SE8302488L - REAR WELDING PROCEDURE WITH NON-MELTING ELECTROD IN GAS GAS MOSPHOSES - Google Patents

REAR WELDING PROCEDURE WITH NON-MELTING ELECTROD IN GAS GAS MOSPHOSES

Info

Publication number
SE8302488L
SE8302488L SE8302488A SE8302488A SE8302488L SE 8302488 L SE8302488 L SE 8302488L SE 8302488 A SE8302488 A SE 8302488A SE 8302488 A SE8302488 A SE 8302488A SE 8302488 L SE8302488 L SE 8302488L
Authority
SE
Sweden
Prior art keywords
pass
gas
arc
per unit
energy
Prior art date
Application number
SE8302488A
Other languages
Unknown language ( )
Swedish (sv)
Other versions
SE461198B (en
SE8302488D0 (en
Inventor
Jury Semenovich Ischenko
Vladislav Vasilievich Roschin
Viktor Alexandrovich Bukarov
Vladimir Alexandrovic Khavanov
Nina Alexeevna Frolova
Original Assignee
Jury Semenovich Ischenko
Vladislav Vasilievich Roschin
Bukarov Viktor A
Vladimir Alexandrovic Khavanov
Nina Alexeevna Frolova
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Jury Semenovich Ischenko, Vladislav Vasilievich Roschin, Bukarov Viktor A, Vladimir Alexandrovic Khavanov, Nina Alexeevna Frolova filed Critical Jury Semenovich Ischenko
Publication of SE8302488D0 publication Critical patent/SE8302488D0/en
Publication of SE8302488L publication Critical patent/SE8302488L/en
Publication of SE461198B publication Critical patent/SE461198B/en

Abstract

The inert gas arc welding process employing a non-consumable electrode consists of the following steps. Before the welding process the edges (5, 6) of a butt joint (1) are machined to produce a truncated surface (7) and the electrode is lowered the whole depth (h) of the weld seam. The truncated surface (7) is then melted over the whole thickness ( delta o) in the first pass and a weld root (8) of the first layer (9) is formed. With each successive pass the energy of the arc (4) per unit length is changed relative to the preceding pass. When a depth of h SIMILAR (0.3 to 0.4) delta of the weld seam is reached and its width is B SIMILAR (1.0 to 1.3)h, the electrode (2) is removed from the region of the weld seam and is arranged above the surface of the butt joint (1) in the region of the joint (3). Furthermore, the energy of the arc (4) per unit length is discontinuously raised compared to the preceding pass and the edges (5b, 6b) of the butt joint (1) are completely melted, with the formation of a layer (13) on the surface of the joint, whereupon the energy of the arc (4) per unit length is changed from pass to pass. <IMAGE>
SE8302488A 1982-09-28 1983-05-02 PROCEDURE WELDING IN A MULTIPLE CIRCUIT WITH DIFFERENT WELDING ENERGY BETWEEN THE CURVES SE461198B (en)

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
SU3387687 1982-09-28

Publications (3)

Publication Number Publication Date
SE8302488D0 SE8302488D0 (en) 1983-05-02
SE8302488L true SE8302488L (en) 1984-03-29
SE461198B SE461198B (en) 1990-01-22

Family

ID=20994385

Family Applications (1)

Application Number Title Priority Date Filing Date
SE8302488A SE461198B (en) 1982-09-28 1983-05-02 PROCEDURE WELDING IN A MULTIPLE CIRCUIT WITH DIFFERENT WELDING ENERGY BETWEEN THE CURVES

Country Status (4)

Country Link
CS (1) CS235162B1 (en)
DD (1) DD230812A1 (en)
DE (1) DE3328204C2 (en)
SE (1) SE461198B (en)

Families Citing this family (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
DE10306863B3 (en) * 2003-02-19 2004-07-15 Daimlerchrysler Ag Edge joint arc welding method e.g. for component half shells of automobile foot pedal, has at least one of welded parts formed with spacer around its edge prior to welding

Family Cites Families (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
US3494019A (en) * 1964-05-29 1970-02-10 Yawata Seitetsu Kk Process for butt welding of irons and steels
SU518292A1 (en) * 1972-03-27 1976-06-25 Предприятие П/Я М-5729 Method of arc fusion welding
SU740429A1 (en) * 1976-06-10 1980-06-15 За витель Multipass welding method

Also Published As

Publication number Publication date
DD230812A1 (en) 1985-12-11
DE3328204C2 (en) 1986-12-18
SE461198B (en) 1990-01-22
DE3328204A1 (en) 1984-03-29
CS235162B1 (en) 1985-05-15
SE8302488D0 (en) 1983-05-02

Similar Documents

Publication Publication Date Title
DE3775234D1 (en) METHOD FOR APPLYING A WELDED SEAM ON A THIN PART OF A SUBSTRATE.
ES481106A1 (en) Method of welding metal parts.
SE8302488D0 (en) REAR WELDING PROCEDURE WITH NON-MELTING ELECTROD IN GAS GAS MOSPHOSES
JPH06114587A (en) Butt welding method for thick plates
JPS63112088A (en) Laser beam machining method
JPS61293691A (en) Welding method by laser
JPS5794473A (en) Arc spot welding method
JPS5633192A (en) Welding process for copper and copper alloy
JPS61266185A (en) Double electrode mig welding method
JPS5519444A (en) Welding method of low temperature steel
JPS5564983A (en) Foil seam welding device
JPS57156876A (en) High speed butt welding method of thin material
JPS55117583A (en) High energy density beam welding method
JPS64218A (en) Remelt treating method for metal surface
Simonik et al. Submerged Nonconsumable Electrode Welding With Regulation of the Welding Current
JPS551953A (en) Arc welding method
JPS54150342A (en) Circular arc welding method
JP2534853B2 (en) High-speed Tig dressing method
JPS61253181A (en) Tic arc welding method for repairing
JPS54148158A (en) Plasma arc build up process
JPS53127346A (en) High speed submerged arc welding method for groove
JPS574389A (en) Welding method for aluminum material
JPS5736076A (en) Three o&#39;clock butt gas shielded arc welding method for al or al alloy
JPS5890382A (en) Submerged arc welding method with low heat input
Costley Butt Welding Process

Legal Events

Date Code Title Description
NUG Patent has lapsed

Ref document number: 8302488-5

Effective date: 19921204