SU87916A1 - The method of intensification of burning and grinding and increase the strength and sulfate resistance of cements - Google Patents
The method of intensification of burning and grinding and increase the strength and sulfate resistance of cementsInfo
- Publication number
- SU87916A1 SU87916A1 SU394883A SU394883A SU87916A1 SU 87916 A1 SU87916 A1 SU 87916A1 SU 394883 A SU394883 A SU 394883A SU 394883 A SU394883 A SU 394883A SU 87916 A1 SU87916 A1 SU 87916A1
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- cements
- intensification
- burning
- grinding
- strength
- Prior art date
Description
vJcoocHiiocTb ирсд.иугаемого способа за к.ПО ч по тс в том, что в СЬ:П,Свук5 ;;месь до оожпга взод тси ilnic И.1И (Ь тн:,:с ll|))Lli.leIIiiь;e огходы . В .чтг5е добавок. (;Mc Il-uii-a. могут быт, . 1 зсчип;ь; ()(c(;)o-i;i ic. i4UJCOBr5in иыам извсстKOBofl соргкиисгк ; дь;мовых сазо; и пр. Ко.;ичс1.;тв(1 добавки iliiicji и.тп сз.тьсратиого г)тлода в игилту дсмснт1- Ои сырьевой смеси в ссрссчс тс на гипс (; б:лт1 экв1П а.тепт11о и.чиvJcoocHiiocTb of the irds.diagable method for the software of hp in terms of the fact that in СБ: П, Свук5 ;; мес до Оожпга уцпсi ilnic И.1И (L tn:,: с ll |)) . In .5d additives. (; Mc Il-uii-a. Can be life,. (1 supplement iliiicji i.tp cz.ratsygoy g) tloda igiltu dsmsnt1-Oi raw mix in the ssssssch ts on gypsum (; b: lt1 eq1p a.tep11o i.chi
nO. ОКИС.ЮВ В UCAiCllTHOAinO. OKIS.YUV UCAiCllTHOAi
i--:.in iKCiJc.i - :. in iKCiJc.
Добавка пгпса п.тн отходов г, П1;хту lUMc rfTHon (b:)bfBOi смеси иск/почаст п(.ч)бходи 1С)ст иос/юду-ощсП .юбанки гипса к к.тпгп-сору при 1К)лК)л о.Additive pgps p.tn of waste g, P1; htu lUMc rfTHon (b:) bfBOi mixture of lawsuit / will p (.ch) go 1C) cIos / yudu-ps. l about
i I j) с Д М о т П 3 о б р с т с Н и i I j) with D M about t P 3 about b r with t with N and
Сп;соб иптснсисЬпкаци: обжига и lifiAK.i.ia и ПОВЫП1СИИЯ прочпости и с.ть(1)атостопкост11 цслнмпов путем д(м;;в. к с;)рьспои vMccn гипса и.;;1 cy.ibchaTiniix промими.тсниых отходов , о т д и ч а IO : и П с тем. что, с ие.тью уве.тичспи производи;; . iiiiiiCTn ::еП. с ;и/ксн расхода Toii.iiBa, ::с:. уч1ЧП1 MaixpoiiojincTOir ст:1у;-;ту:)ь: neNieiiTnoio K.niHKeiia и :к)1ь;::1е -И5; niioMiiocni а су.1Ь(|)атоcTOilKocru ICMcHTOB. innc li.nj c тьфатныс i;ii(, отходы впод;п 15 состав сыр1)ево.: смеси до ее об/ чИ;а. в ко.тичсствс (в пересчетеCn; compilation: firing and lifiAK.i.ia and POPURSION of hardness and t. (1) athostostost11 tslnmpov by d (m ;; w. To c;) yielding vMccn of gypsum and;; 1 cy waste, about t d and ch and IO: and P with that. that, with you, you will produce;; . iiiiiiCTn :: eP. with; and / ksn consumption Toii.iiBa, :: with :. school1 MaixpoiiojincTOir article: 1y; -; that:) b: neNieiiTnoio K.niHKeiia and: to) 1b; :: 1e -I5; niioMiiocni a su.1b (|) atocTOilKocru ICMcHTOB. innc li.nj with tfatnys i; ii (, waste in the way; p 15 composition of syl1) evo: mixture to its rev / hI; a. in cons. (in terms of
г: IiinCI. К;5ГГВаЛСИТ1Ч)М М О (Ч-;у.Т Я рП () содержапию в цементном к.тинкеро по.1утор1 ь;х окис ,тов.g: IIinCI. K; 5GGVALSIT1CH) MMO (P-; y.T. I rP () content in cement cement p. Tkero 1tutor1; x oxide, comrade.