KR890010300A
KR890010300A KR870014995A KR870014995A KR890010300A KR 890010300 A KR890010300 A KR 890010300A KR 870014995 A KR870014995 A KR 870014995A KR 870014995 A KR870014995 A KR 870014995A KR 890010300 A KR890010300 A KR 890010300A
Authority
KR
South Korea
Prior art keywords
composite yarn
low shrinkage
latent crimped
crimped composite
manufacturing
Prior art date
Application number
KR870014995A
Other languages
Korean (ko)
Other versions
KR900003340B1 (en
Inventor
류윤호
김우종
박세웅
Original Assignee
이상철
주식회사 코오롱
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 이상철, 주식회사 코오롱 filed Critical 이상철
Priority to KR1019870014995A priority Critical patent/KR900003340B1/en
Publication of KR890010300A publication Critical patent/KR890010300A/en
Application granted granted Critical
Publication of KR900003340B1 publication Critical patent/KR900003340B1/en

Links

Classifications

    • DTEXTILES; PAPER
    • D01NATURAL OR MAN-MADE THREADS OR FIBRES; SPINNING
    • D01FCHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS; APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBON FILAMENTS
    • D01F8/00Conjugated, i.e. bi- or multicomponent, artificial filaments or the like; Manufacture thereof

Abstract

내용 없음No content

Description

잠재권축성 복합사의 제조방법Manufacturing method of latent crimped composite yarn

본 내용은 요부공개 건이므로 전문내용을 수록하지 않았음Since this is an open matter, no full text was included.

제1도는 본 발명에 사용된 방사구금공의 예,1 is an example of a spinneret used in the present invention,

제2도는 본 발명에 사용된 방사구금장치의 예,2 is an example of a spinneret used in the present invention,

제3도는 본 발명으로 제조된 복합사의 단면형태.Figure 3 is a cross-sectional shape of the composite yarn produced by the present invention.

Claims (2)

저수축성분으로서 고유점도가 0.65-0.70인 폴리에스테르 수지를 사용하고, 고수축성분으로서 고유점도가 저수축성분보다 0.1이상 차이가 나는 고유점도가 0.75-0.80인 공중합 폴리에스테르 수지를 사용하여 저수축부-고수축부-저수축부의 단면형태(제3도의 단면형태)를 갖는 복합사를 방사하되, 저수축부 : 고수축부 : 저수축부의 중량비가 1:2:1이 되도록 방사한 다음, 1단 연신 배율이 총연신배율의 60-80%가 되게 1단 연신하고 이어서 2단 연신하는 잠재권축성 복합사의 제조방법.Low shrinkage is achieved by using a polyester resin with an intrinsic viscosity of 0.65-0.70 as a low shrinkage component, and a copolyester polyester resin with an intrinsic viscosity of 0.75-0.80 having an intrinsic viscosity of at least 0.1 difference from the low shrinkage component as a high shrinkage component. Spinning the composite yarn having the cross-sectional shape of the sub-high shrinkage portion-low shrinkage portion (the cross-sectional shape of FIG. 3), and the low shrinkage portion: high shrinkage portion: spun so that the weight ratio of the low shrinkage portion is 1: 2: 1, and then A method for producing a latent crimped composite yarn in which the draw ratio is drawn in one step so that the draw ratio is 60-80% of the total draw magnification and then drawn in two steps. 제1항에 있어서, 2단 연신함에 있어서, 예열로울러의 온도를 85℃정도로 하고, 제2로울러의 온도를 110℃-130℃로 하는 잠재권축성 복합사의 제조방법.The method for producing a latent crimped composite yarn according to claim 1, wherein in the two-stage drawing, the preheating roller temperature is about 85 ° C and the second roller temperature is 110 ° C-130 ° C. ※ 참고사항 : 최초출원 내용에 의하여 공개하는 것임.※ Note: The disclosure is based on the initial application.
KR1019870014995A 1987-12-26 1987-12-26 The method of potential crimping conjugated yarn KR900003340B1 (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
KR1019870014995A KR900003340B1 (en) 1987-12-26 1987-12-26 The method of potential crimping conjugated yarn

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
KR1019870014995A KR900003340B1 (en) 1987-12-26 1987-12-26 The method of potential crimping conjugated yarn

Publications (2)

Publication Number Publication Date
KR890010300A true KR890010300A (en) 1989-08-08
KR900003340B1 KR900003340B1 (en) 1990-05-14

Family

ID=19267367

Family Applications (1)

Application Number Title Priority Date Filing Date
KR1019870014995A KR900003340B1 (en) 1987-12-26 1987-12-26 The method of potential crimping conjugated yarn

Country Status (1)

Country Link
KR (1) KR900003340B1 (en)

Also Published As

Publication number Publication date
KR900003340B1 (en) 1990-05-14

Similar Documents

Publication Publication Date Title
KR890010300A (en) Manufacturing method of latent crimped composite yarn
KR890002452A (en) Manufacturing method of conductive polyester fiber
KR950001653B1 (en) Manufacturing process for polyester composite fiber having crimp tendency
KR910012367A (en) Manufacturing method of low shrinkage high strength polyester fiber
KR920012540A (en) Manufacturing method of low shrink polyester
KR880007830A (en) Manufacturing method of crimping fineness polyester yarn
KR940014978A (en) Polyester latent crimping bisqueeze blend fiber and its manufacturing method
GB1016861A (en) Improvements in or relating to filaments having a longitudinally extending sharp-edge configuration
KR910008197A (en) Manufacturing method of polyester biaxial blended yarn
KR970074990A (en) Method for producing high strength low shrink polyester fiber
KR960023292A (en) High Elongation Low Shrinkage Polyester Fiber and Manufacturing Method Thereof
KR950014383A (en) Manufacturing method of polyester shrink shrink blended yarn
KR960010920A (en) Manufacturing method of high strength low shrink polyester fiber
KR890006870A (en) Manufacturing method of conductive polyester fiber
KR970001627A (en) High Strength Low Shrink Polyethylene Naphthalate Fiber
KR970010732B1 (en) Composite fiber of two component and its manufacturing method
KR940000624A (en) Manufacturing Method of Polyester Stance
KR930013288A (en) Polyester tire cord and tire cord manufacturing method
KR910012368A (en) Manufacturing method of high strength polyester fiber
KR880003042A (en) Manufacturing method of composite fiber
KR970027380A (en) High strength low shrinkage polyester fiber
KR970011052A (en) Manufacturing method of polyester microfiber
KR940014979A (en) Manufacturing method of spun-like composite polyester yarn
KR910009979A (en) Manufacturing method of polyester shrink shrink blended yarn
JPS55122014A (en) Polyester fiber and its production

Legal Events

Date Code Title Description
A201 Request for examination
G160 Decision to publish patent application
E701 Decision to grant or registration of patent right
GRNT Written decision to grant
FPAY Annual fee payment

Payment date: 19970418

Year of fee payment: 8

LAPS Lapse due to unpaid annual fee