SU1388269A1 - Intermittent abrasive wheel - Google Patents

Intermittent abrasive wheel Download PDF

Info

Publication number
SU1388269A1
SU1388269A1 SU853916411A SU3916411A SU1388269A1 SU 1388269 A1 SU1388269 A1 SU 1388269A1 SU 853916411 A SU853916411 A SU 853916411A SU 3916411 A SU3916411 A SU 3916411A SU 1388269 A1 SU1388269 A1 SU 1388269A1
Authority
SU
USSR - Soviet Union
Prior art keywords
protrusion
abrasive
circle
decrease
wheel
Prior art date
Application number
SU853916411A
Other languages
Russian (ru)
Inventor
Иван Михайлович Буюкли
Original Assignee
Одесский Политехнический Институт
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Одесский Политехнический Институт filed Critical Одесский Политехнический Институт
Priority to SU853916411A priority Critical patent/SU1388269A1/en
Application granted granted Critical
Publication of SU1388269A1 publication Critical patent/SU1388269A1/en

Abstract

Изобретение относитс  к механической обработке материалов св занным абразивом и позвол ет повысить производительность обработки и стойкость круга. Дл  этого в абразивном прерывистом круге, рабоча  поверхность которого выполнена в виде чередующихс  выступов и впадин, каждый выступ содержит элементы разной зернистости , последовательно убывающей (возрастающей) в окружном направлении . Такое выполнение выступа приводит к снижению диспергировани , что обусловливает снижение теплонапр жент ности в зоне обработки и дает возможность вести процесс шлифовани  на более интенсивных режимах обработ- ки либо увеличить отношение длины выступа к длине впадины. 1 ил.The invention relates to the machining of materials associated with abrasives and allows for improved processing performance and durability of the wheel. To do this, in an abrasive intermittent wheel, the working surface of which is made in the form of alternating protrusions and depressions, each protrusion contains elements of different grain sizes, successively decreasing (increasing) in the circumferential direction. Such an embodiment of the protrusion leads to a decrease in dispersion, which causes a decrease in the thermal stress in the treatment zone and makes it possible to carry out the grinding process on more intensive processing modes or to increase the ratio of the protrusion length to the depression length. 1 il.

Description

Изобретение относитс  к механической обработке материалов св занным абразивом (алмазом, эльбором .и др.) - к шлифованию.This invention relates to the machining of materials associated with abrasive (diamond, elbor, etc.) to grinding.

Целью изобретени   вл етс  повышение производительности обработки и стойкости круга.The aim of the invention is to increase the processing performance and durability of the wheel.

В предлагаемом круге, рабоча  поверхность которого выполнена в виде чередующихс  выступов и впадин, каждый выступ содержит элементы разной зернистости, последовательно убывающей (возрастающей) в окружном направлении .In the proposed circle, the working surface of which is made in the form of alternating protrusions and depressions, each protrusion contains elements of different grain sizes, successively decreasing (increasing) in the circumferential direction.

На чертеже представлена схема съема припуска выступом прерывистого круга, выполненного из крупнозернистых и мелкозернистых участков с убыванием зернистости в пределах выступа от тыльной части к фронтальной .The drawing shows the removal scheme allowance protrusion intermittent circle, made of coarse-grained and fine-grained areas with a decrease in grain size within the protrusion from the rear to the front.

На чертеже обозначены О - ось вращени  круга; GJ - углова  скорость вращени  круга; „рое продоль на  подача издели ; L - участок шлифуемой поверхности, сформированный одним выступом; К - круг; Д - изделие; МЗ - мелкозернистый участок выступа круга; КЗ - крупнозернистый участок выступа круга; 1 - 3 - режущие зерна крупнозернистого участка выступа круга; 4 - 8 - режущие зерна мелкозернистого участка выстельно большей части верхнего сло  припуска, а мелкозернистым участком - сравнительно тонкий слой с оконча- тельным формированием шероховатости поверхности. Работа последующих выс- тупов аналогичнаIn the figure, O is the axis of rotation of the circle; GJ is the angular velocity of rotation of the circle; „Make longitudinal feed of the product; L is the area of the ground surface formed by one protrusion; K is a circle; D - product; MH - fine-grained portion of the protrusion of the circle; KZ - coarse-grained portion of the circle protrusion; 1 - 3 - cutting grains of the coarse-grained portion of the protrusion of the circle; 4 - 8 - cutting grains of the fine-grained section of the uppermost part of the upper seam allowance, and the fine-grained section of the relatively thin layer with the final formation of surface roughness. The work of subsequent performances is similar.

