SU390175A1 - Способ рафинирования магния - Google Patents

Способ рафинирования магния

Info

Publication number
SU390175A1
SU390175A1 SU1741960A SU1741960A SU390175A1 SU 390175 A1 SU390175 A1 SU 390175A1 SU 1741960 A SU1741960 A SU 1741960A SU 1741960 A SU1741960 A SU 1741960A SU 390175 A1 SU390175 A1 SU 390175A1
Authority
SU
USSR - Soviet Union
Prior art keywords
magnesium
ligature
zirconium
refining
refination
Prior art date
Application number
SU1741960A
Other languages
English (en)
Inventor
В. В. Род кин Э. Н. Сулейменов А. И. Папин витель Н. А. Байтенев
Original Assignee
Т. Е. Худайбергенов , А. М. Кунаев Институт металлургии , обогащени Казахской ССР
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Т. Е. Худайбергенов , А. М. Кунаев Институт металлургии , обогащени Казахской ССР filed Critical Т. Е. Худайбергенов , А. М. Кунаев Институт металлургии , обогащени Казахской ССР
Priority to SU1741960A priority Critical patent/SU390175A1/ru
Application granted granted Critical
Publication of SU390175A1 publication Critical patent/SU390175A1/ru

Description

1
Изобретение относитс  к технологии рафинировани  металлического магни , примен емого в качестве восста-новител  при магниетермическом получении металлического циркони .
Известен способ рафинировани  магни  солевой лигатурой низших хлоридов металлов, по которому рафинирова.ние осуществл ют солевой лигатурой низших хлоридов титана при расходе титана 0,2% от веса магни .
Недостатком известного способа  вл етс  введение в магний титана, который в значительной степени сказываетс  на качестве металлического циркони , получаемого магниетермическим способом.
Предложенный способ отличаетс  от известного тем, что рафинирование осуществл ют солевой лигатурой низших хлоридов циркони  при соотношении хлоридов кали  и натри  от 3 : 1 до 1 : 3 и содержании |Циркони 2-6 вес.% Это способствует получению высокочистого магни .
Солевую лигатуру КС1-NaCl-ZrCb-ZrCl;; ввод т в виде твердых кусков размером 20-60 мм на поверхность жидкого магни  с температурой 680 - 720°С. Соотношение KCL : NaCL равно от 3 : 1 до 1:3, содержание циркони  в лигатуре 2 - 6 вес.%, количество лигатуры берут из расчета получени  металлического циркони  0,18 - 0,45% и выше от
веса жидкого магни . Высокодисперсный р -фипирующий агент - металличоскпп unpKonnii образуетс  по реакции:
ZrCI, + + MgCU 2ZrCI., + 3Mg 2Zr -f SMgCIj
Свежевосстановленный цирконий обладает .наибольшей геттерной способностью и поэтому активно адсорбирует примеси из магни . Применение низших хлоридов циркони  в чистом виде затруднительно из-за гигроскопичности и высокой химической активности.
Способ апробирован в лабораторных услови х .
При М ер. Магний-сырец в количестве 2,8 кг расплавл ют в стальном стакане и при температуре 700°С ввод т лигатуру следующего состава: KCL : NaCL 1 : 1, количество ZrCL, составл ет 7% от веса лигатуры. Лигатуру ввод т в количестве 150 г, т. е. количество металлического циркони  составл ет 0,21% от веса магни . Врем  перемешивани  и расплавлени  лигатуры 8 мин. Общее количество примесей при рафинировании снижаетс  с 0,37 до
0,011%. Металлического циркони  в магнии остаетс  0,008%.
Предмет изобретени 
Способ рафинировани  магни  солевой лигатурой низших хлоридов металлов, отличаю3 . щийс  тем, что, с целью получени  высокочистого магни , рафинирова«ие осуществл ют солевой лигатурой низших хлоридов циркони  4 при соотношении хлоридов кали  и натри  of 3 : 1 до 1 :3 и содержании циркони  2 - 6 вес.%
SU1741960A 1972-01-31 1972-01-31 Способ рафинирования магния SU390175A1 (ru)