PL6014B1 - I, Michael Aktiengesellschaft fur chemische und metallurgische Industrie (Berlin, Germany \ Deodorizing agent for tanning. - Google Patents

I, Michael Aktiengesellschaft fur chemische und metallurgische Industrie (Berlin, Germany \ Deodorizing agent for tanning. Download PDF

Info

Publication number
PL6014B1
PL6014B1 PL6014A PL601426A PL6014B1 PL 6014 B1 PL6014 B1 PL 6014B1 PL 6014 A PL6014 A PL 6014A PL 601426 A PL601426 A PL 601426A PL 6014 B1 PL6014 B1 PL 6014B1
Authority
PL
Poland
Prior art keywords
tanning
industrie
berlin
michael
germany
Prior art date
Application number
PL6014A
Other languages
Polish (pl)
Filing date
Publication date
Application filed filed Critical
Publication of PL6014B1 publication Critical patent/PL6014B1/en

Description

J'ici wszciistwo: 13 stycznia 1925 r. (Niemw).Przy wyrobie sztucznego jedwabiu wo- dorosiarczek sodowy jako srodek denitry- fikuijacy dotychczas byl bardzo malo sto¬ sowany, (poniewaz do powyzszych celów wymiajgany jesit produkt nadzwyczajnie czy¬ sty, i z tego powodu do wyrobu nitrojedwa- biu nie stosuje sie lugów wodcrosiarczku sodowego, które otrzymuje ;sie jako odpad¬ ki w innych galeziach przemyslu.Zaiuwlazonloi, ze lugiJ wioldJcrosiarczku so¬ dowego, otrzymane w dinzych ilosciach jako produkty uboczne w rozmaitych procesach przemyslowych, nadaja sie jako srodek od¬ wlaszajacy przy garbowaniu, przyczem o- kazalo isie, ze za sitoscwanie wodoroisiarcz- ku sodowego, zmieszanego z wapnem, jest daleko korzystniejsze w porównaniu do u- zywanego dotychczas wylacznie wapna- siarcziku- sodowego wzglednie wapnicy ar¬ senu. Skóra waipnicwana zapomoca wodo- rosiarczku sodowego i wapna, daje skóre, która lepiej tworzy liczka i lepiej sie chwy¬ ta, niz produkt, otrzymany zapomoca siarcz¬ ku 'sodowego lub wapnicy arsenu. Surówki, otrzymane ze skór zapomoca wapnic wapna i wodorcsiairiczku sodowego, sa zinaicznie jasniejsze od otrzymanych zapomoca siarczku sodowego i wapna, co prawdopo¬ dobnie pochodzi stad, ze techniczny lug wodoroisiarezku sodowego nie zawiera ze¬ laza, czem rózni sie od technicznego siarcz¬ ku sodowego, zawierajacego zawsze pewne ilosci siarczku zelaza;. Obecnosc zelaza na¬ daje surówkom kolor ciemniejiszy i wywo-s luje niepozadane plamy, pochodzace od zelaza. Dalej skóry przy zastosowaniu wapnie woidorosiarcziku sodowego i wapna nie pecznieja tak bardzo, jak przy uzyciu zwyklej wapnicy siarczku sodowego, co jest bardzo wazne dla licznych rodzajów skór.Znane juz jieisit ziaisltosjowladte miaisici liufb kremu, skladaijacego siie z wapna gaszone¬ go (ilasowanogo) i z rozczynu wodorosiarcz- ku sodowego 5—8° Be, odpowiadajacego zawiartosci 6—9° Be wodorosiarczku sodo¬ wego, do usuwania pierza i sieirsci przy wy¬ robie sztucznych futer i t d., przyczetn na- kllaid^a isSe piciwyizislza imaisc na miiaizdine totdinio- snych skórek. Sposób ten nadaje sie tylko przy Kaisfosioiw)a|n!:b isitezoneigo wodo.ro- siiairczlkiu isodtowtegto, i jak -dlotajd roiie byilo wiia- domem, ze lug wodorosiarczku sodowego, silnie rozcienczony, zmieszany z wapnem, wywoluje nietylko zupelne odwilaszanie skór, lecz -dziala tez tak ochraniajaco na skóre, ze ostatecznie otrzymuje sie skóre, która odnosnie do tworzenia liczek jesit lepsza i lepiej sie chwyta, niz skóra, otrzy¬ mana zapomoca siarczku sodowego.Przyklad: 10 czesci wapna gasi sie wo¬ da i dodaje lug wodorosiarczku sodowego, odpowiadajacy 0,25 czesciom wodoro¬ siarczku sodowego. Calosc napelnia sie do 1000 czesci i zastosowurje mase otrzymana w ten sposób do wapnienia, zaleznie od skór, które iriaja byc wapnitome. Taikawapni¬ ca riaidiaijle isie inp. bardlzo dio loidwllaisizaniia slkór cfe!Lecy)ch i kroiwicih. EHa skór, które trudniej sie odwlaszaja, jak np. dla kipsów lub skór bawolichl podnosi sie ilosc wodo¬ rosiarczku rodowego podwójnie lub potrój¬ nie. Dla skór losiowych uprzezowych, u których rozchodzi sie o silne oddzialywa¬ nie i bardzo szybkie odwlaszanie, podnosi sie ilosc wodorosiarczku sodowego jeszcze wiecej, az do mniej wiecej 5,5 g na litr.Trwlatniiie odwilaisiziaoilai iziailezy od matury iskót, od zfaistosowameij iilicsfci sredków cdWla- szaijacycih, od itelmlpeaiaftury ciecizy wapien¬ nej, od