carbon atoms
flotation
hydrocarbon radical
formula
compound
Prior art date
Application number
SU731984184A
Other languages
Russian (ru)
Inventor
Шуберт Хайнрих
Раатц Винфрид
Мозер Герхард
Бохния Дитер
Балдауф Хорст
Original Assignee
Феб Бергбау Унд Хюттенкомбинат "Альберт Функ" Фрайберг (Инопредприятие)
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Феб Бергбау Унд Хюттенкомбинат "Альберт Функ" Фрайберг (Инопредприятие) filed Critical Феб Бергбау Унд Хюттенкомбинат "Альберт Функ" Фрайберг (Инопредприятие)
Application granted granted Critical
Publication of SU1034782A1 publication Critical patent/SU1034782A1/en

Links

Classifications

    • BPERFORMING OPERATIONS; TRANSPORTING
    • B03SEPARATION OF SOLID MATERIALS USING LIQUIDS OR USING PNEUMATIC TABLES OR JIGS; MAGNETIC OR ELECTROSTATIC SEPARATION OF SOLID MATERIALS FROM SOLID MATERIALS OR FLUIDS; SEPARATION BY HIGH-VOLTAGE ELECTRIC FIELDS
    • B03DFLOTATION; DIFFERENTIAL SEDIMENTATION
    • B03D1/00Flotation
    • B03D1/001Flotation agents
    • B03D1/004Organic compounds
    • B03D1/008Organic compounds containing oxygen
    • BPERFORMING OPERATIONS; TRANSPORTING
    • B03SEPARATION OF SOLID MATERIALS USING LIQUIDS OR USING PNEUMATIC TABLES OR JIGS; MAGNETIC OR ELECTROSTATIC SEPARATION OF SOLID MATERIALS FROM SOLID MATERIALS OR FLUIDS; SEPARATION BY HIGH-VOLTAGE ELECTRIC FIELDS
    • B03DFLOTATION; DIFFERENTIAL SEDIMENTATION
    • B03D2201/00Specified effects produced by the flotation agents
    • B03D2201/02Collectors
    • BPERFORMING OPERATIONS; TRANSPORTING
    • B03SEPARATION OF SOLID MATERIALS USING LIQUIDS OR USING PNEUMATIC TABLES OR JIGS; MAGNETIC OR ELECTROSTATIC SEPARATION OF SOLID MATERIALS FROM SOLID MATERIALS OR FLUIDS; SEPARATION BY HIGH-VOLTAGE ELECTRIC FIELDS
    • B03DFLOTATION; DIFFERENTIAL SEDIMENTATION
    • B03D2203/00Specified materials treated by the flotation agents; Specified applications
    • B03D2203/02Ores
    • B03D2203/04Non-sulfide ores

Landscapes

  • Manufacture And Refinement Of Metals (AREA)
  • Lubricants (AREA)

Abstract

1414039 Froth flotation BERGBAU-UND HUTTENKOMBINAT ALBERT FUNK VEB 21 Dec 1973 [27 Dec 1972] 59420/73 Heading B2H In a process for the flotation of tin ores there is used as a collector a compound of the formula: in which c n is a hydrocarbon radical containing 3 carbon atoms, at least one of the hydrogen atoms of which has been replaced by a substituent with a negative induction effect, R is an aliphatic hydrocarbon radical containing at least 2 carbon atoms, and M represents a hydrogen ion or an alkali metal cation; and/or a compound of the formula: in which A represents 1, 2, 3 or 4 substituents with a negative induction effect and R' is an aliphatic hydrocarbon radical; and/or a compound of the formula in which C m is a hydrocarbon radical, C k and C 1 are hydrocarbon radicals with k and l= 0, 1, 2 or 3 carbon atoms; and R 1 , R 2 , and R 3 represent hydrogen or hydrocarbon radicals. Suitable substituents having a negative induction effect are F, Cl, Br, I, COO-, OH and COOM. The flotation process is preferably carried out at a pH of 2 to 8 in the presence of foaming non-ionic polar and/or non-polar additives e.g. alcohols, and/or of oils and/or of suppressants e.g. sodium hexafluorosilicate, waterglass or starch. Examples describe the use of α-bromohexadecanoic acid, the sodium salt of tridecane-1, 3-carboxylic acid, and the sodium salt of α, α-undecane-dicarboxylic acid as collectors.

