RU2615938C1 - Сплав на основе магния - Google Patents
Сплав на основе магния Download PDFInfo
- Publication number
- RU2615938C1 RU2615938C1 RU2016124011A RU2016124011A RU2615938C1 RU 2615938 C1 RU2615938 C1 RU 2615938C1 RU 2016124011 A RU2016124011 A RU 2016124011A RU 2016124011 A RU2016124011 A RU 2016124011A RU 2615938 C1 RU2615938 C1 RU 2615938C1
- Authority
- RU
- Russia
- Prior art keywords
- magnesium
- alloy
- titanium
- silver
- zinc
- Prior art date
Abstract
Изобретение относится к области цветной металлургии, в частности к составам сплавов на основе магния, которые могут быть использованы для изготовления корпусов приборов и инструментов. Сплав на основе магния содержит, мас.%: цинк 1,6-1,8; титан 0,1-0,2; бор 0,06-0,08; алюминий 2,4-2,8; серебро 0,6-0,9; магний - остальное. Сплав характеризуется повышенной прочностью. 1 табл.
Description
Изобретение относится к области цветной металлургии, в частности к составам сплавов на основе магния, которые могут быть использованы для изготовления корпусов приборов и инструментов.
Известен сплав на основе магния, мас.%: цинк 1,8-2,5; неодим 0,8-1,2; цирконий 0,7-1,0; титан 0,1-0,2; магний - остальное [1].
Задачей изобретения является повышение прочности сплава.
Технический результат достигается тем, что сплав на основе магния, содержащий цинк, титан, дополнительно включает бор, алюминий и серебро, причем компоненты находятся при следующем соотношении, мас.%: цинк 1,6-1,8; титан 0,1-0,2; бор 0,06-0,08; алюминий 2,4-2,8; серебро 0,6-0,9; магний - остальное.
В таблице приведены составы сплава на основе магния.
Повышение прочности сплава на основе магния достигается комплексным влиянием компонентов, входящих в его состав. Цинк, алюминий и серебро повышают прочность сплава, титан и бор способствуют измельчению его структурных составляющих.
Сплав выплавляют под флюсом ВИ2 (флюс содержит, мас.%: MgCl2 40,0-48,0; KCl 30,0-40,0; BaCl2 5,0; CaF2 3,0-5,0) в стационарных толстостенных стальных тиглях. После рафинирования и модифицирования расплав отстаивают в течение 10-15 мин при температуре 700-720°С и разливают по металлическим формам (при заливке форм струю металла припудривают молотой серой для предотвращения загорания).
Источник информации
1. SU 1678881, С22С 23/04, 1991.
Claims (1)
- Сплав на основе магния, содержащий цинк и титан, отличающийся тем, что он дополнительно включает бор, алюминий и серебро, причем компоненты находятся при следующем соотношении, мас.%: цинк 1,6-1,8; титан 0,1-0,2; бор 0,06-0,08; алюминий 2,4-2,8; серебро 0,6-0,9; магний - остальное.