rodzaju ruchu skór, i trwa od 6 do kilkudziesieciu godzin. PL PLJ'ici ubiquity: January 13, 1925 (German). In the production of rayon, sodium sulphide as a denitrifying agent has so far been very little used (because for the above purposes the product is extremely clean, and therefore Because of this, the production of nitro bisulfide is not used for the production of sodium hydrosulphide, which is obtained as waste in other branches of industry. The accumulation of a long sodium dihydrosulphide, obtained in large amounts as by-products in various industrial processes, is suitable as A deodorant for tanning, it has been shown that screening sodium hydrogen sulphide mixed with lime is far more advantageous compared to the previously used only sodium sulphide lime or arsenic lime. sodium hydrosulphide and lime give a skin which forms better and grips better than the product obtained with sulphide. arsenic calcification. Pig iron obtained from the skins with lime lime and sodium hydride are zinically lighter than those obtained with sodium sulphide and lime, which is probably due to the fact that the technical slurry of sodium hydroxide does not contain iron, which is different from technical sodium sulphide always containing a certain amount of iron sulfide; The presence of iron gives the pig iron a darker color and causes undesirable iron stains. Moreover, the leather does not swell as much with the use of sodium sulphide lime and lime, as with the use of ordinary sodium sulphide lime, which is very important for many types of leather. The already well-known crème liufb of lime and slaked lime is already known. of a sodium bisulfide solution of 5-8 ° Be, corresponding to a content of 6-9 ° Be of sodium bisulfide, for the removal of feathers and whistles in the manufacture of faux fur, and so on, and is also piciwizislza imaisc on miiaizdine totdinio - dream skins. This method is only suitable for Kaisfosioiv) a | n!: Bisitezoneigo of water, siiairczlkiu and sodium water, and how - the intake of the swarm was known that the slug of sodium hydrosulphide, strongly diluted, mixed with lime, causes not only complete dehydration of skin but - it also protects the skin so that the final result is a skin which, with regard to the formation of counters, is better and grips better than the skin obtained with sodium sulphide. Example: 10 parts of lime are quenched with water and added lye sodium bisulfide, corresponding to 0.25 parts of sodium bisulfide. The whole is filled up to 1000 parts and the mixture obtained in this way is used for calcification, depending on the hides that are iridescent to lime. Taikawapnica riaidiaijle isie inp. bardlzo dio loidwllaisizaniia slkór cfe! Lecy) ch i kroiwicih. For skins that are more difficult to dehash, such as, for example, for kips or buffalo skins, the amount of rhodium hydrosulphide is doubled or tripled. For harness moose skins, which are characterized by a strong influence and very rapid dehumidification, the amount of sodium bisulfide is increased even more, up to approximately 5.5 g per liter. The dehumidification takes longer, and the difference between the spell exam, - shaijacycih, from itelmlpeaaphthura of limestone chaff, from the type of skin movement, and lasts from 6 to several dozen hours. PL PL

Claims (1)

1. Zastrzezenie patentowe. Srodek odwlaszaijacy do garbowania, znamienny tem, ze sklada sie z rozczynu wodorosiarczku sodowego, polaczonego z wapnem, o zawartosci wodorosiarczku so¬ dowego ponizej 1%. I. Micha el Aktiengesellsch af t fur chemische und me t al 1 urg is c h e Industrie. Zastepca: M. Zoch, rzecznik patentowy. Druk L. Boguslawskiego, Warszawa. PL PL1. Patent claim. A tanning deodorizing agent, characterized in that it consists of a sodium bisulfide solution combined with lime, with a sodium bisulfide content of less than 1%. I. Micha el Aktiengesellsch af t fur chemische und me t al 1 urg is c h e Industrie. Deputy: M. Zoch, patent attorney. Printed by L. Boguslawski, Warsaw. PL PL
PL6014A 1926-01-04 I, Michael Aktiengesellschaft fur chemische und metallurgische Industrie (Berlin, Germany \ Deodorizing agent for tanning. PL6014B1 (en)