Description

Изобретение относитс  к обогащен оловосодержащих руд, особенно касси теритовых, методом флотации. Известны способы флотации кассит рита в кислЬй или щелочной средах при рН 2-9 с использованием модификаторов , вспенивателей и в качестве собирателей алкилсульфатов, монокар боновых кислот и их мыл и другие ре агенты ClJ. В практике флотации наиболее шир ко исполвзуют.монокарбоновые кислот и их мыла. Однако способы, использующие ука занные собиратели, не обеспечивают достижени  удовлетворительных показателей флотации, что обусловлено следующим. Растворимость в воде алифатических монокарбоновых кислот в змачительной степени зависит от температуры пульпы. Растворимость кислот содержащих более 10 атомов углерода а составе, углеводородной цепи, при комнатной температуре невелика . Она существенно уменьшаетс  по мере увеличени  длины цепи. Констан ты диссоциации упом нутых монокарбоновых кислот, особенно пригодных дл  флотации вследствие длины их углеводородной цепи, наход тс  в области значений, меньших 10 . Поэтому они не используютс  в среде, у .которой рН меньше 5, а это. особенно неблагопри тно дл  флотации касс., так как он лучше всего флотируетс  с применением анионоактивных флотоагентов в области кислых сред. Кроме того, анионы насыщенных и ненасыщенных алифатических монокарбоноаых кислот реагируют с много валентными катионами, растворимыми в флотационной системе, образу  при этом осаждающиес  нерастворимые продукты. За счет этого из состава флотационной системы выводитс  эффективно действующий флотоагент, ввиду чего расход реагента возрастает . Избирательность алифатических монокарбоновых кислот можно улучшать за счет добавлени  модифицирующих реактивов, что приводит к увеличению удельных затрат на тонну РУДЫ. Целью изобретени   вл етс  разработка способа флотации касситерита , основанного на применении относительно дешевых реагентов, позвол ющих повысить извлечение олова в концентрат. Поставленна  цель достигаетс  тем, что согласно способу обогащени  оловосодержащих руд, заключающемус  в измельчении руды, обработке пульпы модификатором, вспе-. нивателем и собирателем и флотации касситерита в кислой или щелочной среде при рН 2-8, осуществл ют с выведением в процесс в качестве собирател  замещенных карбоновых кислот или их солей с карбоксильными группами в положении от 0 до 7с отрйцате.пьным J-эффекте формулы . R-R-COOH ( соон) : . /-;; где R - насыщенна  или ненасыщенна  : . алифатическа  или аромати- . чёска  углеводородна  группа с числом атомов углерода t R - алифатическа  углеводородна  группа с числом атомов углерода 1-3 или циклопарафинова  углеводородна  группа с числом углерода , или . ароматическа  углеводородна  группа; М - катион щелочного металла или водород;. m-l-i. Преимущество указанных реагентов собирателей , заключаетс  в том, что применение определенных заместителей улучшает растворимость реагента в воде, константу диссоциации И избирательность действи  при ф/ютации. За счет этих факторов уменьшаетс  образование продуктов осажде и  в процессе флотации, а также снижаетс  образование мицел и димеризаци . Предлагаемый способ осуществл ют следующим образом. . Руду измельчают, обесшламливают, создают определенную плотность пульпы . Затем ввод т модификатор, достигают требуемой величины рН пульпы, ввод т собиратель и вспениватель. В()едение ка1кдого реагента сопровождаетс  кондиционированием в течение оптимального дл  данного реагента времени. .Затем ос: ществл ют флотацию касситерита. Пример. Испытывают следую щие реагенты: ТридикандиС ILCU-сн кар.боновв  кислота(-1,3) и ее Соль ЛентадекандйyU f а соон карбонрва  кислотд(-1j3) Ундекандйкар СООН С Н rCHj брнова  - СООН слота(-1,1) Пентадекёндй: .СООН карбрноаай С,Н СН - соон кйслота(-1,1) Нонадекандикарг соон С Н-СНбонова  кислоч л- соон ,1) сбои Пентадекантрикдрбойова  ки- . ( слота(-1,) 82 4 и другие в сравнении с действием известных собирателей: стиролфосфо ,новой и толуолфосфоновой. флотируют руду с содержанием олова 0,30-0,35 обесшламливают по классу 20 мкм. Плотность пульпы 25%) рН среды переменное. Вспениватель: ксиленол или октандиол. Расход известного собирател  200§00 ч/т, предлагаемого 50-100-г/г. Осуществление предложенного способа обеспечивает увеличение олова в концентрат по меньшей мере на 10%.; Таким образом, данное изобретем ние обеспечивает повышение технологических показателей обогащени  оловосодержащих руд.This invention relates