SU435290A1 - Способ модифицирования стали и сплавов - Google Patents
Способ модифицирования стали и сплавовInfo
- Publication number
- SU435290A1 SU435290A1 SU1807024A SU1807024A SU435290A1 SU 435290 A1 SU435290 A1 SU 435290A1 SU 1807024 A SU1807024 A SU 1807024A SU 1807024 A SU1807024 A SU 1807024A SU 435290 A1 SU435290 A1 SU 435290A1
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- steel
- modification
- alloys
- alkaline earth
- earth metals
- Prior art date
Description
1
Изобретение относитс к электрометаллургии .
Известен способ введени реагентов в сталь порци ми с интервалом 5-15 мин за 5-60 мин до выпуска из печи, причем кажда порци может составить 0,05-0,20% от веса расплава.
Недостатком известного способа вл етс нестабильность усвоени элементов - модификаторов .
Цель изобретени - обеспечение стабильных результатов модифицировани при минимальной загр зненности стали кислородом и неметаллическими включени ми, т. е. повышение качества металла и увеличение выхода годного.
Согласно предлагаемому способу щелочноземельные металлы ввод т в период рафинировани в течение 5-60 мин с последующей выдержкой металла в печи в течение 2- 10 мин.
Во врем модифицировани щелочноземельные металлы раствор ютс в расплаве. Образующиес продукты раскислени всплывают в шлак.
Применение щелочноземельных металлов в сочетании позвол ет, кроме того, формировать наиболее благопри тные неметаллические включени .
10
Предмет изобретени
Способ модифицировани стали и сплавов в электропечи введением щелочноземельных металлов, отличающийс тем, что, с целью повышени качества металла и увеличени выхода годного, щелочноземельные металлы ввод т в период рафинировани в течение 5-60 мин с последующей выдержкой металла в печи в течение 2-10 мин.