SU1222633A1 - Способ концентрировани щелочно-алюминатных растворов - Google Patents
Способ концентрировани щелочно-алюминатных растворов Download PDFInfo
- Publication number
- SU1222633A1 SU1222633A1 SU843788306A SU3788306A SU1222633A1 SU 1222633 A1 SU1222633 A1 SU 1222633A1 SU 843788306 A SU843788306 A SU 843788306A SU 3788306 A SU3788306 A SU 3788306A SU 1222633 A1 SU1222633 A1 SU 1222633A1
- Authority
- SU
- USSR - Soviet Union
- Prior art keywords
- aluminate solutions
- evaporation
- solutions
- alkali
- concentrating
- Prior art date
Description
«
Изобретение относитс к цветной металлургии и может быть использовано в производстве глинозема.
Цель изобретени - ускорение процесса.
Пример. Выпариванию подвергают 150 см маточного раствора содта ва, г/дм : (общ) 144,9; ) 126,4; (к.б) 18,5; «к 3,5 без добавок (контрольный опыт) и .с добавками кетона состава С. Выпаривание растворов ведут при 120 С в течение 100 мин.
Результаты опытов представлены в таблице.
В таблице прдставЛены опыты с кетовом , содержащим четыре атома углерода (С4), так как кетоны с содержанием 4-6 углеродных атомов (с 4, С 5 и С) одинаково действуют на скорость выпаривани щелочно-алюми-: натных растворов. Кетон, содержащий семь атомов углерода, не может быть использован в качестве добавки, так
Редактор Н.Гунько
Составитель Н.Целикова
Техред Л.Олейник Корректор А.Зимокосов
1665У22 Тираж 450Подписное
ВНИИПИ Государственного комитета СССР
по делам изобретений и открытий 113а35, Москва, Ж-35, Раушска наб„, д. 4/5
Филиал ППП Патент, г.Ужгород, ул.Проектна , 4
226332
как он плохо растворим в щелочно-алю- минатном растворе.
Из таблицы следует, что выпаривание щелочно-алюминатного раствора с
5 добавками кетона состава С в количестве 0,005-0,1 г/дм идет интенсивнее по сравнению с контрольным опытом на 5,4-12,1%. При уменьшении концентрации указанной добавки до
10 0,001 г/дм не наблюдаетс заметного ускорени выпаривани раствора. С увеличением концентрации добавки ке- ,тона состава С выше 0,1 г/дм процесс выпаривани ускор етс не на .
15 много, но при этом резко возрастают затраты на реагент. Вследствие применени дорогосто щего материала удорожаетс процесс.
По известному способу скорость вы20 паривани составл ет по Ка20(к) 0,063-0,085 г/дм , мин.
Предлагаемьй способ позвол ет увеличить скорость выпаривани щелочно- алюминатньгх рс1створов на 5,4-12,1%.
Claims (2)
1. СПОСОБ КОНЦЕНТРИРОВАНИЯ ЩЕЛОЧНО-АЛЮМИНАТНЫХ РАСТВОРОВ, включающий выпаривание их с органической добавкой, отличающийся тем, что, с целью ускорения процесса, в качестве органической добавки используют предельные кетоны С.НЯО-С6Н140.
2. Способ по п. 1, отличающийся тем, что кетоны вводят в количестве 0,005-0,1 г/дм3.
ί