to a tin-rich ore, especially cassterite ores, by flotation. There are known methods for flotation of cassitic ritol in acidic or alkaline media at pH 2–9 using modifiers, blowing agents and as collectors of alkyl sulfates, monocarboxylic acids and their soaps, and other ClJ reagents. In flotation practice, the most widely used monocarboxylic acids and their soaps are. However, methods using these collectors do not achieve satisfactory flotation rates, due to the following. The solubility of aliphatic monocarboxylic acids in water depends on the temperature of the pulp. The solubility of acids containing more than 10 carbon atoms and the composition of the hydrocarbon chain, at room temperature is small. It decreases significantly as the chain length increases. The dissociation constants of said monocarboxylic acids, especially suitable for flotation due to the length of their hydrocarbon chain, are in the range of values less than 10. Therefore, they are not used in an environment where pH is less than 5 and that. It is particularly unfavorable for flotation of cascade plants, since it is best flotation using anionic flotation agents in the field of acidic media. In addition, the anions of saturated and unsaturated aliphatic monocarboxylic acids react with the multivalent cations soluble in the flotation system, thus forming precipitated insoluble products. Due to this, an effective flotation agent is removed from the composition of the flotation system, as a result of which the consumption of the reagent increases. The selectivity of aliphatic monocarboxylic acids can be improved by adding modifying reagents, which leads to an increase in unit costs per ton of ore. The aim of the invention is to develop a method for flotation of cassiterite, based on the use of relatively cheap reagents, which make it possible to increase the recovery of tin in the concentrate. This goal is achieved by the fact that according to the method of enrichment of tin-containing ores, which consists in grinding ore, processing the pulp with a modifier, extracting it. nastomer and collector and flotation of cassiterite in an acidic or alkaline medium at pH 2-8, carried out with the removal in the process as a collector of substituted carboxylic acids or their salts with carboxyl groups in the position from 0 to 7c. The J-effect of the formula. R-R-COOH (soon):. / - ;; where R is saturated or unsaturated:. aliphatic or aromatic. A hydrocarbon group with the number of carbon atoms t R is an aliphatic hydrocarbon group with 1–3 carbon atoms or a cycloparaffin hydrocarbon group with a carbon number, or. aromatic hydrocarbon group; M - alkali metal cation or hydrogen ;. m-l-i. The advantage of these collector reagents is that the use of certain substituents improves the solubility of the reagent in water, the dissociation constant, and the selectivity of action during f / yation. Due to these factors, the formation of products precipitated and during the flotation process is reduced, and the formation of micelles and dimerization is also reduced. The proposed method is carried out as follows. . Ore is crushed, desliming, create a certain density of pulp. Then the modifier is introduced, the required pH value of the pulp is reached, the collector and the blowing agent are introduced. In (), the consumption of each reagent is followed by conditioning for an optimum time for the reagent. Then os: there is a flotation of cassiterite. Example. The following reagents are tested: TridicandIs ILCU-ct.carboxylic acid (-1.3) and its salt Lentadecine yf a soon carbonate acid (-1j3) UndecedicCOOL C H rCHj brnova - COOH slots (-1,1) Pentadeconde:. COOH Carrno-Aay C, H CH - Soon Acid (-1.1) Nonadecanicarg Soon C H-CHonbone Acidic L-Soon, 1) Failures of Pentadecantricdrboyova ki-. (slots (-1,) 82 4 and others in comparison with the action of well-known collectors: styrenolphospho, new and toluolophosphonic. Float ore with a tin content of 0.30-0.35 is saliated according to the class of 20 microns. The pulp density is 25%) pH is variable . Foaming agent: xylenol or octanediol. Consumption of the famous collector 200§00 p / t, the proposed 50-100-g / g. The implementation of the proposed method provides an increase in tin concentrate at least 10% .; Thus, this invention provides an increase in the technological indicators of the enrichment of tin-containing ores.

