SU61325A1 - Способ ведени ваграночного процесса - Google Patents

Способ ведени ваграночного процесса

Info

Publication number
SU61325A1
SU61325A1 SU32037A SU32037A SU61325A1 SU 61325 A1 SU61325 A1 SU 61325A1 SU 32037 A SU32037 A SU 32037A SU 32037 A SU32037 A SU 32037A SU 61325 A1 SU61325 A1 SU 61325A1
Authority
SU
USSR - Soviet Union
Prior art keywords
peat
management
coke
mineral
cupola
Prior art date
Application number
SU32037A
Other languages
English (en)
Inventor
А.К. Фанбулов
Original Assignee
А.К. Фанбулов
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by А.К. Фанбулов filed Critical А.К. Фанбулов
Priority to SU32037A priority Critical patent/SU61325A1/ru
Application granted granted Critical
Publication of SU61325A1 publication Critical patent/SU61325A1/ru

Description

Попытки применить сырой торф дл  выплавки чугуна в вагранках до сих пор сводились к смешиванию сырого торфа с древесным углем или минеральным коксом.
Известно, что чугун, выплавленный на торфе, содерлшт значительно меньше серы, чем чугун, выплавленный на минеральном коксе, поэтому чем больше содержани  торфа в топливной калоше, тем выплавленный чугун доброкачественнее.
По предлагаемому способу ваграночный процесс ведут так, что плавка начинаетс  на минеральном коксе, затем - дл  последующих топливных калош - используют только сырой торф. При этом торф до подхода калош к зоне плавлени  полностью коксуетс .
В каждую калошу берут торфа примерно в 3-3,5 раза больше по весу, чем минерального кокса. Это необходимо дл  того, чтобы сохранить ту же высоту, какую топливна  калоша имеет при минеральном коксе.
Плавление чугуна происходит при температуре не ниже той, котора  примен етс  при работе на минеральном коксе. Газы, образующиес  при этом процессе, можно использовать дл  подогрева воздуха.
Применение данного способа дает не только технический, но и экономический эффект, так как дорогосто щее топливо - минеральный кокс замен етс  более дешевым сырым торфом, притом без ущерба дл  качества чугуна.
Предмет изобретени 
Способ ведени  ваграночного процесса, отличающийс  тем, что плавку начинают на минеральном коксе, а дл  всех последующих топливных калош используют только сырой торф, с тем чтобы коксование торфа завершалось до подхода калош к зоне плавлени .
SU32037A 1940-04-09 1940-04-09 Способ ведени ваграночного процесса SU61325A1 (ru)