Prior art keywords
fluidized bed
sulphide ores
temperature
roasting sulphide
roasting
Prior art date
Application number
SU7001494087A
Other languages
Russian (ru)
Inventor
Наталья Георгиевна Буриченкова
Владимир Викторович Ануров
Ольга Васильевна Назарова
Александр Васильевич Морозов
Валерий Игоревич Герарди
Владислав Александрович Живописцев
Владимир Сергеевич Петровский
Original Assignee
Предприятие П/Я В-8830
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Предприятие П/Я В-8830 filed Critical Предприятие П/Я В-8830
Priority to SU7001494087A priority Critical patent/SU569618A1/en
Application granted granted Critical
Publication of SU569618A1 publication Critical patent/SU569618A1/en

Links

Landscapes

  • Manufacture And Refinement Of Metals (AREA)

Description

ры в огарке, Хонаентраци  502Ог 12 до 16,3% и конценграци  осгагочного кислор{ да до 5%), его поддерживают с коррекцией по составу отход щего газа.Butts in the cinder, the concentration 502Og 12 to 16.3%, and the concentration of the oxygen from the oxygen (yes to 5%), it is supported with a correction in the composition of the exhaust gas.

Характеристика способа Линейно св зана с концентрацией сернистого ангидрида.. Мо к но поддерживать необходимую область обжига , использу  и концентрацию SOg в обжиговом газе:Characterization of the method is linearly related to the concentration of sulfur dioxide. Mo to maintain the required firing area using the concentration of SOg in the kiln gas:

до концентрации 14.2-14,3% SOg-окислительна  область; концентраци  14,3-14,7% SCfe- переходна  область} |выше концентрации 14,7% 50 -магнетизирующа  область.to a concentration of 14.2-14.3% SOg-oxidative region; a concentration of 14.3-14.7% SCfe-transition region} | above a concentration of 14.7% 50-the magnetization region.

Лабораторные исследовани  показали, что дл  получени  огарка в виде магнетита в печи кип щего сло  КС-2ОО, производитель ностью 8 тн/м в сутки температура слой Laboratory studies have shown that to obtain an calcine in the form of magnetite in a KS-2OO fluidized bed furnace, with a capacity of 8 tons / m per day, the temperature is

составила 680-690 С, температура отход щего газа-8О5-810 С, т.е. интервал разности составил 105-110 С, но область существовани  магнетизирующего обжига была тире и составила 9О-1ЗО С. Сера в огарке (магнетите)после циклона не превышала 1%amounted to 680-690 C, the temperature of the exhaust gas-8O5-810 C, i.e. the difference interval was 105-110 ° C, but the area of the existence of magnetising roasting was a dash and was 9O-1ZO C. Sulfur in the calcine (magnetite) after the cyclone did not exceed 1%

Claims (1)

Формула изобретени  Способ обжига сульфидных руд в кип щем слое, включающий регулирование кислородсодержащего дуть  и загрузку материала, отличающийс  тем, что с целью повыщени  производительности печи, получени  малосернистого магнетита, обжиг ведут при температуре в слое на 90-1 ЗО С ниже, чем температура отход щего газа, причем интервал разности температуры поддерживаю с коррекцией пр «составу обжигового газа.The invention The method of burning sulphide ores in a fluidized bed, including the regulation of oxygen-containing blowing and loading of the material, characterized in that in order to increase the productivity of the furnace, to obtain low-sulfur magnetite, the firing is carried out at a temperature in the layer by 90-1 ° C to lower than the temperature gas, and the interval of the temperature difference is maintained with the correction of the ae of the calcined gas.
SU7001494087A 1970-11-13 1970-11-13 Method for roasting sulphide ores in fluidized bed SU569618A1 (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
SU7001494087A SU569618A1 (en) 1970-11-13 1970-11-13 Method for roasting sulphide ores in fluidized bed

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
SU7001494087A SU569618A1 (en) 1970-11-13 1970-11-13 Method for roasting sulphide ores in fluidized bed

Publications (1)

Publication Number Publication Date
SU569618A1 true SU569618A1 (en) 1977-08-25

Family

ID=20460176

Family Applications (1)

Application Number Title Priority Date Filing Date
SU7001494087A SU569618A1 (en) 1970-11-13 1970-11-13 Method for roasting sulphide ores in fluidized bed

Country Status (1)

Country Link
SU (1) SU569618A1 (en)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN111057838A (en) * 2019-12-23 2020-04-24 中国科学院过程工程研究所 High-phosphorus hematite and limonite fluidized roasting system and method

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN111057838A (en) * 2019-12-23 2020-04-24 中国科学院过程工程研究所 High-phosphorus hematite and limonite fluidized roasting system and method

Similar Documents

Publication Publication Date Title
GB1364934A (en) Recovery of metal values
SU569618A1 (en) Method for roasting sulphide ores in fluidized bed
GB694036A (en) Improvements in and relating to the production of sulphur dioxide
US1749125A (en) Two-step sulphatizing roast
ES449057A1 (en) Apparatus for calcining powder materials
SU571198A3 (en) Method of two-stage roasting of pyrite in reactors with fluidized bed
US3633894A (en) Method of making calcined minerals with reduced sulfur content
SU403733A1 (en) METHOD OF OBTAINING BATTLED WELLRANGES
SU865782A2 (en) Method of sulfitizing annealing of sulfide materials
SU150629A1 (en) Method for removing mice from lead-zinc and other dusts
SU1507728A1 (en) Method of processing gypsum material
SU431119A1 (en) PIRIT BURNING METHOD
SU116773A1 (en) The method of obtaining nodded nitrous oxide
GB463122A (en) Recovery of sulphur
SU119342A1 (en) The method of roasting sulphide zinc concentrates in a fluidized bed
RU2061076C1 (en) Process of preparation of molybdenum oxide concentrate
US1151515A (en) Cementitious product.
SU136495A1 (en) Ultramarine production method
US2026775A (en) Process for sulphating the non-ferrous metals contained in ferruginous sulphide oresor roasts
SU916385A1 (en) Method for roasting pyrate concentrates
SU1303573A1 (en) Method for producing lime in rotary furnace
RU2061075C1 (en) Process of preparation of oxide molybdenum concentrate
SU110295A1 (en) Method for processing vanadium-containing iron ores
SU1063770A1 (en) Process for producing sulfur dioxide and lime
RU2336239C2 (en) Method for aluminous cement processing