram of forming a lamellar layer according to an embodiment of the present invention; [Fig. 5] is a flow chart showing a step of forming a container according to an embodiment of the method of the present invention; [Fig. 6A] [FIG. 6B] is a schematic longitudinal cross-sectional view of the embodiment of FIG. 6A; [FIG. 7A] is a longitudinal sectional view of another container manufactured by the method embodiment of the present invention; [FIG. 7B] Figure 7 is a partially enlarged view of the embodiment of Figure 7A; [Fig. 8A] is a schematic cross-sectional view of still another container manufactured by the method embodiment of the present invention; and [Fig. 8B] is a partial enlarged view of the embodiment of Figure 8A .

Claims (10)

一種陽離子水性溶液製造防止墨料汙染包裝材料之方法,其包括下列步驟: 提供基材,其係提供一基材,做為該防墨料汙染包裝材料的基底; 形成墨料層,其係將一墨料層形成於該基材之至少一表面; 形成介面層,其係將一陽離子水性溶液之介面層形成於該墨料層上;以及 形成淋膜層,其係將一淋膜層形成於該基材或該介面層上。A method for producing a cationic aqueous solution for preventing ink from contaminating a packaging material, comprising the steps of: providing a substrate, which is provided as a substrate, as a substrate for contaminating the packaging material; and forming an ink layer, which is An ink layer is formed on at least one surface of the substrate; an interface layer is formed on the ink layer by forming an interface layer of a cationic aqueous solution; and a coating layer is formed, which forms a coating layer On the substrate or the interface layer. 如申請專利範圍第1項所述之方法,其中該基材為一紙質基材或一高分子基材。The method of claim 1, wherein the substrate is a paper substrate or a polymer substrate. 如申請專利範圍第1項所述之方法,其中該墨料層係為一水性墨料層。The method of claim 1, wherein the ink layer is an aqueous ink layer. 如申請專利範圍第1項所述之方法,其中該陽離子水性溶液又含有乙烯亞胺水性聚合物。The method of claim 1, wherein the cationic aqueous solution further comprises an ethyleneimine aqueous polymer. 如申請專利範圍第1項所述之方法,其中該介面層係為總固含量5%~50%之乙烯亞胺水性聚合物所形成。The method of claim 1, wherein the interface layer is formed by an aqueous ethyleneimine polymer having a total solid content of 5% to 50%. 如申請專利範圍第5項所述之方法,其中該乙烯亞胺水性聚合物中含有1%~25%之含胺基聚合物。The method of claim 5, wherein the ethyleneimine aqueous polymer contains from 1% to 25% of the amine-containing polymer. 如申請專利範圍第1項所述之方法,其中該淋膜層為一高分子材料之淋膜層。The method of claim 1, wherein the coating layer is a coating layer of a polymer material. 如申請專利範圍第1項所述之方法,其中該淋膜層係為聚丙烯(PP)、聚氯乙烯(PVC)、聚乙烯(PE)、低密度聚乙烯(LDPE)、高密度聚乙烯(HDPE)、聚苯乙烯 (PS)、丙烯腈-丁二烯-苯乙烯共聚合物(ABS)、聚醯胺樹脂(Nylon)、聚酯樹脂(PET)或乙烯-醋酸乙烯共聚物(EVA樹脂)所形成。The method of claim 1, wherein the coating layer is polypropylene (PP), polyvinyl chloride (PVC), polyethylene (PE), low density polyethylene (LDPE), high density polyethylene. (HDPE), polystyrene (PS), acrylonitrile-butadiene-styrene copolymer (ABS), polyamide resin (Nylon), polyester resin (PET) or ethylene-vinyl acetate copolymer (EVA) Resin) formed. 如申請專利範圍第1項所述之方法,其進一步包括一形成容器之步驟,以形成一防墨料汙染容器。The method of claim 1, further comprising the step of forming a container to form an ink repellent contaminated container. 如申請專利範圍第9項所述之方法,其中該防墨料汙染容器為一杯體、一碗體或一盒體。The method of claim 9, wherein the ink-repellent contaminated container is a cup, a bowl or a box.
TW106138029A 2017-11-03 2017-11-03 Cationic aqueous solution used in the manufacture method to prevent the packaging material is contaminated ink TW201918370A (en)