SU1556420A1 - Материал для анодов электролитических и оксидно-полупроводниковых конденсаторов - Google Patents

Материал для анодов электролитических и оксидно-полупроводниковых конденсаторов

Info

Publication number
SU1556420A1
SU1556420A1 SU4291031/21A SU4291031A SU1556420A1 SU 1556420 A1 SU1556420 A1 SU 1556420A1 SU 4291031/21 A SU4291031/21 A SU 4291031/21A SU 4291031 A SU4291031 A SU 4291031A SU 1556420 A1 SU1556420 A1 SU 1556420A1
Authority
SU
USSR - Soviet Union
Prior art keywords
reduced
anodes
niobium
specific charge
electrolytic
Prior art date
Application number
SU4291031/21A
Other languages
English (en)
Inventor
А.В. Елютин
Ю.Б. Патрикеев
Н.С. Воробьева
В.В. Ковалев
Т.Б. Касенов
А.С. Петухова
Original Assignee
Научно-исследовательский и проектный институт редкометаллической промышленности
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Научно-исследовательский и проектный институт редкометаллической промышленности filed Critical Научно-исследовательский и проектный институт редкометаллической промышленности
Priority to SU4291031/21A priority Critical patent/SU1556420A1/ru
Application granted granted Critical
Publication of SU1556420A1 publication Critical patent/SU1556420A1/ru

Abstract

Изобретение относится к порошковой металлургии и может быть использовано в производстве порошковых материалов для изготовления объемно-пористых анодов оксидно-полупроводниковых конденсаторов. Цель изобретения - повышение удельного заряда, уменьшение токов утечки и снижение материалоемкости конденсаторов. Материал содержит тантал или ниобий и дополнительно водород 0,1 - 1 мас. % . Получение материала включает предварительную дегазацию исходного слитка тантала или ниобия при температуре 500С и остаточном давлении 1,3 Па в течение 0,5 ч и гидрирование при давлении водорода 0.7·10Па при температуре 700 С в течение 2 ч, затем при температуре 400С в течение 12 ч с последующим охлаждением до 180С в течение 4 ч. После охлаждения до комнатной температуры полученный материал измельчают до дисперсности 0,1 - 100 мкм. Образцы анодов обеспечивают удельный заряд 16 - 30 мКл/г и токи утечки 1 - 7 мкА. 3 табл.
SU4291031/21A 1987-07-28 1987-07-28 Материал для анодов электролитических и оксидно-полупроводниковых конденсаторов SU1556420A1 (ru)

Priority Applications (1)

Application Number Priority Date Filing Date Title
SU4291031/21A SU1556420A1 (ru) 1987-07-28 1987-07-28 Материал для анодов электролитических и оксидно-полупроводниковых конденсаторов

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
SU4291031/21A SU1556420A1 (ru) 1987-07-28 1987-07-28 Материал для анодов электролитических и оксидно-полупроводниковых конденсаторов

Publications (1)

Publication Number Publication Date
SU1556420A1 true SU1556420A1 (ru) 1994-02-28

Family

ID=60527304

Family Applications (1)

Application Number Title Priority Date Filing Date
SU4291031/21A SU1556420A1 (ru) 1987-07-28 1987-07-28 Материал для анодов электролитических и оксидно-полупроводниковых конденсаторов

Country Status (1)

Country Link
SU (1) SU1556420A1 (ru)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US6702869B2 (en) 1999-05-12 2004-03-09 Cabot Corporation High capacitance niobium powders and electrolytic capacitor anodes

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US6702869B2 (en) 1999-05-12 2004-03-09 Cabot Corporation High capacitance niobium powders and electrolytic capacitor anodes

Similar Documents

Publication Publication Date Title
JPS526374A (en) Anode structure for electrolysis
GB1372294A (en) Electric accumulator
ES463922A1 (es) Un metodo para la fabricacion de una aleacion para uso en elalmacenamiento de hidrogeno.
GB765073A (en) Improvements in or relating to electric alkaline accumulators
DE60004108D1 (de) Herstellung von stickstoff enthaltendes tantal- oder niobiumpulver und festelektrolytkondensator
GB2147611A (en) Process for treating the surface of valve metals with chalcogens
GB1446693A (en) Hydrogen storage electrodes for galvanic cells
GB1467851A (en) Aluminium alloy foils for use in high-voltage electrolytic capacitors
GB925079A (en) Electrolysis of salt solutions
SU1556420A1 (ru) Материал для анодов электролитических и оксидно-полупроводниковых конденсаторов
GB951726A (en) Process for making anodes for electrolytic condensers
GB822250A (en) Porous electrodes for electric accumulators and a method for the production thereof
US2301390A (en) Primary cell
Danninger et al. Phosphorus embrittlement of tungsten heavy alloys
CN108165829A (zh) 一种钇-镁-钙-镍系ABn型储氢合金及其制备方法
GB1236739A (en) Improvements in a zinc electrode and method of forming
ES432149A1 (es) Procedimiento para la obtencion de briquetas de laton sinte-rizadas.
GB1133777A (en) Process for the preparation of finely divided, non-pyrophoric nitrides of zirconium, hafnium, niobium and tantalum
GB973810A (en) Improvements in and relating to the electrolytic production of hydrogen
SU416590A1 (ru)
SU1432946A1 (ru) Способ получения гидридных фаз, содержащих тантал
ES435889A1 (es) Procedimiento y dispositivo para la preparacion de persul- fatos de metales alcalinos por electrolisis.
GB1399195A (en) Copper base alloy
GB1151654A (en) Electrolytic Cells
FR2028157A1 (en) Preparation of solutions of hydroxylamine - salts from nitric oxide