1one
Изобретение относитс к области получени соединений фосфора, в частности монофторфосфата бари .The invention relates to the field of producing phosphorus compounds, in particular barium monofluorophosphate.
Известен способ получени монофторфосфата бари путем плавлени при температуре выше метафосфата бари и фторида бари , вз тых в эквимолекул рных количествах , и кристаллизации из расплава монофторфосфата бари .A known method for producing barium monofluorophosphate is by melting at temperatures above barium metaphosphate and barium fluoride, taken in equimolar amounts, and crystallization from barium monofluorophosphate melt.
При осуществлении известного способа происходит частичное разложение монофторфосфата бари с потерей фтора и образованием б-Ва2Р2О7. При этом в продукте содержитс всего 20% монофторфосфата бари .In the implementation of the known method, partial decomposition of barium monofluorophosphate occurs with loss of fluorine and the formation of b-Ba2P2O7. At the same time, only 20% barium monofluorophosphate is contained in the product.
Дл повышени выхода продукта предлагаетс вести процесс при 800-850°С.To increase the yield of the product, it is proposed to conduct the process at 800-850 ° C.
Проведение процесса при 800-850°С позвол ет осуществл ть его без плавлени компонентов , что приводит к увеличению содержани монофторфосфата бари в готовом продукте до 95%.Carrying out the process at 800-850 ° C allows it to be carried out without melting the components, which leads to an increase in the content of barium monofluorophosphate in the finished product to 95%.
Пример. Смешивают 88,4 г Ва(РОз)2 и 52 г Вар2 и помещают смесь в тигель из стеклоуглерода . Закрытый тигель став т в другой тигель из кварцевого стекла и далее - в электрическую печь, нагретую до 850°С. Кварцевый тигель плотно закрывают пришлифованной крышкой. По огнеупорной трубке, вмазанной в крышку, во внутреннюю полость кварцевого тигл подают предварительно осушенный азот или аргон. Через 45-60 мин тигель из печи вынимают и извлекают продукт. В готовом продукте содержитс 95% монофторфосфата бари .Example. 88.4 g of Ba (PO3) 2 and 52 g of Var2 are mixed and the mixture is placed in a glass carbon crucible. A closed crucible is placed in another quartz glass crucible and then in an electric furnace heated to 850 ° C. The quartz crucible is tightly closed with a polished lid. The pre-dried nitrogen or argon is fed into the internal cavity of the quartz crucible through a refractory tube, which is plastered into the lid. After 45-60 minutes, the crucible is removed from the furnace and the product is removed. The finished product contains 95% barium monofluorophosphate.
Предмет изобретени Subject invention
Способ получени монофторфосфата бари путем взаимодействи метафосфата бари с фторидом бари при нагревании, отличающийс тем, что, с целью повышени выхода продукта, процесс ведут при 800-850°С.The method of producing barium monofluorophosphate by reacting barium metaphosphate with barium fluoride by heating, characterized in that, in order to increase the yield of the product, the process is carried out at 800-850 ° C.
Priority Applications (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
SU1880414A SU453351A1 (en) | 1973-02-09 | 1973-02-09 | Method of producing barium monofluorophosphate |
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
SU1880414A SU453351A1 (en) | 1973-02-09 | 1973-02-09 | Method of producing barium monofluorophosphate |
Publications (1)
Publication Number | Publication Date |
---|---|
SU453351A1 true SU453351A1 (en) | 1974-12-15 |
Family
ID=20541732
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
SU1880414A SU453351A1 (en) | 1973-02-09 | 1973-02-09 | Method of producing barium monofluorophosphate |
Country Status (1)
Country | Link |
---|---|
SU (1) | SU453351A1 (en) |
-
1973
- 1973-02-09 SU SU1880414A patent/SU453351A1/en active
Similar Documents
Publication | Publication Date | Title |
---|---|---|
ATE16473T1 (en) | PROCESSES AND FURNACES FOR THE PRODUCTION OF SILICON CARBIDE. | |
SU453351A1 (en) | Method of producing barium monofluorophosphate | |
DK523284D0 (en) | PROCEDURE FOR THE MANUFACTURE OF FINDED, HIGH-EFFECTIVE MAGNIUM AND ITS USE | |
Al-Jabar et al. | The synthesis of perfluoro-1, 6-disubstituted triptycenes containing group IV and group V elements | |
CA1079613A (en) | Process for synthesizing and growing single crystalline beryl out of a molten salt | |
Waterworth et al. | Raman studies into the constitution of gallium iodides of intermediate composition | |
SU392003A1 (en) | METHOD OF OBTAINING ANHYDROUS FLUOROUTANT OF MAGNESIUM, CALCIUM AND STRONTIUM | |
SU512171A1 (en) | The method of obtaining monofluorophosphate alkali and alkaline earth metals | |
US1865204A (en) | Production of volatile fluorides | |
RU1075677C (en) | Method of producing complex salt of tricaprolactamocopper monohydrate dichloride | |
SU874616A1 (en) | Method of producing mixed sodium and calcium phosphate | |
SU513935A1 (en) | Method for producing rare earth metaphosphates | |
SU1216150A1 (en) | Antimony metaphosphate with polymer structure and method of producing same | |
SU1446107A1 (en) | Method of producing dehydrated potassium methasilicate | |
SU481188A1 (en) | The method of producing uranium oxideichloride | |
JPS526309A (en) | Temperature zone melting process using no crucible | |
SU1723037A1 (en) | Method of producing lead sulfide | |
RU1801948C (en) | Method for calcium fluoride production | |
SU658869A1 (en) | Method for producing tungsten trichloride | |
SU559897A1 (en) | The method of producing alkali metal fluorobromates | |
SU516641A1 (en) | The method of obtaining asbestos from the gas phase | |
SU447368A1 (en) | The method of obtaining potassium tridecafluorciconate | |
SU698917A1 (en) | Composition for preparing nitrous oxide | |
SU512210A1 (en) | The method of producing potassium hydromelonate | |
US2356529A (en) | Purifying metals |