SU399942A1 - METHOD OF MANUFACTURING ZINC ELECTRODE CHEMICAL SOURCE CURRENT - Google Patents

METHOD OF MANUFACTURING ZINC ELECTRODE CHEMICAL SOURCE CURRENT

Info

Publication number
SU399942A1
SU399942A1 SU1770883A SU1770883A SU399942A1 SU 399942 A1 SU399942 A1 SU 399942A1 SU 1770883 A SU1770883 A SU 1770883A SU 1770883 A SU1770883 A SU 1770883A SU 399942 A1 SU399942 A1 SU 399942A1
Authority
SU
USSR - Soviet Union
Prior art keywords
source current
zinc electrode
chemical source
electrode chemical
manufacturing zinc
Prior art date
Application number
SU1770883A
Other languages
Russian (ru)
Inventor
В. В. Тризно Л. Г. Рувинский
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed filed Critical
Priority to SU1770883A priority Critical patent/SU399942A1/en
Application granted granted Critical
Publication of SU399942A1 publication Critical patent/SU399942A1/en

Description

(1(one

Известен способ изготовлени  цинкового электрода химического источника тока путем смешивапи  окиси цинка с цинковой пылью и поливиниловым спиртом, многократного пропускани  смеси через сита и сушки с последующей напрессовкой на токоотвод.A known method of making a zinc electrode of a chemical current source is by mixing zinc oxide with zinc dust and polyvinyl alcohol, repeatedly passing the mixture through sieves and drying, followed by pressing on the collector.

При продавливании влажной смеси через отверсти  сита образующиес  стержни слипаютс . В результате в процессе последующей сушки образуютс  агломераты слипшихс  частиц , которые необходимо дробить многократным пропусканием через сита, что усложн ет технологический процесс и способствует истиранию частиц. При этом возникает много пыли, котора  увеличивает количество отходов и нарушает однородность порошка.When the wet mixture is forced through the sieve holes, the resulting rods stick together. As a result, during the subsequent drying, agglomerates of sticky particles are formed, which must be crushed by repeated passage through sieves, which complicates the process and contributes to abrasion of the particles. This creates a lot of dust, which increases the amount of waste and violates the uniformity of the powder.

Целью изобретени   вл етс  упрощение технологии способа.The aim of the invention is to simplify the process technology.

По предложепному способу смесь перед первым пропусканием через сито подсушивают до влажности 12-15%.According to the proposed method, the mixture is first dried through a sieve to a moisture content of 12-15%.

22

В зкую смесь окиси цинка, цинковой пыли и поливипилового спирта подсушивают до влажности 12-15%, после чего пропускают через сито с размером  чеек 1 мм. Полученный грапул т повторно сушат до влажности 0,1-0,5% и пропускают через сито с размером  чеек 2 мм. Затем гранулированную массу напрессовывают на токоотвод.The viscous mixture of zinc oxide, zinc dust, and polyvinyl alcohol is dried to a moisture content of 12–15%, after which it is passed through a 1 mm sieve. The resulting grapule is re-dried to a moisture content of 0.1-0.5% and passed through a sieve with a mesh size of 2 mm. Then the granulated mass is pressed onto the current lead.

При этом электрод имеет высокую однородность и стабильную объемную массу.In this case, the electrode has a high homogeneity and a stable bulk density.

Предмет изобретени Subject invention

Способ изготовлени  цинкового электрода химического источника тока путем смешивани  окиси цинка с цинковой пылью и поливиниловым спиртом, многократного пропускани  смеси через сита и сушки с последуюшей напрессовкой на токоотвод, отличающийс  тем, что, с целью упрощени  технологии, смесь перед первым пропусканием через сито подсушивают до влажности 12-15%.A method of making a zinc electrode of a chemical current source by mixing zinc oxide with zinc dust and polyvinyl alcohol, repeatedly passing the mixture through sieves and drying, followed by pressing onto a collector, characterized in that, in order to simplify the technology, the mixture is dried before the first passing through the sieve to moisture 12-15%.

SU1770883A 1972-04-10 1972-04-10 METHOD OF MANUFACTURING ZINC ELECTRODE CHEMICAL SOURCE CURRENT SU399942A1 (en)