PL654B1 - The method of rolling smooth and shaped solid bars and wires. - Google Patents

The method of rolling smooth and shaped solid bars and wires. Download PDF

Info

Publication number
PL654B1
PL654B1 PL654A PL65421A PL654B1 PL 654 B1 PL654 B1 PL 654B1 PL 654 A PL654 A PL 654A PL 65421 A PL65421 A PL 65421A PL 654 B1 PL654 B1 PL 654B1
Authority
PL
Poland
Prior art keywords
wires
shaped solid
solid bars
cross
section
Prior art date
Application number
PL654A
Other languages
Polish (pl)
Filing date
Publication date
Application filed filed Critical
Publication of PL654B1 publication Critical patent/PL654B1/en

Description

Wynalazek dotyczy sposobu walcowa¬ nia gladkich lub ksztaltowych pretów pel¬ nych lub drutów, przy którym trzy lub cztery walce z glówkami kulistemi tworza zamkniety w sobie kaliber. Wynalazek dazy do tego, zeby zmniejszyc znacznie przekrój drutu przy jednem przepuszcze¬ niu, przyczem zmniejszenie przekroju wy¬ nosi 60 i wiecej %, niz w walcach zwy¬ klych, wobec czego — praktycznie — wal¬ cuje sie w jednym przebiegu produkt wstepny na drut ostateczny, np. odrazu z 5 mm na 2 mm srednicy. Dotychczas nie- znano w walcowaniu drutu tak wielkiego zmniejszenia przekroju w jednym prze¬ biegu, naogól dotychczas przyjmowano jako regule, ze nie mozna zmniejszyc prze¬ kroju w jednym przebiegu wiecej, niz o 25%, przekroju pierwotnego. Azeby.; wiec prze walcowac drut 5 mm srednicy na dwumilimetrowy, nalezaloby przeciagnac go najmniej 5 razy. Prowadzi to do kali¬ brów slabych, praktycznie niewykonal¬ nych, a slaby materjal nie wytrzymuje go¬ raca. Z tej przyczyny zwykle nie walco¬ wano poza 5 mm, tylko zwezano drut da¬ lej przez przeciaganie na zimno. Przyczy¬ na lezy w tern, ze w zwyklej walcarce z górnym i dolnym walcem dziala cisnienie na przeciagniety drut, tylko z dwóch stron, wywolujac poza pozadanem przedluze¬ niem takze rozszerzenie przekroju równo¬ legle do osi walców. Poniewaz kaliber jest zamkniety tylko w plaszczyznie, przecho¬ dzacej przez osie walców, natomiast jest o- twarty w czesciach, polozonych równole¬ gle do tej plaszczyzny w strone wejscia, istniala moznosc tworzenia'sie zadziorów, i azeby zadziory nie byly zbyt wielkie, na¬ lezalo ograniczyc zmniejszenie przekroju w zakresie, podanym powyzej.Wynalazek polega na spostrzezeniu, zejezeli cisnienie walcowe dziala pod wply¬ wem znanych przyrzadów wiecej, niz z dwóch stron w kierunku osi drutu, i jezeli stosuje sie kaliber zamkniety nietylko w plaszczyznie osiowej czyli prawdziwy lej, mozna osiagnac praktycznie dowolne zmniejszenie przekroju.Na rysunku uwidoczniono fig. 1 i 2, jako przyklad wykonania, urzadzenie odpo¬ wiednie do przeprowadzenia sposobu.Na fig. 1 wskazano z trzech glówek ku¬ listych (a, b, c) utworzony zamkniety ka¬ liber. Przez ruch wahadlowy tam i zpo- wrotem, lub obrót glówek kulistych wo¬ kolo osi (d, e, i), wszystkich w jednym kierunku, zostaje materjal skrawedziowa- ny i dodatkowo przeciagniety, czyli wal¬ cowany, poczem opuszcza narzedzie w przekroju, utworzonym przez powierzch¬ nie glówek kulistych w plaszczyznie ich osi. Przez odpowiednia budowe takich cze¬ sci skladowych leja mozna otrzymac róz¬ nego ksztaltu przekroje, nawet druty o przekroju róznego ksztaltu, na ich dlugo¬ sci stale sie powtarzajacego.Na fig. 2 wskazano wykonanie narze¬ dzia, skladajacego sie z szesciu czesci ku¬ listych (A, B, C, D, E, F). PL PLThe invention relates to a process for rolling smooth or shaped solid bars or wires in which three or four spherical head rolls form an enclosed caliber. The invention strives to significantly reduce the cross-section of the wire with one pass, since the cross-section reduction is 60% or more than in conventional rolls, so that the wire is practically rolled in one pass. final, e.g. immediately from 5 mm by 2 mm in diameter. Hitherto, in wire rolling, such a large reduction of the cross-section in one pass has not been known, and it has been generally accepted as a rule that the cross-section cannot be reduced by more than 25% of the original cross-section in one pass. To.; So if you roll a 5mm wire into 2mm, you would have to pull it at least 5 times. This leads to weak, practically unworkable calibers and the poor material does not withstand fever. For this reason, usually no more than 5 mm was rolled, only the wire was tapped further by cold drawing. The reason for this is that in a conventional rolling mill with upper and lower rolls, pressure is exerted on the drawn wire only from two sides, causing, apart from the desired extension, also an expansion of the cross-section parallel to the axis of the rolls. As the caliber is closed only in the plane passing through the axes of the rollers, but is open in the portions parallel to this plane towards the entrance, it was possible to create burrs and lest the burrs were too large for The invention consists in the observation that the cylindrical pressure acts by known instruments on more than two sides in the direction of the wire axis, and if the caliber is closed not only in the axial plane, i.e. a real funnel , practically any reduction of the cross-section can be achieved. Figures 1 and 2 are shown as an exemplary embodiment, an apparatus suitable for carrying out the method. Figure 1 shows a closed box formed from three spherical heads (a, b, c) ¬ liber. By swinging back and forth, or the rotation of the spherical heads around the axis (d, e, i), all in one direction, the material is cut and additionally stretched, i.e. rolled, and then it leaves the tool in cross-section, formed by the surfaces of the spherical heads in the plane of their axis. By appropriate construction of such funnel components, it is possible to obtain cross-sections of various shapes, even wires of a different cross-section, constantly repeating their length. Fig. 2 shows the design of a tool consisting of six parts leaves (A, B, C, D, E, F). PL PL

Claims (1)

1. Zastrzezenie patentowe. Sposób walcowania gladkich lub ksztal¬ towych pretów pelnych lub drutów, w któ¬ rym trzy walce lub wiecej tworza zamkniety kaliber, tern znamienny, ze wytwarza sie w jednem przejsciu bardzo silne zmniejszenie przekroju, znacznie wieksze o 60% i wiecej, niz w walcach zwyklych. Carl Alexis Achterfeldt. Zastepca: Cz. Raczynski, rzecznik patentowy.Do opisu patentowego Na 654. m MKLGRA'r'.K:/!!,\NSi ..' .VABS2ft*ifc PL PL1. Patent claim. A method of rolling smooth or shaped solid bars or wires in which three or more rolls form a closed caliber, characterized by the fact that in one pass a very strong reduction in cross-section is produced, significantly greater by 60% and more than in ordinary rolls. . Carl Alexis Achterfeldt. Deputy: Vol. Raczynski, patent attorney. To the patent description Na 654. m MKLGRA'r'.K: / !!, \ NSi .. '. VABS2ft * ifc PL PL
PL654A 1921-03-30 The method of rolling smooth and shaped solid bars and wires. PL654B1 (en)