NO934529D0 - Beskyttelse av metalloverflater mot korrosjon - Google Patents
Beskyttelse av metalloverflater mot korrosjonInfo
- Publication number
- NO934529D0 NO934529D0 NO934529D NO934529D NO934529D0 NO 934529 D0 NO934529 D0 NO 934529D0 NO 934529 D NO934529 D NO 934529D NO 934529 D NO934529 D NO 934529D NO 934529 D0 NO934529 D0 NO 934529D0
- Authority
- NO
- Norway
- Prior art keywords
- protection
- metal surfaces
- against corrosion
- surfaces against
- corrosion
- Prior art date
Links
Classifications
-
- B—PERFORMING OPERATIONS; TRANSPORTING
- B63—SHIPS OR OTHER WATERBORNE VESSELS; RELATED EQUIPMENT
- B63B—SHIPS OR OTHER WATERBORNE VESSELS; EQUIPMENT FOR SHIPPING
- B63B59/00—Hull protection specially adapted for vessels; Cleaning devices specially adapted for vessels
- B63B59/04—Preventing hull fouling
-
- C—CHEMISTRY; METALLURGY
- C23—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; CHEMICAL SURFACE TREATMENT; DIFFUSION TREATMENT OF METALLIC MATERIAL; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION IN GENERAL
- C23C—COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL
- C23C4/00—Coating by spraying the coating material in the molten state, e.g. by flame, plasma or electric discharge
- C23C4/02—Pretreatment of the material to be coated, e.g. for coating on selected surface areas
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y10—TECHNICAL SUBJECTS COVERED BY FORMER USPC
- Y10T—TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION
- Y10T428/00—Stock material or miscellaneous articles
- Y10T428/24—Structurally defined web or sheet [e.g., overall dimension, etc.]
- Y10T428/24802—Discontinuous or differential coating, impregnation or bond [e.g., artwork, printing, retouched photograph, etc.]
- Y10T428/24917—Discontinuous or differential coating, impregnation or bond [e.g., artwork, printing, retouched photograph, etc.] including metal layer
-
- Y—GENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y10—TECHNICAL SUBJECTS COVERED BY FORMER USPC
- Y10T—TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION
- Y10T428/00—Stock material or miscellaneous articles
- Y10T428/24—Structurally defined web or sheet [e.g., overall dimension, etc.]
- Y10T428/24802—Discontinuous or differential coating, impregnation or bond [e.g., artwork, printing, retouched photograph, etc.]
- Y10T428/24926—Discontinuous or differential coating, impregnation or bond [e.g., artwork, printing, retouched photograph, etc.] including ceramic, glass, porcelain or quartz layer
Landscapes
- Chemical & Material Sciences (AREA)
- Engineering & Computer Science (AREA)
- Mechanical Engineering (AREA)
- Plasma & Fusion (AREA)
- Ocean & Marine Engineering (AREA)
- Physics & Mathematics (AREA)
- Combustion & Propulsion (AREA)
- Chemical Kinetics & Catalysis (AREA)
- Materials Engineering (AREA)
- Metallurgy (AREA)
- Organic Chemistry (AREA)
- Coating By Spraying Or Casting (AREA)
- Other Surface Treatments For Metallic Materials (AREA)
- Catching Or Destruction (AREA)
Applications Claiming Priority (2)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
GB919112499A GB9112499D0 (en) | 1991-06-11 | 1991-06-11 | Improved corrosion protection of marine structures |
PCT/GB1992/001052 WO1992022676A1 (en) | 1991-06-11 | 1992-06-11 | Protection of metal surfaces against corrosion |
Publications (1)
Publication Number | Publication Date |
---|---|
NO934529D0 true NO934529D0 (no) | 1993-12-10 |
Family
ID=10696431
Family Applications (2)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
NO934529A NO934529L (no) | 1991-06-11 | 1993-12-10 | Beskyttelse av metalloverflater mot korrosjon |
NO934529D NO934529D0 (no) | 1991-06-11 | 1993-12-10 | Beskyttelse av metalloverflater mot korrosjon |
Family Applications Before (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
