SU388058A1 - - Google Patents

Info

Publication number
SU388058A1
SU388058A1 SU1662692A SU1662692A SU388058A1 SU 388058 A1 SU388058 A1 SU 388058A1 SU 1662692 A SU1662692 A SU 1662692A SU 1662692 A SU1662692 A SU 1662692A SU 388058 A1 SU388058 A1 SU 388058A1
Authority
SU
USSR - Soviet Union
Prior art keywords
metal
gallium
deposited
coating
trisubstituted
Prior art date
Application number
SU1662692A
Other languages
English (en)
Inventor
В. А. Ларионов Л. Б. Андреев Б. А. Красюк М. Б. Вайнштейн
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed filed Critical
Priority to SU1662692A priority Critical patent/SU388058A1/ru
Application granted granted Critical
Publication of SU388058A1 publication Critical patent/SU388058A1/ru

Description

СПОСОБ ХИМИЧЕСКОГО ОСАЖДЕНИЯ МЕТАЛЛОВ
1
Изобретение относитс  к области нанесени  металлических покрытий.
Известен способ химического осаждени  металлов на металлическую поверхность из раствора, содержащего соль осаждаемого металла , при контактировании покрываемой поверхности с металлом более электроотрицательным , чем осаждаемый.
Предлагаемый способ отличаетс  от известного тем, что в качестве соли осаждаемого металла используют хлористый галлий, в в ;раствор ввод т лимоннокислый натрий и трехзамещенный едкий натр три определенном соотношении компонентов и процесс ведут при 18-30°С и рН 13-14.
Сущность предлагаемого способа заключаетс  в том, что, с целью нанесени  галлиевого покрыти  на металлическую поверхность ее обрабатывают раствором, содержащим, г/л: Хлористый галлий200-300
Лимоннокислый натрий5--15
Трехзамещенный едкий «атр 250-400, процесс обработки ведут при контактировании покрываемой поверхности с металлом более электроотрицательным, чем осаждаемый, при 18-30°С и рН 13-14 в течение 30- 50 мин.
Пример. Галлиевое покрытие нанос т на поверхность медных изделий с щелью их диффузионной пайки.
Осаждение галли  осуществл ют из раствора , содержащего,
Хлористый галлий240
Лимо-ннокислый натрий10
Трехзамещенный едкий натр (уд. вес 1,507)300,
при контактировании покрываемой поверхности с алюминием, при 18-30°С и рП 14 в течение 40 мин.
В результате получают равномерное по толщине покрытие, которое отвечает всем требовани м , предъ вл емым при диффузионной пайке.
Предмет изобретени 
Способ химического осаждени  металлов на металлическую поверхность из раствора, содержащего соль осаждаемого .металла, при контактировании покрываемой поверхности с металлом более электроотрицательным, чем осаждаемый, отличающийс  тем, что, с целью осаждени  галлиевого покрыти , в качестве соли осаждаемого металла используют хлористый галлий, в раствор ввод т лимоннокислый «атрий и, едкий натр при следующем соотнощении .компонентов,
Хлористый галлий200-300
Лимоннокислый натрий5-15
Трехзамещенный едкий натр 250-400, и процесс ведут при 18-30°С и рН 13-14.
SU1662692A 1971-05-31 1971-05-31 SU388058A1 (ru)