SU577184A1 - Способ получени цементного сырьевого шлама - Google Patents

Способ получени цементного сырьевого шлама

Info

Publication number
SU577184A1
SU577184A1 SU7602365985A SU2365985A SU577184A1 SU 577184 A1 SU577184 A1 SU 577184A1 SU 7602365985 A SU7602365985 A SU 7602365985A SU 2365985 A SU2365985 A SU 2365985A SU 577184 A1 SU577184 A1 SU 577184A1
Authority
SU
USSR - Soviet Union
Prior art keywords
sludge
preparing raw
raw cement
magnesium oxide
slime
Prior art date
Application number
SU7602365985A
Other languages
English (en)
Inventor
Леонид Яковлевич Шевченко
Леонид Абрамович Бернштейн
Людмила Ивановна Гудилина
Original Assignee
Государственный Всесоюзный Институт По Проектированию И Научно-Исследовательским Работам "Южгипроцемент"
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Государственный Всесоюзный Институт По Проектированию И Научно-Исследовательским Работам "Южгипроцемент" filed Critical Государственный Всесоюзный Институт По Проектированию И Научно-Исследовательским Работам "Южгипроцемент"
Priority to SU7602365985A priority Critical patent/SU577184A1/ru
Application granted granted Critical
Publication of SU577184A1 publication Critical patent/SU577184A1/ru

Description

ный на основе обработанного реагентами известн кового шлама, содержит до 5% окиси магни , т.е. отвечает заданному минералогическому составу и может быть использован дл  получени  портландцёмента .
Изобретение позвол ет использовать в качестве исходного сырь  дл  получени  портландцементного клинкера высокомагнезиальные известн ки, ранее не примен вшиес .

Claims (1)

  1. Формула изобретени 
    Способ получени  цементного сырьевого шлама путем измельчени  известн кового шлама с повышенным содержанием окиси магни  и последующего совместного помола его с глин ным шламом, о тличающийс  тем, что, с целью уменьшени  содержани  окиси магни , известн ковый шлам последовательно смешивают с хлорным железом и пирофосфатом натри  и обрабатывают раствором омыленного тлллового масла.
SU7602365985A 1976-06-01 1976-06-01 Способ получени цементного сырьевого шлама SU577184A1 (ru)