TW200940318A - Method for making plastic shrinkage film with environment-friendly materials - Google Patents

Method for making plastic shrinkage film with environment-friendly materials Download PDF

Info

Publication number
TW200940318A
TW200940318A TW97112750A TW97112750A TW200940318A TW 200940318 A TW200940318 A TW 200940318A TW 97112750 A TW97112750 A TW 97112750A TW 97112750 A TW97112750 A TW 97112750A TW 200940318 A TW200940318 A TW 200940318A
Authority
TW
Taiwan
Prior art keywords
film
thickness
folded
plastic film
tubular
Prior art date
Application number
TW97112750A
Other languages
English (en)
Chinese (zh)
Other versions
TWI331559B (enExample
Inventor
Qi-zan YANG
Original Assignee
Qi-zan YANG
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Qi-zan YANG filed Critical Qi-zan YANG
Priority to TW97112750A priority Critical patent/TW200940318A/zh
Publication of TW200940318A publication Critical patent/TW200940318A/zh
Application granted granted Critical
Publication of TWI331559B publication Critical patent/TWI331559B/zh

Links

Landscapes

  • Shaping By String And By Release Of Stress In Plastics And The Like (AREA)
  • Shaping Of Tube Ends By Bending Or Straightening (AREA)
TW97112750A 2008-03-25 2008-04-09 Method for making plastic shrinkage film with environment-friendly materials TW200940318A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
TW97112750A TW200940318A (en) 2008-03-25 2008-04-09 Method for making plastic shrinkage film with environment-friendly materials

Applications Claiming Priority (2)

Application Number Priority Date Filing Date Title
TW97110453 2008-03-25
TW97112750A TW200940318A (en) 2008-03-25 2008-04-09 Method for making plastic shrinkage film with environment-friendly materials

Publications (2)

Publication Number Publication Date
TW200940318A true TW200940318A (en) 2009-10-01
TWI331559B TWI331559B (enExample) 2010-10-11

Family

ID=44867961

Family Applications (1)

Application Number Title Priority Date Filing Date
TW97112750A TW200940318A (en) 2008-03-25 2008-04-09 Method for making plastic shrinkage film with environment-friendly materials

Country Status (1)

Country Link
TW (1) TW200940318A (enExample)

Also Published As

Publication number Publication date
TWI331559B (enExample) 2010-10-11

Similar Documents

Publication Publication Date Title
TWI429691B (zh) 熱可收縮性聚酯膜
JPH0222052A (ja) 熱収縮性積層フイルム及びその製造方法
NZ564572A (en) Integrated process for making inflatable article
JPS5934590B2 (ja) 改善された熱収縮発泡体スリ−ブを有する容器およびその製法
CN104401076B (zh) 一种ldpe高发泡复合hdpe膜及其制备方法
WO2009143663A1 (zh) 应用环保材料制成收缩胶膜的制法改良及其装置
US20060243842A1 (en) Pre-stretched wrapping film roll with entrapped air and method
CN102376195B (zh) 模内标签与制作方法
TW200940318A (en) Method for making plastic shrinkage film with environment-friendly materials
JPH02103122A (ja) 二軸延伸ポリアミド系フィルム及びその製造方法
KR20120014451A (ko) 발포 폼보드 제조방법 및 그 제조장치
CN206067119U (zh) 一种塑料薄膜复合生产线
CN204604943U (zh) 一种背封条生产系统
JP2019093695A (ja) パッキングフィルムのブローイング、引き伸ばし装置及び方法
WO2009135341A1 (zh) 应用环保树脂材料制成收缩塑料膜的方法
TWI328505B (enExample)
CN111590936A (zh) 一种高收缩聚烯烃热收缩薄膜的生产方法
CN111070654A (zh) 吹膜法单面哑光pvc热收缩标签膜的制备方法
JPH0564589B2 (enExample)
JP2011073364A (ja) 樹脂成形品の成形方法
CN118893885B (zh) 一种带有发泡层的面膜包装用复合膜袋及其制备方法
CN201891012U (zh) 热缝机结构
CN201978860U (zh) 用于生产电子保护膜的涂布机的放卷整平装置
JP3549222B2 (ja) 熱可塑性樹脂チューブの同時二軸延伸方法及び得られた延伸チューブの熱セット方法
CN204506044U (zh) 一种热隔离用合成纸

Legal Events

Date Code Title Description
MM4A Annulment or lapse of patent due to non-payment of fees