SU482474A1 - The method of imitation mother of pearl - Google Patents

The method of imitation mother of pearl

Info

Publication number
SU482474A1
SU482474A1 SU1964236A SU1964236A SU482474A1 SU 482474 A1 SU482474 A1 SU 482474A1 SU 1964236 A SU1964236 A SU 1964236A SU 1964236 A SU1964236 A SU 1964236A SU 482474 A1 SU482474 A1 SU 482474A1
Authority
SU
USSR - Soviet Union
Prior art keywords
pearl
imitation
mother
imitation mother
polymethyl methacrylate
Prior art date
Application number
SU1964236A
Other languages
Russian (ru)
Inventor
Марк Юдович-Яковлевич Немлихер
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed filed Critical
Priority to SU1964236A priority Critical patent/SU482474A1/en
Application granted granted Critical
Publication of SU482474A1 publication Critical patent/SU482474A1/en

Description

1one

Изобретение относитс  к области имитации перламутра.The invention relates to the field of imitation nacre.

Известен способ имитации перламутра, по которому изделие изготавливают прессованием полиметилметакрилата с «жемчужным патом и полистиролом под давлепием 150- 320 кг/см при температуре 170-190°С. После отверждени  мономера получают листовые заготовки с перламутровым рисунком. Однако при известном способе используют дефицитный «жемчужный пат.There is a method of imitation nacre, according to which the product is made by pressing polymethyl methacrylate with pearl stalemate and polystyrene under pressure of 150-320 kg / cm at a temperature of 170-190 ° C. After curing of the monomer, sheet blanks with a pearlescent pattern are obtained. However, with the known method using a scarce "pearl Pat.

С целью исключени  дефицитного сырь  заготовки из полиметилметакрилата нагревают до 240-300°С и прессуют при давлении 15-40 кг/см в течение 0,5-1 мин.In order to eliminate the scarce raw material, polymethyl methacrylate billet is heated to 240-300 ° C and pressed at a pressure of 15-40 kg / cm for 0.5-1 min.

При этом во врем  прессовани  заготовка, уменьша сь по толщине в 5-ЛО раз, создает причудливый перламутроподобиый рисунок.At the same time, during pressing, the billet, having decreased in thickness by a factor of 5 -LO, creates a fancy pearl-like pattern.

Предметизобретеии The subject of the invention

Способ имитации перламутра путем нагрева и прессовани  полиметилметакрилата, отличающийс  тем, что, с целью исключеПИЯ дефицитного сырь , листовые заготовки из .полиметилметакрилата натревают до 240- 300°С и прессуют при давлении 15-40 кг/см в течение 0,5 мин-1 мии.A method of imitating nacre by heating and pressing polymethyl methacrylate, characterized in that, in order to eliminate the deficient raw material, sheet blanks of polymethyl methacrylate are shed to 240-300 ° C and pressed at a pressure of 15-40 kg / cm for 0.5 min-1 missions.

Приоритет 11.12.66.Priority 11.12.66.

SU1964236A 1973-09-27 1973-09-27 The method of imitation mother of pearl SU482474A1 (en)