Съем верхних слоев припуска крупнозернистыми участками выступов при- Removal of the upper layers of the allowance with coarse-grained areas of protrusions

10 водит к снижению работы диспергировани , что обуславливает снижение теплонапр женности в зоне обработки . Уменьшение теплонапр женности дает возможность вести процесс шли15 фовани  на более интенсивных режимах обработки, либо увеличить отношение длины выступа к длине впадины. Это повьш1ает производительность и снижает темп износа круга.10 leads to a reduction in the dispersion work, which causes a decrease in the thermal intensity in the treatment zone. Reducing the heat capacity makes it possible to carry out the process of skaning on more intensive processing modes, or to increase the ratio of the length of the protrusion to the length of the depression. This increases productivity and reduces wheel wear.

20Съем припуска, прилегающего к20Remove allowance adjacent to

окончательно формируемой поверхности мелкозернистыми участками выступов , улучшает шероховатость шлифуемой поверхности,finally formed surface with fine-grained areas of protrusions, improves the roughness of the ground surface,

.-25Таким образом, имеет место объеди . нение при двух различных зернистос- т х по длине выступа чернового и чистового шлифовани  в одноопераци- онное При трех зернистост х - в.-25So, there is a union. at two different granularities x along the length of the protrusion of rough and finish grinding into a single operation. At three granularities - in

30 один прием реализуетс  черновое, получистовое и чистовое птифование и т.д.30, one method is implemented for rough, semi-finishing and finishing stocking, etc.

Выбор количества участков с различной зернистостью и соотношение их длинThe choice of the number of areas with different grain sizes and the ratio of their lengths

тупа круга; R,, R, R,, R4 - радиусы 35 выступе может быть рассчитано поstupid circle; R ,, R, R ,, R4 - the radius 35 of the ledge can be calculated by

известным зависимост м, либо опреде- , лено экспериментально дл  конкретсоответственно траектории движени  зе- зерен 1,2 и 3 относительно издели ;known dependencies, or determined experimentally for a specific, respectively, trajectory of the grains 1,2 and 3 relative to the product;

траектории движени  зерен относительно оси вращени  круга; 1 , 2, 3the path of movement of the grains relative to the axis of rotation of the circle; 1, 2, 3

ных условий обработки.processing conditions.

Конструктивно выступ с участкамиStructurally protrusion with areas

4 - траектории движени  зерен 4-8 относительно издели ; R,.R4 - обусловлено  влением самооформлени  профил  выступа при прерывистом шлифовании .4 shows the trajectories of the movement of the grains 4-8 relative to the product; R, .R4 - due to the phenomenon of self-shaping profile of the protrusion with intermittent grinding.

При вращении круга зерна относительно детали перемещаютс  по трохо- идальным . Зерно 1 - по кривой 1 , зерно 2 - по кривой 2 , зерно 3 - по кривой 3 , зерна 4-8 - по кривым 4, Зерно 1 срезает спой металла, ограниченный кривой 1 , зерно 2 срезает- слой -метапла, ограниченньй кривыми 1 и 2 , зерно 3 срезает слой, ограниченный кривыми 2 и З и т.д. Из взаимного расположени  указанных кривых вродно, что крупнозернистом участком ,осуществл етс  съем значи40When the circle is rotated relative to the part, the grains move along the trochoidal. Grain 1 - on curve 1, grain 2 - on curve 2, grain 3 - on curve 3, grain 4-8 - on curves 4, Grain 1 cuts off the metal yield limited by curve 1, grain 2 cuts off - the layer is melted, limited by curves 1 and 2, grain 3 cuts a layer bounded by curves 2 and 3, etc. From the mutual arrangement of these curves, it is apparent that a coarse-grained area is eaten significant.

4545

различной зернистости может быть выполнен известными способами, например приклеиванием, либо механическим креплением к периферии диска секторов св занного абразива различной зернистости.Different grain sizes can be made by known methods, for example, by gluing or mechanically fixing the sectors of the associated abrasive of various grain sizes to the periphery of the disk.

