SU50965A1 - Способ переработки лопаритовых руд или концентратов - Google Patents

Способ переработки лопаритовых руд или концентратов

Info

Publication number
SU50965A1
SU50965A1 SU165607A SU165607A SU50965A1 SU 50965 A1 SU50965 A1 SU 50965A1 SU 165607 A SU165607 A SU 165607A SU 165607 A SU165607 A SU 165607A SU 50965 A1 SU50965 A1 SU 50965A1
Authority
SU
USSR - Soviet Union
Prior art keywords
niobium
ores
tantalum
concentrates
loparite
Prior art date
Application number
SU165607A
Other languages
English (en)
Inventor
К.К. Белоглазов
А.Н. Кузнецов
Original Assignee
К.К. Белоглазов
А.Н. Кузнецов
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by К.К. Белоглазов, А.Н. Кузнецов filed Critical К.К. Белоглазов
Priority to SU165607A priority Critical patent/SU50965A1/ru
Application granted granted Critical
Publication of SU50965A1 publication Critical patent/SU50965A1/ru

Description

в последнее врем  как в металлургии , так и в радиотехнике редкие металлы-ниобий и тантал наход т все большее и ббльшее применение. Причиной , тормоз щей внедрение этих металлов в промышленность,  вл етс  с одной стороны трудность, переработки как самих тантало ниобиевых руд, так и получение металлического тантала и ниоби , а с другой стороны незначительное количество руд, из которых экономически выгодно было бы получать соединени  тантала и ниоби . Большой интерес представл ют руды , недавно открытые на Кольском полуострове, содержащие на р ду с редкими земл ми соединени  тантала и ниоби ; из них особое место по своему значению занимает лопарит , содержащий (в чистом минерале) п тиокисей тантала и ниоби  до 12%, редких земель до 32%, окиси титана 39/О В не обогащенных лопартиовых рудах содержание редких земель-0 ,65% и п тиокисей тантала и ниоби -0,21%. Обработка лопарита вызывает чрезвычайно большие затруднени  (в химическом отношении); этот минерал не раствор етс  в обычных кислотах, а требует обработки плавиковой кислотой или сплавлени  со щелочами. При этих операци х окись титана переходит в раствор, и отделение ее от соединени  ниоби  и тантала чрезвычайно затруднительно. Авторами насто щего изобретени  разработан способ при котором извлечение редких земель и п тиокисей тантала и ниоби  идет совместно с отделени ми их от окиси титана и пустой породы. Предлагаемый, согласно насто щему изобретению, способ заключаетс  в следующем. Руда содержаща  минерал лопарит или лопаритовый концентрат , смешиваетс  с хлористым аммонием в отнощении 1 :1 и окисью меди 0,05-0,10 по весу. Шихта постепенно нагреваетс  до температуры 200-250 и выдерживаетс  при этой температуре несколько часов (от 3 до 4), затем температура повыщаетс  до 350-400 с целью отгона избытка хлористого аммони . При этих услови х TiOs не дает хлористых соединений , что позвол ет провести полное отделение титана от ниоби  и тантала. Спек выщелачиваетс  слабой азотной кислотой при температуре 80°, отфильтровываетс  от осадка, содержащего пустую породу и всю окись титана. Из фильтрата осаждаютс  аммиаком все редкие земли и окиси тантала и ниоби . Осадок отфильтровываетс . Раствор, содержащий аммонийные соли и соли меди, поступает на регенерацию хлористого аммони  и меди.
Осадок редких земель и окисей тантала и ниоби  обрабатываетс  уже обычным способом с целью отделени  редких земель. Так как при этом способе обработки руды окись титана в раствор не переходит, то это обсто тельство значительно упрощает отделение п тиокисей тантала и ниоби  от редких земель.
Выход редких земель и окисей тантала и ниоби  при этом способе доПредмет изобретени .
Способ переработки лопаритовых руд или концентратов, отличающийс  тем, что в исходную руду (или концентрат ), смещанную с хлориетым аммонием, добавл ют в количестве до 0,1 части по весу окись меди, после чего шихту нагревают сначала до 200-250°, выдерживают при этой температуре несколько часов, затем, в цел х отгонки избытка хлористого амхони , температуру подымают до 350-400° и полученный спек выщелачивают слабой азотной кислотой, осадок, содержащий пустую породу и окись титана, отфильтровывают, а из фильтрата обычным способом осаждают редкие земли вместе с танталом и ниобием.
SU165607A 1936-06-07 1936-06-07 Способ переработки лопаритовых руд или концентратов SU50965A1 (ru)