RU96106566A - METHOD OF MODIFICATION OF WOOD - Google Patents

METHOD OF MODIFICATION OF WOOD

Info

Publication number
RU96106566A
RU96106566A RU96106566/04A RU96106566A RU96106566A RU 96106566 A RU96106566 A RU 96106566A RU 96106566/04 A RU96106566/04 A RU 96106566/04A RU 96106566 A RU96106566 A RU 96106566A RU 96106566 A RU96106566 A RU 96106566A
Authority
RU
Russia
Prior art keywords
preforms
modifier
compaction
impregnation
melt
Prior art date
Application number
RU96106566/04A
Other languages
Russian (ru)
Other versions
RU2103163C1 (en
Inventor
Ф.Ф. Данилов
А.Н. Захаров
М.А. Изотов
В.Д. Харламов
Original Assignee
Ф.Ф. Данилов
А.Н. Захаров
М.А. Изотов
В.Д. Харламов
Filing date
Publication date
Application filed by Ф.Ф. Данилов, А.Н. Захаров, М.А. Изотов, В.Д. Харламов filed Critical Ф.Ф. Данилов
Priority to RU96106566A priority Critical patent/RU2103163C1/en
Priority claimed from RU96106566A external-priority patent/RU2103163C1/en
Application granted granted Critical
Publication of RU2103163C1 publication Critical patent/RU2103163C1/en
Publication of RU96106566A publication Critical patent/RU96106566A/en

Links

Claims (2)

1. Способ модификации древесины, включающий сушку и пропитку заготовок путем выдерживания их в расплаве модификатора и последующего охлаждения в расплаве модификатора, а также уплотнение заготовок, отличающийся тем, что уплотнение заготовок осуществляют перед сушкой и пропиткой, сушку и пропитку уплотненных заготовок осуществляют при размещении их в матричных обоймах, при этом заготовки выдерживают при температуре расплава модификатора 100 - 155oC в течение 4 - 8 ч и охлаждают при температуре расплава не менее, чем на 25oC ниже первоначальной температуры расплава модификатора в течение 1,5 - 2 ч.1. A method of modifying wood, including drying and impregnation of preforms by keeping them in the melt of the modifier and subsequent cooling in the melt of the modifier, as well as compaction of the preforms, characterized in that the compaction of the preforms is carried out before drying and impregnation, drying and impregnation of the compacted preforms is carried out when placing them in matrix clips, while the workpieces are kept at a melt temperature of the modifier of 100 - 155 o C for 4 to 8 hours and cooled at a melt temperature of not less than 25 o C below the original the melt temperature of the modifier for 1.5 to 2 hours 2. Способ по п.1, отличающийся тем, что уплотнение заготовок осуществляют путем их обжатия поперек волокон до степени обжатия 1,7 - 2,5. 2. The method according to claim 1, characterized in that the compaction of the preforms is carried out by crimping them across the fibers to a compression ratio of 1.7 - 2.5.
RU96106566A 1996-03-28 1996-03-28 Method of wood modification RU2103163C1 (en)