RU2318761C1 - Raw mix - Google Patents
Raw mix Download PDFInfo
- Publication number
- RU2318761C1 RU2318761C1 RU2006136612/03A RU2006136612A RU2318761C1 RU 2318761 C1 RU2318761 C1 RU 2318761C1 RU 2006136612/03 A RU2006136612/03 A RU 2006136612/03A RU 2006136612 A RU2006136612 A RU 2006136612A RU 2318761 C1 RU2318761 C1 RU 2318761C1
- Authority
- RU
- Russia
- Prior art keywords
- alumina
- production
- neutralization
- product
- lime milk
- Prior art date
Abstract
Description
Изобретение относится к составам сырьевых смесей, используемых в производстве глиноземистого цемента.The invention relates to compositions of raw mixtures used in the production of alumina cement.
Известны различные глиноземистые цементы, получаемые из сырьевых смесей, состоящих из глинозема и известняков [1].There are various alumina cements obtained from raw mixtures consisting of alumina and limestone [1].
Известна сырьевая смесь следующего состава: продукт нейтрализации известковым молоком сточных вод производства диатидбензола 40-50%; технический глинозем 50-60 [2]. Прочность цемента, полученного с применением такой сырьевой смеси, при сжатии составляет 23-54 кгс/см2.Known raw mix of the following composition: the product of the neutralization of lime milk waste water production of diatidbenzene 40-50%; industrial alumina 50-60 [2]. The strength of cement obtained using such a raw material mixture under compression is 23-54 kgf / cm 2 .
Цель изобретения состоит в повышении прочности цемента, полученного с применением сырьевой смеси.The purpose of the invention is to increase the strength of cement obtained using a raw mix.
Цель достигается тем, что в состав сырьевой смеси, содержащей продукт нейтрализации известковым молоком сточных вод производства диэтилбензола и технический глинозем, дополнительно вводят сернокислый глинозем, при следующем соотношении компонентов, мас.%: продукт нейтрализации известковым молоком сточных вод производства диэтилбензола 40-42; технический глинозем 56-57; сернокислый глинозем 2-3. Соотношение продукта нейтрализации известковым, молоком сточных вод производства диэтилбензола и технического глинозема равно 3:4.The goal is achieved by the fact that in the composition of the raw material mixture containing the product of neutralization with lime milk waste water production of diethylbenzene and technical alumina, additionally introduced sulfate alumina, in the following ratio of components, wt.%: Product neutralization of lime milk waste water production of diethylbenzene 40-42; technical alumina 56-57; alumina sulfate 2-3. The ratio of the product of neutralization with lime, milk, wastewater from the production of diethylbenzene and industrial alumina is 3: 4.
В таблице приведены составы сырьевой смеси.The table shows the composition of the raw mix.
Источники информацииInformation sources
1. Попов К.Н. Материаловедение для каменщиков, монтажников конструкций. - М.: Высш. шк., 1991, С.89-90.1. Popov K.N. Materials science for masons, installers of structures. - M .: Higher. school., 1991, S. 89-90.
2. Авторское свидетельство СССР №1557120, C04B 7/32, 1990.2. Copyright certificate of the USSR No. 1557120, C04B 7/32, 1990.
Claims (2)