MY158226A - Method for improving the stability of aluminum electrolytic cell and electrolytic cell - Google Patents
Method for improving the stability of aluminum electrolytic cell and electrolytic cellInfo
- Publication number
- MY158226A MY158226A MYPI2011005845A MYPI2011005845A MY158226A MY 158226 A MY158226 A MY 158226A MY PI2011005845 A MYPI2011005845 A MY PI2011005845A MY PI2011005845 A MYPI2011005845 A MY PI2011005845A MY 158226 A MY158226 A MY 158226A
- Authority
- MY
- Malaysia
- Prior art keywords
- electrolytic cell
- aluminum
- stability
- aluminum electrolytic
- improving
- Prior art date
Links
Classifications
-
- C—CHEMISTRY; METALLURGY
- C25—ELECTROLYTIC OR ELECTROPHORETIC PROCESSES; APPARATUS THEREFOR
- C25C—PROCESSES FOR THE ELECTROLYTIC PRODUCTION, RECOVERY OR REFINING OF METALS; APPARATUS THEREFOR
- C25C3/00—Electrolytic production, recovery or refining of metals by electrolysis of melts
- C25C3/06—Electrolytic production, recovery or refining of metals by electrolysis of melts of aluminium
- C25C3/08—Cell construction, e.g. bottoms, walls, cathodes
Applications Claiming Priority (1)
Application Number | Priority Date | Filing Date | Title |
---|---|---|---|
CN2009100877421A CN101580949B (zh) | 2009-06-24 | 2009-06-24 | 一种提高铝电解槽稳定性的方法 |
Publications (1)
Publication Number | Publication Date |
---|---|
MY158226A true MY158226A (en) | 2016-09-15 |
Family
ID=41363259
Family Applications (1)
Application Number | Title | Priority Date | Filing Date |
---|---|---|---|
MYPI2011005845A MY158226A (en) | 2009-06-24 | 2009-12-10 | Method for improving the stability of aluminum electrolytic cell and electrolytic cell |
Country Status (3)
Country | Link |
---|---|
CN (1) | CN101580949B (zh) |
MY (1) | MY158226A (zh) |
WO (1) | WO2010148608A1 (zh) |
Families Citing this family (7)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
CN101580949B (zh) * | 2009-06-24 | 2010-08-25 | 中国铝业股份有限公司 | 一种提高铝电解槽稳定性的方法 |
CN102121116A (zh) * | 2010-01-07 | 2011-07-13 | 贵阳铝镁设计研究院 | 可更换的铝电解槽阴极阻流装置 |
WO2011082658A1 (zh) * | 2010-01-07 | 2011-07-14 | 中铝国际工程有限责任公司 | 可更换的铝电解槽阴极阻流装置 |
RU2454490C1 (ru) * | 2010-11-02 | 2012-06-27 | Общество с ограниченной ответственностью "Легкие металлы" | Электролизер для производства алюминия |
US8795507B2 (en) | 2011-08-05 | 2014-08-05 | Alcoa Inc. | Apparatus and method for improving magneto-hydrodynamics stability and reducing energy consumption for aluminum reduction cells |
CN105862078B (zh) * | 2016-03-28 | 2018-06-22 | 沈阳化工大学 | 一种利用瓷砖废渣制备铝电解槽干式防渗料及其制备方法 |
CN112877732B (zh) * | 2021-01-13 | 2022-02-22 | 东北大学 | 一种减少铝电解槽沉淀形成的阴极结构 |
Family Cites Families (13)
Publication number | Priority date | Publication date | Assignee | Title |
---|---|---|---|---|
US4093524A (en) * | 1976-12-10 | 1978-06-06 | Kaiser Aluminum & Chemical Corporation | Bonding of refractory hard metal |
