SU531694A1 - The method of cold welding gray iron - Google Patents

The method of cold welding gray iron

Info

Publication number
SU531694A1
SU531694A1 SU2029572A SU2029572A SU531694A1 SU 531694 A1 SU531694 A1 SU 531694A1 SU 2029572 A SU2029572 A SU 2029572A SU 2029572 A SU2029572 A SU 2029572A SU 531694 A1 SU531694 A1 SU 531694A1
Authority
SU
USSR - Soviet Union
Prior art keywords
cold welding
gray iron
gray
iron
welding
Prior art date
Application number
SU2029572A
Other languages
Russian (ru)
Inventor
Геннадий Васильевич Фомичев
Original Assignee
Каменский Комбинат Искусственного Волокна
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Каменский Комбинат Искусственного Волокна filed Critical Каменский Комбинат Искусственного Волокна
Priority to SU2029572A priority Critical patent/SU531694A1/en
Application granted granted Critical
Publication of SU531694A1 publication Critical patent/SU531694A1/en

Description

чающийс  тем, что, с целью повышени  качества сварного шва и снижени  термических напр жений в соединенин, разделку кромок выполн ют стуненчатой с максимальной шириной разделки 0,5-0,7 толщины свариваемого металла и дополнительным углублением внутри разделки на 0,1-0,15 толщины свари заемого металла с последующим наилавлением подготовительных слоев на всю поверхность разделки параллельными валиками, приDue to the fact that, in order to improve the quality of the weld and reduce thermal stresses in the joint, the edge grooves are made stepwise with a maximum groove width of 0.5-0.7 of the thickness of the metal to be welded and an additional recess inside the groove by 0.1-0, 15 thickness of the weld metal with the subsequent fusion of the preparatory layers on the entire surface of the cutting with parallel rollers, with

i/TOM между подготовительными сло ми оставл ют зазор, равный 107-,1 диаметра электрода, а после наплавки валиков полученный зазор заилавл ют.The i / TOM between the preparatory layers left a gap of 107-, 1 the diameter of the electrode, and after the welds were deposited, the resulting gap was cast.

Источники информации, прин тые во внимание при экспертизе:Sources of information taken into account in the examination:

1. Г. А. Асиковска , Ю. И. Журавицкий «Газова  сварка , М., Машииостроение , 1974 г. стр. 64, рис. 37 а.1. G. A. Asikovska, Yu. I. Zhuravitsky “Gas welding, M., Mashiostroenie, 1974, p. 64, fig. 37 a.

SU2029572A 1974-06-03 1974-06-03 The method of cold welding gray iron SU531694A1 (en)