SU138299A1 - The method of surface treatment of electroluminescent powder - Google Patents

The method of surface treatment of electroluminescent powder

Info

Publication number
SU138299A1
SU138299A1 SU675689A SU675689A SU138299A1 SU 138299 A1 SU138299 A1 SU 138299A1 SU 675689 A SU675689 A SU 675689A SU 675689 A SU675689 A SU 675689A SU 138299 A1 SU138299 A1 SU 138299A1
Authority
SU
USSR - Soviet Union
Prior art keywords
surface treatment
powder
electroluminescent powder
solution
electroluminescent
Prior art date
Application number
SU675689A
Other languages
Russian (ru)
Inventor
И.А. Миронов
Original Assignee
И.А. Миронов
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by И.А. Миронов filed Critical И.А. Миронов
Priority to SU675689A priority Critical patent/SU138299A1/en
Application granted granted Critical
Publication of SU138299A1 publication Critical patent/SU138299A1/en

Description

Способ поверхностной обработки порошка электролгоминофора на основе сульфида цинка, активированного медью дл  удалени  внешнего сло  сульфида меди с частиц электролюминофора, известен .A method for the surface treatment of an electromhomophor powder based on zinc sulfide activated by copper to remove the outer layer of copper sulfide from electroluminophore particles is known.

Предложен сцособ поверхностной обработки порошка электролюминофора , с целью удалени  внешнего сло  сульфида меди с частиц электролюминофора, заключающийс  в обработке цорошка аммиачным раствором в присутствии окислител .A surface treatment method for the electroluminescent powder is proposed to remove the outer layer of copper sulphide from the electroluminescent particles, which consists in treating the powder with an ammonia solution in the presence of an oxidizing agent.

АммиаЧНый раствор содержит:Ammonium solution contains:

100 г/л NHs. 50 г/л СОз и оки1слитель (воздух, перекись водорода, персульфат аммони ).100 g / l NHs. 50 g / l CO2 and oxidant (air, hydrogen peroxide, ammonium persulfate).

Порошок электролюминофора загружаетс  в емкость и заливаетс  аммиачным раствором, который готовитс  из карбоната аммони  и аммиака.The electroluminescent powder is loaded into the container and poured with ammonia solution, which is prepared from ammonium carbonate and ammonia.

В раствор вводитс  также персульфат аммони  (из расчета 5% по весу), если он используетс  в качестве окислител .Ammonium persulfate (at the rate of 5% by weight) is also added to the solution if it is used as an oxidizing agent.

Соотношение порошка IH раствора должно быть 1:3:4 ио весу.The ratio of powder IH solution should be 1: 3: 4 and its weight.

Суспензи  электролюмино|фора в аммиачном растворе нагреваетс  при умеренном перемешиваииИ до 60°. этой температуре обработка идет 2-3 час, если прореагированный раствор периодически мен етс  на свежий через 20-30 мин. Если в качестве окислител  используетс  воздух, то процесс также ведетс  при 60°, причем необходимо обеспечить наилучшей контакт суспензии с продуваемым через нее воздухом.The suspension of the electroluminescence in an ammonia solution is heated with moderate stirring to 60 °. This temperature is treated for 2-3 hours if the reacted solution periodically changes to fresh after 20-30 minutes. If air is used as an oxidizing agent, the process is also carried out at 60 °, and it is necessary to ensure the best contact of the suspension with the air blown through it.

При смене раствора через 20-30 млн обработка продолжаетс  3 час.When changing the solution after 20-30 million, the treatment lasts 3 hours.

В этом случае в аммиачный раствор вводитс  тиосульфат натри  в количестве 5-10 г1л.In this case, sodium thiosulfate in an amount of 5-10 g1l is added to the ammonia solution.

При использовании в качестве окислител  перекиси водорода обработку можно вести при комнатной температуре. При этом переWhen used as an oxidizing agent for hydrogen peroxide, the treatment can be carried out at room temperature. At the same time

SU675689A 1960-08-02 1960-08-02 The method of surface treatment of electroluminescent powder SU138299A1 (en)