US4383910A (en) * | 1981-05-21 | 1983-05-17 | Reynolds Metals Company | Alumina reduction cell |
US4436598A (en) * | 1983-09-28 | 1984-03-13 | Reynolds Metals Company | Alumina reduction cell |
US4450054A (en) * | 1983-09-28 | 1984-05-22 | Reynolds Metals Company | Alumina reduction cell |
US4631121A (en) * | 1986-02-06 | 1986-12-23 | Reynolds Metals Company | Alumina reduction cell |
US4919782A (en) * | 1989-02-21 | 1990-04-24 | Reynolds Metals Company | Alumina reduction cell |
AU2293499A (en) * | 1998-02-11 | 1999-08-30 | Moltech Invent S.A. | Distribution of alumina-rich electrolyte in aluminium electrowinning cells |
NZ511514A (en) * | 1998-11-17 | 2003-08-29 | Alcan Int Ltd | Wettable and erosion/oxidation-resistant carbon-composite materials containing a metal boride |
AU2002321684A1 (en) * | 2001-07-13 | 2003-01-29 | Moltech Invent S.A. | Alloy-based anode structures for aluminium production |
CN100478500C (zh) * | 2007-03-02 | 2009-04-15 | 冯乃祥 | 一种异形阴极碳块结构铝电解槽 |
CN201367467Y (zh) * | 2009-03-03 | 2009-12-23 | 沈阳铝镁设计研究院 | 节能降耗型铝电解槽 |
CN201367472Y (zh) * | 2009-03-05 | 2009-12-23 | 沈阳铝镁设计研究院 | 槽底出电铝电解槽阴极结构 |
CN101580949B (zh) * | 2009-06-24 | 2010-08-25 | 中国铝业股份有限公司 | 一种提高铝电解槽稳定性的方法 |
-
2009
- 2009-06-24 CN CN2009100877421A patent/CN101580949B/zh active Active
- 2009-12-10 MY MYPI2011005845A patent/MY158226A/en unknown
- 2009-12-10 WO PCT/CN2009/075470 patent/WO2010148608A1/zh active Application Filing
Also Published As
Publication number | Publication date |
---|---|
CN101580949A (zh) | 2009-11-18 |
CN101580949B (zh) | 2010-08-25 |
WO2010148608A1 (zh) | 2010-12-29 |
Similar Documents
Publication | Publication Date | Title |
---|---|---|
MY158226A (en) | Method for improving the stability of aluminum electrolytic cell and electrolytic cell | |
GB2514679A (en) | Electrolytic production of powder | |
CN201793769U (zh) | 一种铝电解用导气型预焙阳极 | |
MY168646A (en) | Surface modified stainless steel cathode for electrolyser | |
CN203878226U (zh) | 一种电解槽结构 | |
CN201598340U (zh) | 铝电解用穿孔阳极 | |
CN201883156U (zh) | 一种铝电解槽的阳极结构 | |
WO2013170310A8 (en) | Drained cathode electrolysis cell for production of rare earth metals | |
CN2931501Y (zh) | 一种铝电解槽阴极异型导电钢棒 | |
CN100582310C (zh) | 一种铝电解的预焙阳极及其制备方法 | |
CN104032329B (zh) | 上插阴极式镁电解槽 | |
CN202030834U (zh) | 铝电解生产用阴极 | |
CN202246904U (zh) | 内腔阴极结构铝电解槽 | |
CN204111883U (zh) | 一种新型硫酸钴电解槽 | |
CN203095847U (zh) | 锡槽加铁槽 | |
CN102560546A (zh) | 一种铝电解槽的阳极结构 | |
CN203411621U (zh) | 一种铝电解槽阴极内衬结构 | |
CN201793768U (zh) | 一种铝电解阳极结构 | |
CN203065592U (zh) | 一种铜电解槽 | |
CN101949035B (zh) | 铝电解用新型组合石墨化异型阴极 | |
CN201801607U (zh) | 一种铝电解用组合式阳极炭块 | |
CN201354385Y (zh) | 铝电解槽阴极碳块结构 | |
CN203270053U (zh) | 铝电解槽熔池 | |
CN204999984U (zh) | 铝电解槽阳极防护结构 | |
CN202030835U (zh) | 复合碳块阴极 |