KR930013179A - 시효 경화될 수 있는 구리합금을 제품의 최종규격에 가깝게 주조할 때 변온응력을 받는 주조 롤 및 주조 휠의 제조에 사용하는 방법 - Google Patents
시효 경화될 수 있는 구리합금을 제품의 최종규격에 가깝게 주조할 때 변온응력을 받는 주조 롤 및 주조 휠의 제조에 사용하는 방법 Download PDFInfo
- Publication number
- KR930013179A KR930013179A KR1019920025225A KR920025225A KR930013179A KR 930013179 A KR930013179 A KR 930013179A KR 1019920025225 A KR1019920025225 A KR 1019920025225A KR 920025225 A KR920025225 A KR 920025225A KR 930013179 A KR930013179 A KR 930013179A
- Authority
- KR
- South Korea
- Prior art keywords
- casting
- nickel
- copper alloy
- beryllium
- achieve
- Prior art date
Abstract
본 발명은 1.0 내지 2.6%의 니켈, 0.1내지 0.45%의 베릴륨 및 제조조건상의 불순물과 통상적인 가공 첨가물을 포함한 잔여 성분의 구리로 조성되고, 200HB이상의 브리넬 경도와 38m/Ω㎟을 초과하는 전기전도도를 가지는 시효경화될 수 있는 구리합금을, 제품의 최종규격에 가깝게 주조할때 변온응력을 받는 주조 롤 주조 휠의 제조에 사용하는 방법에 관한 것이다.
Description
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음
Claims (6)
1.0내지 2.6%의 니켈, 0.1내지 0.45%의 베릴륨 및 제조조건상의 불순물과 통상적인 가공 첨가물울 포함한 잔여 성분의 구리로 조성되고, 200HB이상의 브리넬 경도와 38m/Ω㎟을 초과하는 전기전도도를 가지는 시효경화될 수 있는 구리합금을 제품의 최종규격에 가깝게 주조할때 변온응력을 받는 주조 롤 주조 휠의 제조에 사용하는 방법.
제1항에 있어서, 제1항에 기재된 목적을 달성하기 위해 0.05내지 0.25%의 지르코늄을 함유하는 시효경과될 수 있는 구리합금의 사용방법.
제1항 또는 제2항에 있어서, 제1항에 기재된 목적을 달성하기 위해 1.4내지 2.2%의 니켈, 0.2내지 0.35%의 베릴륨, 0.15내지 0.2%의 지르코늄 및 제조조건상의 불순물과 통상적인 가공 첨가물을 포함한 잔여 성분의 구리를 함유하는 시효경화될수 있는 구리합금의 사용방법
제1항 또는 제3항에 있어서, 제1항에 기재된 목적을 달성하기 위해 니켈성분이 1.2%이상일 경우 베릴륨에 대한 니켈의 성분비(Ni/Be)가 5이상으로 되는 시효경화될 수 있는 구리합금의 사용방법.
제4항에 있어서, 제1항에 기재된 목적을 달성하기 위해 베릴륨에 대한 니켈의 비율이 5.5내지 7.5의 범위에 있는 시효경화될 수 있는 구리합금의 사용방법.
제1항 내지 제5항 어느 한 항에 있어서, 제1항에 목적을 달성하기 위해 니켈성분이 전체적으로 또는 부분적으로 코발트에 의해 대체되는 시효경화될 수 있는 구리합금의 사용방법.
※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.