SU58660A1 - Galvanic cell - Google Patents

Galvanic cell

Info

Publication number
SU58660A1
SU58660A1 SU2472A SU2472A SU58660A1 SU 58660 A1 SU58660 A1 SU 58660A1 SU 2472 A SU2472 A SU 2472A SU 2472 A SU2472 A SU 2472A SU 58660 A1 SU58660 A1 SU 58660A1
Authority
SU
USSR - Soviet Union
Prior art keywords
zinc
galvanic cell
acid
negative pole
positive plate
Prior art date
Application number
SU2472A
Other languages
Russian (ru)
Inventor
П.А. Молчанов
Original Assignee
П.А. Молчанов
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by П.А. Молчанов filed Critical П.А. Молчанов
Priority to SU2472A priority Critical patent/SU58660A1/en
Application granted granted Critical
Publication of SU58660A1 publication Critical patent/SU58660A1/en

Description

Предлагаетс  легкий гальванический элемент, в частности, дл  радио-зондов .A lightweight galvanic cell is offered, in particular for radio probes.

Наиболее выгодным элементом дл  легких батарей  вл етс , как известно, элемент, в котором положительным полюсОМ служит положительна  пластина кислотного аккумул тора, а отрицательным - цинк. Однако, практическое применение этого элемента ограничиваетс  тем, что кислота быстро разъедает цинк, и элемент приходит в негодность. Амальгамирование цинка задерживает растворение цинка, но не позвол ет хранить батарею, та-к как ртуть, поднима сь по цинку, разъедает бпай цинка с свинцом. Дл  избежани  указанных вредных  влений предлагаетс , согласно изобретению, следующа  конструкци  отрицательного полюса.The most advantageous element for light batteries is, as is known, the element in which the positive plate of the acid battery is a positive plate and the negative one is zinc. However, the practical application of this element is limited by the fact that the acid quickly corrodes zinc, and the element becomes unusable. Amalgamation of zinc delays the dissolution of zinc, but does not allow the battery to be stored, as mercury rises over zinc, eats away the lead of zinc with lead. In order to avoid these harmful phenomena, according to the invention, the following construction of the negative pole is proposed.

Беретс  железна  пластинка соответствующих размеров и посредством электролиза или макани  в расплавленный загустевающий цинк покрываетс  слоем цинка -в той части, котора  должна быть опущена в кислоту. После этого оцинкованную часть покрывают амальгамой (опусканием в ртуть) и получают стойкий отрицательный полюс элемента.An iron plate of appropriate size is taken and, by electrolysis or dipping, the molten thickening zinc is coated with a layer of zinc in the part to be dipped into the acid. After that, the galvanized part is coated with amalgam (by lowering into mercury) and a stable negative pole of the element is obtained.

Предмет изобретени .The subject matter of the invention.

Гальванический элемент, одним полюсом которого служит положительна  пластинка кислотного аккумул тора, а другим - цинк, отличающийс  тем, что в качестве отрицательного полюса использована железна  пластинка , покрыта  слоем амальгамированното цинка на той ее части, которой она погружаетс  в кислоту.A galvanic cell, one pole of which is a positive plate of an acid battery, and the other is zinc, characterized in that an iron plate is used as a negative pole, is covered with a layer of amalgamated zinc on the part of it that plunges into acid.

SU2472A 1939-11-01 1939-11-01 Galvanic cell SU58660A1 (en)