NO934529A NO934529L (no) | 1991-06-11 | 1993-12-10 | Beskyttelse av metalloverflater mot korrosjon |
Country Status (8)
Country | Link |
---|---|
US (1) | US5516586A (no) |
EP (1) | EP0587709B1 (no) |
JP (1) | JPH07502071A (no) |
CA (1) | CA2111004A1 (no) |
DE (1) | DE69219773T2 (no) |
GB (1) | GB9112499D0 (no) |
NO (2) | NO934529L (no) |
WO (1) | WO1992022676A1 (no) |
Families Citing this family (18)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
ZA948161B (en) * | 1993-10-18 | 1995-05-25 | Dale Graham Hobson | Sealing of cylinder heads |
US6063212A (en) * | 1998-05-12 | 2000-05-16 | United Technologies Corporation | Heat treated, spray formed superalloy articles and method of making the same |
US6177201B1 (en) | 1998-06-17 | 2001-01-23 | A. O. Smith Corporation | Porcelain enamel coating for high-carbon steel |
US6308765B1 (en) | 1998-11-04 | 2001-10-30 | Grigoriy Grinberg | Method of making tools having a core die and a cavity die |
US6257309B1 (en) | 1998-11-04 | 2001-07-10 | Ford Global Technologies, Inc. | Method of spray forming readily weldable and machinable metal deposits |
US6155330A (en) * | 1998-11-04 | 2000-12-05 | Visteon Global Technologies, Inc. | Method of spray forming metal deposits using a metallic spray forming pattern |
JP3468739B2 (ja) * | 1999-12-27 | 2003-11-17 | 新東ブレーター株式会社 | 高耐食性かつ対カーボン低接触抵抗性金属の燃料電池用セパレーターへの付着方法 |
US6365222B1 (en) | 2000-10-27 | 2002-04-02 | Siemens Westinghouse Power Corporation | Abradable coating applied with cold spray technique |
US6491208B2 (en) | 2000-12-05 | 2002-12-10 | Siemens Westinghouse Power Corporation | Cold spray repair process |
US6444259B1 (en) | 2001-01-30 | 2002-09-03 | Siemens Westinghouse Power Corporation | Thermal barrier coating applied with cold spray technique |
DE10333165A1 (de) * | 2003-07-22 | 2005-02-24 | Daimlerchrysler Ag | Pressgehärtetes Bauteil und Verfahren zur Herstellung eines pressgehärteten Bauteils |
DE102004050474A1 (de) * | 2004-10-16 | 2006-04-20 | Mtu Aero Engines Gmbh | Verfahren zur Herstellung eines mit einer Verschleißschutzbeschichtung beschichteten Bauteils |
DE102005030266A1 (de) * | 2005-06-29 | 2007-01-18 | Mtu Aero Engines Gmbh | Schaufel einer Turbomaschine mit einer Schaufelspitzenpanzerung |
US8113025B2 (en) * | 2007-09-10 | 2012-02-14 | Tapphorn Ralph M | Technique and process for controlling material properties during impact consolidation of powders |
US20110104991A1 (en) * | 2008-03-12 | 2011-05-05 | Enbio Limited | Nozzle configurations for abrasive blasting |
US8065898B2 (en) * | 2008-07-29 | 2011-11-29 | Hamilton Sundstrand Corporation | Method and article for improved adhesion of fatigue-prone components |
DE102009033620A1 (de) * | 2009-07-17 | 2011-01-20 | Mtu Aero Engines Gmbh | Kaltgasspritzen von oxydhaltigen Schutzschichten |
US9675999B1 (en) | 2014-05-15 | 2017-06-13 | Glasslined Technologies, Inc. | Facile chemically-resistant coatings |
Family Cites Families (16)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
GB585879A (en) * | 1944-07-24 | 1947-02-27 | American Cyanamid Co | Improvements in the repair of enamel and glass-lined chemical equipment |
US3475141A (en) * | 1966-12-07 | 1969-10-28 | Robertson Co H H | Porcelain-enamel on galvanized steels by means of an aluminum coat |
US3482951A (en) * | 1967-07-19 | 1969-12-09 | Robertson Co H H | Porcelain enameled aluminum articles |
US3754976A (en) * | 1971-12-06 | 1973-08-28 | Nasa | Peen plating |
US3956028A (en) * | 1972-09-25 | 1976-05-11 | United States Steel Corporation | Temporary scale retardant coatings |
FR2236017A1 (en) * | 1973-07-02 | 1975-01-31 | Commissariat Energie Atomique | Protecting steel against corrosive gas - esp fluorine arising from uranium hexafluoride |
