KR940014865A - 고온 저항성 니켈-크롬 합금 - Google Patents
고온 저항성 니켈-크롬 합금 Download PDFInfo
- Publication number
- KR940014865A KR940014865A KR1019930004764A KR930004764A KR940014865A KR 940014865 A KR940014865 A KR 940014865A KR 1019930004764 A KR1019930004764 A KR 1019930004764A KR 930004764 A KR930004764 A KR 930004764A KR 940014865 A KR940014865 A KR 940014865A
- Authority
- KR
- South Korea
- Prior art keywords
- alloy
- magnesium
- cerium
- calcium
- iron
- Prior art date
Abstract
본 발명은 중량단위로 55-65% 니켈, 19-25%크롬, 1-4.5% 알루미늄, 0.045-0.3% 이트륨, 0.15-1% 티타늄, 0.005-0.5% 탄소, 0.1-1.5% 규소, 0-1% 망간, 0.005% 이상총량의 마그네슘, 칼슘 및 세륨, 0.5% 이하 총량의 마그네슘과 칼슘, 1% 이하의 세륨, 0.0001-0.1% 붕소, 0-0.5% 지르코늄, 0.0001-0.1%질소, 0-10%코발트와 나머지로서 철 및 불순물로 이루어진 내열 및 내식성 합금을 제공한다.
Description
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음
제1도는 1165℃온도 및 대기중에 놓인 각종합금의 중량변화 대 시간의 그래프를 보여즌다.
제2도는 1200℃온도 및 대기중에 놓인 각종합금의 중량변화 대 시간이 그래프를 보여준다.
Claims (15)
- 중량단위로 55-65% 니켈, 19-25%크롬, 1-4.5% 알루미늄, 0.045-0.3% 이트륨, 0.15-1% 티타늄, 0.005-0.5% 탄소, 0.1-1.5% 규소, 0-1% 망간, 0.005% 이상총량의 마그네슘, 칼슘 및 세륨, 0.5% 이하 총량의 마그네슘과 칼슘, 1% 이하의 세륨, 0.0001-0.1% 붕소, 0-0.5% 지르코늄, 0.0001-0.1%질소, 0-10%코발트와 나머지로서 철 및 불순물로 구성된 내열 및 내식성 합금
- 제1항에 있어서, 크롬이 19-22%이고 알루미늄은 2.5-4.0%이며, 이트륨은 0.05-0.15%이고, 티타늄은 0.15-0.75%이고 규소는 0.5-1%인 것을 특징으로 하는 합금.
- 제1항에 있어서, 탄소는 0.01-0.3%, 마그네슘은 0.005-0.2%, 붕소는 0.001-0.5% 또한 질소는 0.001-0.1%인 것을 특징으로 하는 합금
- 제1항에 있어서, 철은 20% 이하인 것을 특징으로 하는 합금.
- 제1항에 있어서, 철은 10-18%인 것을 특징으로 하는 합금.
- 중량단위로 57.5-62.5% 니켈, 19-22% 크롬, 2.5-4% 알루미늄, 0.05-0.15 이트륨, 0.15-0.75% 디타늄, 0.01-0.3% 탄소, 0.5-1% 규소, 0-1% 망간, 0.005%중량의 마그네슘, 칼슘 및 세륨 0.2%총량의 마그네슘 과 칼슘, 1%이하의 세륨, 0.001-0.05%의 붕소, 0-0.4%의 지르코늄, 0-5%코발트와 나머지로서 철 및 불순물로 구성된 내열 및 내식성 합금.
- 제6항에 있어서, 크롬은 19.5-21%이고, 알루미늄은 2.7-3.5%이며, 이트륨은 0.05-0.07% 이고 티타늄은 0.3-0.75%인 것을 특징으로 하는 합금.
- 제6항에 있어서, 탄소는 0.05-0.15%마그네슘은 0.005-0.2%, 붕소는 0.001-0.01% 또한 질소는 0.001-0.05%인 것을 특징으로 하는 합금.
- 제6항에 있어서, 철은 20% 이하인 것을 특징으로 하는 합금.
- 제6항에 있어서, 철은 10-18%인 것을 특징으로 하는 합금.
- 제6항에 있어서, 합금은 0-0.5%동, 0-0.5%의 몰디브덴 0-0.3% 니오븀, 0-0.1% 바나듐과 약 0-0.1% 텅스텐을 함유하는 것을 특징으로 하는 합금.
- 중량단위로 57.5-65.5% 니켈, 19.5-21%크롬, 2.7-3.5% 알루미늄, 0.05-0.07% 이트륨, 0.3-0.75% 티타늄, 10-18%철, 0.5-1% 규소, 0-0.5% 망간, 0.005% 총량의 마그네슘, 칼슘 및 세륨, 0.2% 이하 총량의 마그네슘과 칼슘, 1% 이하의 세륨, 0.001-0.01% 붕소, 0-0.2% 지르코늄, 0.001-0.05%질소, 0-1%코발트와 나머지인 불순물로 구성된 내열 및 내식성 합금
- 제12항에 있어서, 합금에 0-0.5%동, 0-0.5%몰리브덴, 0-0.3%니오븀, 0-0.1%바나듐과 0.01%텅스텐을 포함하는 것을 특징으로 하는 합금.
- 제12항에 있어서, 합금에 0.1%이하 총량의 납, 주석, 안티몬, 비스무트, 인, 황과 산소를 포함하는 것을 특징으로 하는 합금.
- 제12항에 있어서, 질소가 0.03% 이상인 것을 특징으로 하는 합금※참고사항:최초출원 내용에 의하여 공개하는 것임.