RU93005821A - Способ защиты от коррозии и налипания - Google Patents
Способ защиты от коррозии и налипанияInfo
- Publication number
- RU93005821A RU93005821A RU93005821/02A RU93005821A RU93005821A RU 93005821 A RU93005821 A RU 93005821A RU 93005821/02 A RU93005821/02 A RU 93005821/02A RU 93005821 A RU93005821 A RU 93005821A RU 93005821 A RU93005821 A RU 93005821A
- Authority
- RU
- Russia
- Prior art keywords
- copper
- fouling
- alloy
- protection against
- against corrosion
- Prior art date
Links
- 238000005260 corrosion Methods 0.000 title claims 3
- 239000010949 copper Substances 0.000 claims 4
- 229910052802 copper Inorganic materials 0.000 claims 4
- RYGMFSIKBFXOCR-UHFFFAOYSA-N copper Chemical compound [Cu] RYGMFSIKBFXOCR-UHFFFAOYSA-N 0.000 claims 3
- 229910000881 Cu alloy Inorganic materials 0.000 claims 2
- 229910001069 Ti alloy Inorganic materials 0.000 claims 2
- 230000003373 anti-fouling Effects 0.000 claims 2
- 239000011248 coating agent Substances 0.000 claims 2
- 238000000576 coating method Methods 0.000 claims 2
- 230000000694 effects Effects 0.000 claims 2
- 239000000654 additive Substances 0.000 claims 1
- 230000002265 prevention Effects 0.000 claims 1
- RTAQQCXQSZGOHL-UHFFFAOYSA-N titanium Chemical compound [Ti] RTAQQCXQSZGOHL-UHFFFAOYSA-N 0.000 claims 1
- 239000010936 titanium Substances 0.000 claims 1
- 229910052719 titanium Inorganic materials 0.000 claims 1
Claims (1)
- Предлагается способ защиты от коррозии и обрастания объектов морской техники путем нанесения противокоррозионных и противообрастающих покрытий. В способе подводную часть объектов изготавливают из триметалла сталь-титановый сплав - медь (или медный сплав), состоящего из нанесенного беспористого титанового слоя толщиной не менее 1 мм, покрытия из меди (или медного сплава) с объемной пористостью от 0,5 до 20%. Для изменения разности потенциалов титановый сплав - покрытие на основе меди в пределах от 80 до 230 мВ в медь вводят 1 - 30% катодных добавок и(или) 0,5 - 15% анодных. Технический результат - обеспечение практически неограниченного срока службы защиты, предотвращение механических повреждений, эффективная регулируемая защита от обрастания в морских бассейнах с различной биологической активностью.