DE2420927A1 (de) * | 1974-04-26 | 1975-10-30 | Mannesmann Ag | Schutzanordnung gegen den schaedlichen bewuchs von durch schutzmittel gegen korrosion geschuetzten unterwasser-stahlbauteilen |
US4309485A (en) * | 1981-02-24 | 1982-01-05 | Ngk Spark Plug Co., Ltd. | Enameled steel plate |
GB2111861B (en) * | 1981-12-22 | 1985-05-01 | Armourcote Surface Treatments | Improvements in methods of coating surfaces to render them abrasion resistant |
US4552784A (en) * | 1984-03-19 | 1985-11-12 | The United States Of America As Represented By The United States National Aeronautics And Space Administration | Method of coating a substrate with a rapidly solidified metal |
US4689271A (en) * | 1984-08-11 | 1987-08-25 | Bayer Aktiengesellschaft | Coating for metallic substrates |
DE3443290C1 (de) * | 1984-11-28 | 1986-02-27 | Schwelm Anlagen & Apparate GmbH, 5830 Schwelm | Verfahren zur Herstellung einer korrosionsfesten Emailbeschichtung hoher elektrischer Isolationsfestigkeit |
DE3536040C1 (de) * | 1985-10-09 | 1987-05-27 | Roland Schnetteler | Verfahren zur beidseitigen Beschichtung von Baendern mit Emailschichten |
US4740388A (en) * | 1986-11-19 | 1988-04-26 | Mikio Nakashima | Painting method by spraying glassy material |
US4959330A (en) * | 1989-06-20 | 1990-09-25 | E. I. Du Pont De Nemours And Company | Crystallizable glass and thick film compositions thereof |
US5037670A (en) * | 1989-11-01 | 1991-08-06 | Cts Corporation | Method of manufacturing a low sheet resistance article |
-
1991
- 1991-06-11 GB GB919112499A patent/GB9112499D0/en active Pending
-
1992
- 1992-06-11 JP JP4511315A patent/JPH07502071A/ja active Pending
- 1992-06-11 DE DE69219773T patent/DE69219773T2/de not_active Expired - Fee Related
- 1992-06-11 US US08/162,203 patent/US5516586A/en not_active Expired - Lifetime
- 1992-06-11 EP EP92912262A patent/EP0587709B1/en not_active Expired - Lifetime
- 1992-06-11 WO PCT/GB1992/001052 patent/WO1992022676A1/en active IP Right Grant
- 1992-06-11 CA CA002111004A patent/CA2111004A1/en not_active Abandoned
-
1993
- 1993-12-10 NO NO934529A patent/NO934529L/no unknown
- 1993-12-10 NO NO934529D patent/NO934529D0/no unknown
Also Published As
Publication number | Publication date |
---|---|
US5516586A (en) | 1996-05-14 |
DE69219773T2 (de) | 1998-01-02 |
NO934529L (no) | 1993-12-10 |
DE69219773D1 (de) | 1997-06-19 |
GB9112499D0 (en) | 1991-07-31 |
CA2111004A1 (en) | 1992-12-23 |
EP0587709A1 (en) | 1994-03-23 |
EP0587709B1 (en) | 1997-05-14 |
JPH07502071A (ja) | 1995-03-02 |
WO1992022676A1 (en) | 1992-12-23 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
NO934529D0 (no) | Beskyttelse av metalloverflater mot korrosjon | |
DE69322141D1 (de) | Korrosionsinhibierende Zusammensetzung | |
DK0526251T3 (da) | Korrosionsinhibitorer | |
DE69305111D1 (de) | Korrosionsbeständige Grundierungzusammensetzung | |
FI946086A0 (fi) | Metallien valmistus mineraaleista | |
NO307425B1 (no) | Korrosjonsinhibitor | |
DE69209009D1 (de) | Metalldichtung | |
DE69212777D1 (de) | Verhinderung von Korrosion und Ablagerungen | |
DE69307780D1 (de) | Metalldichtung | |
DK109395A (da) | Fremgangsmåde til beskyttelse af metaloverflader | |
DE69217136D1 (de) | Metalldichtung | |
NO952188D0 (no) | Tetning av metall | |
DE69314395D1 (de) | Metalldichtung | |
DE69318138T3 (de) | Metalldichtung | |
DE69302205D1 (de) | Korrosionsschutz mit Cu-BTA | |
DE69217547D1 (de) | Laminierte Metalldichtung | |
DE69119717D1 (de) | Korrosionsverhinderung | |
NO923339D0 (no) | Korrosjonsinhibitor | |
TR199501469A2 (tr) | Metal yüzeylerin koroziyondan korunmasi ve sürtünmenin azaltilmasi | |
FI954422A (fi) | Ferroseenin käyttö | |
GB2069880B (en) | Protecting metal surfaces against corrosion | |
DK163687A (da) | Freemgangsmaade til beskyttelse af metal mod korrosion | |
NO940190L (no) | Anvendelse av alpha-ketoglutarat | |
KR930020002U (ko) | 금속적층형 개스킷 | |
KR900009897A (ko) | 부식 억제 도료 조성물 |