KR910012290A - 자성이 우수한 무방향성전기강판의 제조방법 - Google Patents
자성이 우수한 무방향성전기강판의 제조방법 Download PDFInfo
- Publication number
- KR910012290A KR910012290A KR1019890020173A KR890020173A KR910012290A KR 910012290 A KR910012290 A KR 910012290A KR 1019890020173 A KR1019890020173 A KR 1019890020173A KR 890020173 A KR890020173 A KR 890020173A KR 910012290 A KR910012290 A KR 910012290A
- Authority
- KR
- South Korea
- Prior art keywords
- less
- magnetic properties
- electrical steel
- steel sheet
- oriented electrical
- Prior art date
Abstract
내용 없음
Description
본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음
제1도는 냉간압연판의 소둔온도에 따른 최종제품의 자성변화를 나타낸 그래프.
Claims (2)
- C : 0.010%이하, Si : 1.5%이하, Mn : 0.15-1.0%, P : 0.10% 이하, S : 0.007%이하, Al : 0.60% 이하, Sb : 0.01-0.30%, 및 Zr : 0.005-0.10%를 함유하고 나머지 Fe 및 기타불가피하게 첨가되는 불순물로 조성되는 슬라브를 통상의 방법으로 열간압연한 다음, 1단 냉간압연법 혹은 스킨페스를 포함한 2단 냉간압연법에 의해 열연판을 냉간압연처리하는 것을 특징으로 하는 자성이 우수한 무 방향성 전기강판의 제조방법.
- C : 0.010%이하, Si : 1.5%이하, Mn : 0.15-1.0%, P : 0.10% 이하, S : 0.007%이하, Al : 0.60% 이하, Sb : 0.01-0.30%, 및 Zr : 0.005-0.10%를 함유하고 나머지 Fe 및 기타불가피하게 첨가되는 불순물로 조성되는 슬라브를 통상의 방법으로 열간압연한 다음, 이 열연판을 750-900℃에서 1-10분간의 연속소둔 또는 10분-10시간의 상소둔에 의한 예비소둔을 거친후 1단 냉간압연법 혹은 스킨패스를 포함한 2단 냉간압연법에 의해 열연판을 냉간압연 처리하는 것을 특징으로 하는 자성이 우수한 무 방향성 전기강판의 제조 방법.※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.