SU72040A1 - Способ получени силиката натри - Google Patents

Способ получени силиката натри

Info

Publication number
SU72040A1
SU72040A1 SU698A SU353958A SU72040A1 SU 72040 A1 SU72040 A1 SU 72040A1 SU 698 A SU698 A SU 698A SU 353958 A SU353958 A SU 353958A SU 72040 A1 SU72040 A1 SU 72040A1
Authority
SU
USSR - Soviet Union
Prior art keywords
sodium sulfate
sodium
sodium silicate
sand
coal
Prior art date
Application number
SU698A
Other languages
English (en)
Inventor
И.Г. Беспалов
Original Assignee
И.Г. Беспалов
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by И.Г. Беспалов filed Critical И.Г. Беспалов
Priority to SU698A priority Critical patent/SU72040A1/ru
Application granted granted Critical
Publication of SU72040A1 publication Critical patent/SU72040A1/ru

Description

Автором изобретени  предложен способ получени  силиката натри  в шахтной печи. Брикеты, состо щие из сульфата натри  и песка, загружают сверху. В средней части печи имеютс  фурмы дл  подвода светильного газа, благодар  чему в верхней части печи протекает процесс восстановлени  сульфата натри  до сернистого натри . Масса, состо ща  из сернистого натри  и окиси кремни , опускаетс  вниз и попадает в окислительную зону; снизу в печь подаетс  пар и светильный газ.
Образующиес  в зоне окислени  серусодержащие газы (HgS, SOa, COS и др.) поднимаютс  в зону восстановлени  и отчасти восстанавливаютс  до элементарной серы, которую улавливают с помощью электрофильтров , а невосстановленные газы поглощают в абсорбере и затем нейтрализуют.
Предмет изобретени 

Claims (3)

1.Способ получени  силиката натри  обжигом в шахтной печи брикетов, состо щих из сульфата натри , песка и угл , в две стадии: первоначально в восстановленной среде в верхней зоне нечи, с восстановлением сульфата натри  до сернистого натри , а затем в нижней зоне в окислительной среде, до полного нровара массы, отличающийс  тем, что дл  интенсификации восстановительного процесса, в верхнюю зону ввод т светильный газ, а дл  ускорени  образовани  силиката, в нижнюю зону, через противолежащие фурмы подают светильный газ одновременно с паром.
2.Видоизменение способа по п. 1, отличающеес  тем, что брикеты составл ют из смеси сульфата натри  и песка без добавки угл .
3.Прием выполнени  способов по пп. 1 и 2, отличающийс  тем, что удал емые серусодержащие газы улавливают дл  получени  серы известными способами.
SU698A 1947-04-08 1947-04-08 Способ получени силиката натри SU72040A1 (ru)