ФормулаFormula

изобретени the invention

5050

5555

Абразивный прерывистый круг, периферийна  рабоча  поверхность которого выполнена в виде чередующихс  абразивных выступов и впадин, отличающий с  тем, что, с целью повьш1ени  производительности обработки и стойкости круга, каждый выступ выполнен с зернистостью абразива, последовательно убывающей (возрастающей ) в окружном направлении.Abrasive intermittent wheel, the peripheral working surface of which is made in the form of alternating abrasive protrusions and depressions, characterized in that, in order to increase processing performance and durability of the circle, each protrusion is made with abrasive grit, consistently decreasing (increasing) in the circumferential direction.

тельно большей части верхнего сло  припуска, а мелкозернистым участком - сравнительно тонкий слой с оконча- тельным формированием шероховатости поверхности. Работа последующих выс- тупов аналогичнаmost of the upper layer of the allowance, and the fine-grained section is a relatively thin layer with a final formation of surface roughness. The work of subsequent performances is similar.

Съем верхних слоев припуска крупнозернистыми участками выступов при- .Removal of the upper layers of the allowance with coarse-grained areas of the protrusions at-.

10 водит к снижению работы диспергировани , что обуславливает снижение теплонапр женности в зоне обработки . Уменьшение теплонапр женности дает возможность вести процесс шли15 фовани  на более интенсивных режимах обработки, либо увеличить отношение длины выступа к длине впадины. Это повьш1ает производительность и снижает темп износа круга.10 leads to a reduction in the dispersion work, which causes a decrease in the thermal intensity in the treatment zone. Reducing the heat capacity makes it possible to carry out the process of skaning on more intensive processing modes, or to increase the ratio of the length of the protrusion to the length of the depression. This increases productivity and reduces wheel wear.

20Съем припуска, прилегающего к20Remove allowance adjacent to

окончательно формируемой поверхности мелкозернистыми участками выступов , улучшает шероховатость шлифуемой поверхности,finally formed surface with fine-grained areas of protrusions, improves the roughness of the ground surface,

25Таким образом, имеет место объеди . нение при двух различных зернистос- т х по длине выступа чернового и чистового шлифовани  в одноопераци- онное При трех зернистост х - в25Thus, there is a union. at two different granularities x along the length of the protrusion of rough and finish grinding into a single operation. At three granularities - in

30 один прием реализуетс  черновое, получистовое и чистовое птифование и т.д.30, one method is implemented for rough, semi-finishing and finishing stocking, etc.

Выбор количества участков с различной зернистостью и соотношение их длинThe choice of the number of areas with different grain sizes and the ratio of their lengths

ных условий обработки.processing conditions.

Конструктивно выступ с участкамиStructurally protrusion with areas

различной зернистости может быть выполнен известными способами, например приклеиванием, либо механическим креплением к периферии диска секторов св занного абразива различной зернистости.Different grain sizes can be made by known methods, for example, by gluing or mechanically fixing the sectors of the associated abrasive of various grain sizes to the periphery of the disk.

ФормулаFormula

изобретени the invention

Абразивный прерывистый круг, периферийна  рабоча  поверхность которого выполнена в виде чередующихс  абразивных выступов и впадин, отличающий с  тем, что, с целью повьш1ени  производительности обработки и стойкости круга, каждый выступ выполнен с зернистостью абразива, последовательно убывающей (возрастающей ) в окружном направлении.Abrasive intermittent wheel, the peripheral working surface of which is made in the form of alternating abrasive protrusions and depressions, characterized in that, in order to increase processing performance and durability of the circle, each protrusion is made with abrasive grit, consistently decreasing (increasing) in the circumferential direction.

4four

Claims (1)

Формула изобретенияClaim Абразивный прерывистый круг, периферийная рабочая поверхность которого выполнена в виде чередующихся абразивных выступов и впадин, отличающий ся тем, что, с целью повышения производительности обработки и стойкости круга, каждый выступ выполнен с зернистостью абразива, последовательно убывающей (возрастающей) в окружном направлении.An abrasive intermittent circle, the peripheral working surface of which is made in the form of alternating abrasive protrusions and depressions, characterized in that, in order to increase processing productivity and durability of the circle, each protrusion is made with the abrasive grain gradually decreasing (increasing) in the circumferential direction.
SU853916411A 1985-06-26 1985-06-26 Intermittent abrasive wheel SU1388269A1 (en)