SU449976A1 - Alloy for deoxidizing and alloying steel - Google Patents
Alloy for deoxidizing and alloying steelInfo
- Publication number
- SU449976A1 SU449976A1 SU1611736A SU1611736A SU449976A1 SU 449976 A1 SU449976 A1 SU 449976A1 SU 1611736 A SU1611736 A SU 1611736A SU 1611736 A SU1611736 A SU 1611736A SU 449976 A1 SU449976 A1 SU 449976A1
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- alloy
- steel
- deoxidizing
- alloying steel
- alloying
- Prior art date
Description
1one
Изобретение относитс к области черной металлургии и может быть использовано дл повышени качества сталей.The invention relates to the field of ferrous metallurgy and can be used to improve the quality of steel.
Известен сплав дл раскислени и легировани стали, содержаш,ий кремний, марганец, хром, углерод, железо.Known alloy for deoxidation and alloying of steel containing silicon, manganese, chromium, carbon, iron.
С целью повышени пластических свойств обрабатываемой стали в предлагаемый сплав дополнительно ввод т РЗМ, и компоненты вз ты в следующем соотношении, вес. %: Кремний6,5-30,0In order to increase the plastic properties of the steel being treated, REMs are additionally introduced into the proposed alloy, and the components are taken in the following ratio, weight. %: Silicon6.5-30.0
Марганец6,5-30,0Manganese6.5-30.0
Хром0,1-60,0Chrome 0.1-60.0
Углерод0,1-3,0Carbon 0.1-3.0
РЗМ0,1-6,0РЗМ0,1-6,0
ЖелезоОстальноеIronErest
Применение предлагаемого сплава обеспечивает более полное удаление кислорода и снижение содержани серы в обрабаи:,ваемой стали.The use of the proposed alloy provides a more complete removal of oxygen and a decrease in the sulfur content in the processed steel.
Благодар этому сталь, обработанна описываемым сплавом, имеет ударную в зкость Ск до 9,2 кгм/см.Due to this, the steel treated with the alloy described has an impact strength of Ck to 9.2 kgm / cm.
22
Сплав получают методом переплава в дуговой электропечи с основной футеровкой.The alloy is produced by remelting in an electric arc furnace with a base lining.
Соответствующие ферросплавы, стальнойSuitable ferroalloys, steel
лом и другие ввод т в период завалки. Полученный сплав выпускают в ковш, а редкоземельные элементы, например ферроцерий,scrap and others are introduced during the filling period. The resulting alloy is released into the ladle, and rare earth elements, such as ferrocerium,
ввод т в ковш при выпуске в него сплава.is introduced into the ladle when the alloy is released into it.
Предмет изобретени Subject invention
Сплав дл раскислени и легировани стали , содержащий кремний, марганец, хром, углерод, железо, о т л и ч а ю щ и и с тем, что, с целью повышени пластических свойств обрабатываемой стали, в него дополнительно ввод т РЗМ, и компоненты вз ты в следующем соотношении, вес. %:An alloy for deoxidation and alloying of steel containing silicon, manganese, chromium, carbon, iron, and the fact that, in order to increase the plastic properties of the steel being treated, REM and components are additionally introduced into it. taken in the following ratio, weight. %:
Кре.мний0,5-30,0Kret.mniy 0,5-30,0
Марганец6,5-30,0Manganese6.5-30.0
Хром0,1-60,0Chrome 0.1-60.0
Углерод0,1-3,0Carbon 0.1-3.0
РЗМ0,1--0,0РЗМ0,1--0,0
ЖелезоОсг ,IronOsg,