SU413197A1 - - Google Patents

Info

Publication number
SU413197A1
SU413197A1 SU1847179A SU1847179A SU413197A1 SU 413197 A1 SU413197 A1 SU 413197A1 SU 1847179 A SU1847179 A SU 1847179A SU 1847179 A SU1847179 A SU 1847179A SU 413197 A1 SU413197 A1 SU 413197A1
Authority
SU
USSR - Soviet Union
Prior art keywords
refractory
magnesium
tip
iron
porous
Prior art date
Application number
SU1847179A
Other languages
English (en)
Russian (ru)
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed filed Critical
Priority to SU1847179A priority Critical patent/SU413197A1/ru
Application granted granted Critical
Publication of SU413197A1 publication Critical patent/SU413197A1/ru

Links

Landscapes

  • Muffle Furnaces And Rotary Kilns (AREA)
SU1847179A 1972-11-20 1972-11-20 SU413197A1 (no)

Priority Applications (1)

Application Number Priority Date Filing Date Title
SU1847179A SU413197A1 (no) 1972-11-20 1972-11-20

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
SU1847179A SU413197A1 (no) 1972-11-20 1972-11-20

Publications (1)

Publication Number Publication Date
SU413197A1 true SU413197A1 (no) 1974-01-30

Family

ID=20532340

Family Applications (1)

Application Number Title Priority Date Filing Date
SU1847179A SU413197A1 (no) 1972-11-20 1972-11-20

Country Status (1)

Country Link
SU (1) SU413197A1 (no)

Similar Documents

Publication Publication Date Title
SU504462A3 (ru) Способ нагрева металла в выпуском отверстии промежуточной емкости при непрерывной разливке
ES8207229A1 (es) Dispositivo de tratamiento de un bano de metal liquido con- tenido en un recipiente, por inyeccion de gas
ATE50601T1 (de) Vorrichtung und verfahren zum warmhalten von fluessigen metallschmelzen.
KR100583221B1 (ko) 용융 유리용 진공 탈가스 장치 및 진공 탈가스 장치의 온도를 상승시키는 방법
NO155396C (no) Innretning for fysikalsk-kjemisk rensing av flytende metaller og legeringer.
SU413197A1 (no)
PL192625B1 (pl) Sposób odwęglania ciekłej stali
SU540296A1 (ru) Устройство дл обработки жидкого металла магнием, кальцием и их смесью
US3942260A (en) Method and apparatus for drying the refractory lining
US3497196A (en) Device for introducing material into a degassing vessel for steel
JPH0693429A (ja) 真空蒸着装置用るつぼ
ATE25017T1 (de) Vorrichtung zum metallurgischen behandeln von fluessigen metallen.
SU901802A1 (ru) Способ запуска тепловой трубы
SU521317A1 (ru) Способ модифицировани чугуна
US1571289A (en) Casehardening
SU403735A1 (ru) Устройство для продувки жидкого чугуна азотом
SU289748A1 (ru) Устройство дл подачи и слива расплавленного металла из вакуумной печи
SU594177A1 (ru) Устройство дл ввода жидкого магни в чугун
FR2364719A1 (fr) Perfectionnement aux fours a induction pour la coulee ou pour la coulee continue et aux poches de traitement
RU2232363C1 (ru) Шахтная печь сопротивления для термической обработки деталей из сталей и сплавов
SU600192A1 (ru) Печь дл термообработки
GB1121996A (en) Improved method of, and plant for, degassing molten metals or alloys during casting
SU709690A1 (ru) Устройство дл ввода реагентов в жидкий металл
SU1705348A1 (ru) Устройство дл обработки чугуна
SU212278A1 (ru) В.ИБЛИОТЕНА IУСТАНОВКА дл