Claims (1)

СПОСОБ ОБОГАЩЕНИЯ 0ЛО80С0ДЕРЖАЩИХ РУД, заключающийся в обработке пульпы модификатором, вспенивателем и оксигидрильным собирателем и флотации касситерита в кислой или щелочной среде при рН2-8, ‘от л и ч а ющийс я тем, что* ·. с целью повышения извлечения олова в конденсат, в качестве собирателя в пульпу вводят замещенные карбоновые кислоты или их соли с карбоксильными группами в положении от ’ до^г* с отрицательным 1-эффектом формулы R-R’-COOM (С00М) где R - насыщенная или ненасыщенная алифатическая или ароматичес*^ кая углеводородная группа с числом'атомов углеродаMETHOD FOR ENRICHMENT OF 0L80C0-CONTAINING ORES, which consists in treating the pulp with a modifier, blowing agent and oxyhydryl collector and flotation of cassiterite in an acidic or alkaline medium at pH2-8, which is based on the fact that * ·. in order to increase the extraction of tin into the condensate, substituted carboxylic acids or their salts with carboxyl groups in the position from 'to ^ g * with a negative 1-effect of the formula R-R'-COOM (С00М) No. are introduced into the pulp as a collector, where R - saturated or unsaturated aliphatic or aromatic * hydrocarbon group with the number of carbon atoms I 1-25;I 1-25; R - алифатическая углеводородная группа с числом атомов углерода 1-3 или циклопарафиновая углеводородная группа с числом атомов углерода 3-6, или ароматическая углеводородная группа;R is an aliphatic hydrocarbon group with the number of carbon atoms 1-3 or a cycloparaffin hydrocarbon group with the number of carbon atoms 3-6, or an aromatic hydrocarbon group; М - катион щелочного металла или водорода;M is an alkali metal or hydrogen cation; т®1-4.t®1-4. δδζιεοΓ^Τϊδ*0 >δδζιεοΓ ^ Τϊδ * 0 > 1 1034782 . 11 1034782. 1
SU731984184A 1972-12-27 1973-12-26 Stannum containing ore concentration method SU1034782A1 (en)

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
DD167886A DD108217A1 (en) 1972-12-27 1972-12-27

Publications (1)

Publication Number Publication Date
SU1034782A1 true SU1034782A1 (en) 1983-08-15

Family

ID=5489536

Family Applications (1)

Application Number Title Priority Date Filing Date
SU731984184A SU1034782A1 (en) 1972-12-27 1973-12-26 Stannum containing ore concentration method

Country Status (4)

Country Link
CS (1) CS209189B1 (en)
DD (1) DD108217A1 (en)
GB (1) GB1414039A (en)
SU (1) SU1034782A1 (en)

Families Citing this family (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
WO2011085445A1 (en) * 2010-01-14 2011-07-21 Teebee Holdings Pty Ltd Flotation reagents
CN113385305A (en) * 2021-08-03 2021-09-14 广东省科学院资源利用与稀土开发研究所 Halogenated benzohydroxamic acid collecting agent and application thereof in mineral flotation

Also Published As

Publication number Publication date
DD108217A1 (en) 1974-09-12
CS209189B1 (en) 1981-11-30
GB1414039A (en) 1975-11-12

Similar Documents

Publication Publication Date Title
GB478134A (en) A process for removing salts from solutions
US4061568A (en) Method for recovering and stabilizing fat and fatty substances as well as proteins and proteinous substances from process water
SU1034782A1 (en) Stannum containing ore concentration method
US1618105A (en) Process of manufacturing aluminum hydroxide
US3974069A (en) Process for the dehydration of fatty sludge and the recovery of chemicals
US2112298A (en) Metallurgical cyanide process
US2131938A (en) Process for the refining of naphthenic acids
JPS5839894B2 (en) Method for removing phosphorus and silicon from water-soluble smelting slag
SU982362A1 (en) Method of extracting molybdenum
US2358619A (en) Method for reconditioning used solutizer solutions
SU1677075A1 (en) Method of processing solutions containing non-ferrous metals
US1773787A (en) Art of concentration of ores
US2703646A (en) Beneficiation of potash ores and the like
US2976310A (en) Multiple step continuous contacting of immiscible substances
SU1310341A1 (en) Method for flotation extraction of nonferrous metal ions from diluted aqueous solutions
US1572944A (en) Process of softening water
SU944666A1 (en) Depressor for flotation of ores with carbonate enclosing rock
SU956022A1 (en) Method of concentrating carbonate-siliceous phosporite ores
US1771550A (en) Reagent for use in concentration of ores
SU61717A1 (en) The method of separation of compounds of thallium and germanium from solutions of their salts
SU1132981A1 (en) Method of enriching clay potassium-containing ores
SU1477693A1 (en) Water softening method
SU1399364A1 (en) Method of processing solutions containing non-ferrous metals
US3002810A (en) Method for producing sodium borates of lowered iron content
US2087264A (en) Process of clarifying water in connection with softening