SU208953A1 - METHOD OF ELECTROLYSIS OF ANTIMONY FROM ORGANIC ELECTROLYTES - Google Patents

METHOD OF ELECTROLYSIS OF ANTIMONY FROM ORGANIC ELECTROLYTES

Info

Publication number
SU208953A1
SU208953A1 SU1136115A SU1136115A SU208953A1 SU 208953 A1 SU208953 A1 SU 208953A1 SU 1136115 A SU1136115 A SU 1136115A SU 1136115 A SU1136115 A SU 1136115A SU 208953 A1 SU208953 A1 SU 208953A1
Authority
SU
USSR - Soviet Union
Prior art keywords
antimony
electrolysis
organic electrolytes
solution
electrolyte
Prior art date
Application number
SU1136115A
Other languages
Russian (ru)
Original Assignee
Ю. Я. Фиалков , В. П. Басов
Publication of SU208953A1 publication Critical patent/SU208953A1/en

Description

Известен способ электролиза сурьмы из органических электролитов, содержащих трехвалентную сурьму и иделочные галогениды.The known method of electrolysis of antimony from organic electrolytes containing trivalent antimony and fractional halides.

Дл  получени  чистой сурьмы лучших марок в процессе электролиза предлагаетс  в качестве электролита использовать раствор хлоридов лити  и треххлористой сурьмы в метиловом спирте. При этом процесс электролиза ведут при комнатной гемпературе и плотности тока на катоде 0,5-1,0 а/дм.In order to obtain pure antimony of the best brands in the electrolysis process, it is proposed to use as a electrolyte a solution of lithium chlorides and antimony trichloride in methyl alcohol. The process of electrolysis is carried out at room temperature and current density at the cathode of 0.5-1.0 a / dm.

Оптимальное соотношение компонентов электролита: треххлористой сурьмы 380 г/лThe optimal ratio of electrolyte components: antimony trichloride 380 g / l

(5 н. раствор) и хлористого лити  84,8 г/л (2 н. раствор). Электролит готов т обычным способом из реактивных препаратов; плотность его при 25°С .равна 1,53, в зкость 2,97 спз, удельна  электропроводность 2. OM-i-CM-i.(5 n solution) and lithium chloride 84.8 g / l (2 n solution). The electrolyte is prepared in the usual way from reactive preparations; its density at 25 ° С is equal to 1.53, the viscosity is 2.97 spz, specific conductivity 2. OM-i-CM-i.

При катодной плотности 0,5-1,0 а/дм осаждаетс  плотный светло-серый осадок металлической сурьмы высокой степени чистоты.At a cathode density of 0.5-1.0 a / dm, a dense light gray precipitate of high purity metallic antimony precipitates.

Содержание примесей в полученном металлеThe content of impurities in the resulting metal

SU1136115A METHOD OF ELECTROLYSIS OF ANTIMONY FROM ORGANIC ELECTROLYTES SU208953A1 (en)