KR890011985A KR1019880000261A KR880000261A KR890011985A KR 890011985 A KR890011985 A KR 890011985A KR 1019880000261 A KR1019880000261 A KR 1019880000261A KR 880000261 A KR880000261 A KR 880000261A KR 890011985 A KR890011985 A KR 890011985A
Authority
KR
South Korea
Prior art keywords
charcoal
carbonaceous
pitch
prepare
hot air
Prior art date
Application number
KR1019880000261A
Other languages
Korean (ko)
Inventor
서장원
Original Assignee
서장원
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 서장원 filed Critical 서장원
Priority to KR1019880000261A priority Critical patent/KR890011985A/en
Publication of KR890011985A publication Critical patent/KR890011985A/en

Links

Landscapes

  • Solid Fuels And Fuel-Associated Substances (AREA)

Abstract

내용 없음No content

Description

고밀도 성형 숯High density molded charcoal

본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음Since this is an open matter, no full text was included.

Claims (1)

숯의 파편이나 자투리와 톱밥, 왕겨, 볏짚류 등의 복질류를 건류시킨 탄화물을 혼합하여 분쇄기에 집어넣고 분쇄하여 미분말의 형태로 제조하고, 제조된 탄소질 분말 70-80중량부에 클라르, 피치, 등의 탄소질 점결제 10-20중량부와 펄프폐액 이나 페당 밀 5-10중량부를 혼합기에 넣고 페이스 상태의 탄소니상물을 제조하여 성형로울러로 일정한 형태의 성형물을 제조한 다음, 30℃ 이하의 저온에서 저온휘발분을 80% 정도 감소시킨 후, 200℃의 열풍건조기 내에서 약 3시간동안 열풍 건조시켜 나머지 휘발분을 모두 제거하고, 휘발분이 제거된 일정형상이 성형물을 밀폐로에서 공기를 차단시킨 상태에서 약 800℃로 가열하여 점결제로 사용된 클타르, 피치 및 미탄화원료를 완전히 탄화시켜서 제조된 것을 특징으로 하는 성형 숯.Charcoal debris or chopped charcoal and carbonized carbonaceous materials such as sawdust, rice husk, rice straw, etc. are mixed, put into a grinder and pulverized to prepare in the form of fine powder. 10-20 parts by weight of carbonaceous caking agent such as pitch and 5-10 parts by weight of pulp waste liquid or fructose mill were put into a mixer to prepare carbonaceous material in a face state, and then a molded article of a certain shape was produced by a molding roller, and then 30 ° C. After reducing the low-temperature volatile matter by 80% at the following low temperature, hot air dried for about 3 hours in a 200 ℃ hot air dryer to remove all remaining volatile components, and a certain shape in which the volatile components were removed blocks the air from the closed furnace. Molded charcoal, characterized in that prepared by heating to about 800 ℃ in a state of complete carbonization of the tar, pitch and uncarbonized raw materials used as a caking agent. ※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.※ Note: The disclosure is based on the initial application.
KR1019880000261A 1988-01-15 1988-01-15 High density molded charcoal KR890011985A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
KR1019880000261A KR890011985A (en) 1988-01-15 1988-01-15 High density molded charcoal

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
KR1019880000261A KR890011985A (en) 1988-01-15 1988-01-15 High density molded charcoal

Publications (1)

Publication Number Publication Date
KR890011985A true KR890011985A (en) 1989-08-23

Family

ID=68233178

Family Applications (1)

Application Number Title Priority Date Filing Date
KR1019880000261A KR890011985A (en) 1988-01-15 1988-01-15 High density molded charcoal

Country Status (1)

Country Link
KR (1) KR890011985A (en)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
KR20030066825A (en) * 2002-02-05 2003-08-14 청림에스코 주식회사 Process of manufacture of carbon heating unit
KR20030079175A (en) * 2002-04-02 2003-10-10 박영환 Treatment Method of Charcoal

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
KR20030066825A (en) * 2002-02-05 2003-08-14 청림에스코 주식회사 Process of manufacture of carbon heating unit
KR20030079175A (en) * 2002-04-02 2003-10-10 박영환 Treatment Method of Charcoal

Similar Documents

Publication Publication Date Title
US5797972A (en) Sewage sludge disposal process and product
GB1415017A (en) Manufacture of activated carbon
NO974341L (en) Process for making coal
CN105062601A (en) Preparation method and system for green carbon containing biomass
GB1286532A (en) Improvements in and relating to the production of solid fuels
GB2061317A (en) Process for producing coal briquettes to be gasified or devolatilised
KR890011985A (en) High density molded charcoal
JPS61228096A (en) Production of woody solidified fuel
US1668643A (en) Manufacture of fuel briquettes
GB946358A (en) Barbecue briquettes and method of making the same
JPS56100222A (en) Treatment of sludge of paper manufacturing
SU1701735A1 (en) Composition of fuel briquettes
JPS575790A (en) Preparation of solid fuel
JPH0237397B2 (en) KOKEINENRYOYONENKETSUZAINOSEIZOHOHO
JPS55100212A (en) Manufacture of water purifying molded charcoal
Widjaya et al. Utilization of Several Agricultural Wastes into Briquette as Renewable Energy Source
JPS5540761A (en) Molding material
JPS62263287A (en) Production of solid fuel from chaff and rice straw
GB1057045A (en) Process for the production of porous carbon blocks
CN205152166U (en) Preparation system that contains green charcoal of living beings
JPS57100910A (en) Preparation of molded active coke
SU1715830A1 (en) Mixture for producing fuel briquettes
US1103078A (en) Manufacture of briquets and other articles.
ES8202860A1 (en) Fuel briquette with high calorific value - from sawdust and pitch
RU2149890C1 (en) Fuel briquettes' fabrication method

Legal Events

Date Code Title Description
A201 Request for examination
E902 Notification of reason for refusal
E601 Decision to refuse application