RU2012156714A - METHOD FOR PRODUCING MODIFIED POLYVINYL CHLORIDE - Google Patents

METHOD FOR PRODUCING MODIFIED POLYVINYL CHLORIDE Download PDF

Info

Publication number
RU2012156714A
RU2012156714A RU2012156714/04A RU2012156714A RU2012156714A RU 2012156714 A RU2012156714 A RU 2012156714A RU 2012156714/04 A RU2012156714/04 A RU 2012156714/04A RU 2012156714 A RU2012156714 A RU 2012156714A RU 2012156714 A RU2012156714 A RU 2012156714A
Authority
RU
Russia
Prior art keywords
polyvinyl chloride
amount
reaction mass
modified polyvinyl
total reaction
Prior art date
Application number
RU2012156714/04A
Other languages
Russian (ru)
Other versions
RU2538201C2 (en
Inventor
Андрей Сергеевич Дринберг
Александр Александрович Слесарев
Original Assignee
Общество с ограниченной ответственностью "Делтекс"
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Общество с ограниченной ответственностью "Делтекс" filed Critical Общество с ограниченной ответственностью "Делтекс"
Priority to RU2012156714/04A priority Critical patent/RU2538201C2/en
Publication of RU2012156714A publication Critical patent/RU2012156714A/en
Application granted granted Critical
Publication of RU2538201C2 publication Critical patent/RU2538201C2/en

Abstract

1. Способ получения модифицированного поливинилхлорида, включающий смешение в емкостном реакторе сополимера поливинилхлорида и растворителя, и нагрев смеси до 50-60°C, отличающийся тем, что в реакционную смесь вводят винилированный алкид.2. Способ по п.1, отличающийся тем, что количество сополимера поливинилхлорида составляет 20-25 мч от общей реакционной массы.3. Способ по п.1, отличающийся тем, что количество винилированного алкида составляет 6-10 мч от общей реакционной массы.4. Способ по п.1, отличающийся тем, что в качестве растворителя используют толуол в количестве 70-75 мч от общей реакционной массы.1. A method of obtaining a modified polyvinyl chloride, comprising mixing a copolymer of polyvinyl chloride and a solvent in a capacitive reactor, and heating the mixture to 50-60 ° C, characterized in that a vinylated alkyd is introduced into the reaction mixture. 2. The method according to claim 1, characterized in that the amount of the polyvinyl chloride copolymer is 20-25 mph of the total reaction mass. The method according to claim 1, characterized in that the amount of vinylated alkyd is 6-10 mh of the total reaction mass. The method according to claim 1, characterized in that toluene is used as a solvent in an amount of 70-75 mh of the total reaction mass.

Claims (4)

1. Способ получения модифицированного поливинилхлорида, включающий смешение в емкостном реакторе сополимера поливинилхлорида и растворителя, и нагрев смеси до 50-60°C, отличающийся тем, что в реакционную смесь вводят винилированный алкид.1. A method of obtaining a modified polyvinyl chloride, comprising mixing in a capacitive reactor a copolymer of polyvinyl chloride and a solvent, and heating the mixture to 50-60 ° C, characterized in that a vinylated alkyd is introduced into the reaction mixture. 2. Способ по п.1, отличающийся тем, что количество сополимера поливинилхлорида составляет 20-25 мч от общей реакционной массы.2. The method according to claim 1, characterized in that the amount of the polyvinyl chloride copolymer is 20-25 mph of the total reaction mass. 3. Способ по п.1, отличающийся тем, что количество винилированного алкида составляет 6-10 мч от общей реакционной массы.3. The method according to claim 1, characterized in that the amount of vinylated alkyd is 6-10 mh of the total reaction mass. 4. Способ по п.1, отличающийся тем, что в качестве растворителя используют толуол в количестве 70-75 мч от общей реакционной массы. 4. The method according to claim 1, characterized in that the solvent used is toluene in an amount of 70-75 mh from the total reaction mass.
RU2012156714/04A 2012-12-26 2012-12-26 Method of obtaining modified polyvinylchloride RU2538201C2 (en)